A method of forming a feature on a substrate, comprising: a) depositing a barrier layer over the surfaces of an aperture, the barrier layer having a thickness of between about 5 and about 700 Angstroms; b) chemical vapor depositing copper over the surface of the barrier layer without capping the aperture, the chemical vapor deposited copper having a thickness of between about 200 Angstroms and about 1 micron; c) physical vapor depositing copper over the chemical vapor deposited copper at a temperature below about 660° C. so that the physical vapor deposited copper and chemical vapor deposited copper substantially fill the aperture.
Claim 2
Independent Claim
102 words
A method of forming a feature on a substrate, comprising: a) depositing a barrier layer over the surfaces of an aperture, the barrier layer having a thickness of between about 5 and about 700 Angstroms; b) chemical vapor depositing copper over the surface of the barrier layer without capping the aperture, the chemical vapor deposited copper having a thickness of between about 200 Angstroms and about 1 micron; c) physical vapor depositing copper over the chemical vapor deposited copper at a temperature below about 660° C. so that the physical vapor deposited copper and chemical vapor deposited copper substantially fill the aperture.
Claim 3
Dependent Claim
20 words
The method of claim 1, wherein the barrier layer has a thickness of between about 100 and about 200 Angstroms.
Claim 4
Dependent Claim
24 words
The method of claim 1, wherein the physical vapor deposition comprises the physical vapor deposition of copper at a temperature below about 400° C.
Claim 5
Dependent Claim
21 words
The method of claim 1, further comprising performing the method sequentially in an integrated processing system with a common vacuum mainframe.
Claim 6
Dependent Claim
13 words
The method of claim 1, further comprising performing the method in separate chambers.
Claim 7
Dependent Claim
43 words
The method of claim 1, wherein the barrier layer is selected from the group consisting essentially of tungsten (W), niobium (Nb), aluminum silicates, tantalum (Ta), tantalum nitride (TaN), titanium nitride (TiN), physical vapor deposition Ti/N 2 -stuffed, TiSiN, WSiN, or a combination thereof.
Claim 8
Dependent Claim
25 words
The method of claim 1, further comprising: (d) exposing the substrate to oxygen between chemical vapor depositing the copper and physical vapor depositing the copper.
Claim 9
Dependent Claim
37 words
The method of claim 1, wherein the physical vapor deposited copper includes a dopant therein, the method further comprising annealing the physical vapor deposited copper at a temperature of between about 250° C. and about 450° C.
Claim 10
Dependent Claim
11 words
The method of claim 1, wherein physical vapor depositing comprises sputtering.
Claim 11
Dependent Claim
73 words
A process for filling an aperture on a substrate, comprising: a) forming a thin first layer over the surfaces of an aperture; b) forming a thin conformal chemical vapor deposited copper layer over the first layer without substantially capping the aperture; and c) forming a physical vapor deposited copper layer over the chemical vapor deposited copper layer, wherein the physical vapor deposited copper is deposited at a temperature less than about 660° C.
Claim 12
Dependent Claim
73 words
A process for filling an aperture on a substrate, comprising: a) forming a thin first layer over the surfaces of an aperture; b) forming a thin conformal chemical vapor deposited copper layer over the first layer without substantially capping the aperture; and c) forming a physical vapor deposited copper layer over the chemical vapor deposited copper layer, wherein the physical vapor deposited copper is deposited at a temperature less than about 660° C.
Claim 13
Dependent Claim
17 words
The process of claim 10 wherein the first layer is deposited using a physical vapor deposition process.
Claim 14
Dependent Claim
17 words
The process of claim 10 wherein the first layer has a thickness less than about 2000 Angstroms.
Claim 15
Dependent Claim
11 words
The process of claim 10 wherein the first layer comprises tantalum.
Claim 16
Dependent Claim
43 words
The process of claim 10 wherein the first layer is selected from the group consisting essentially of tungsten (W), niobium (Nb), aluminum silicates, tantalum (Ta), tantalum nitride (TaN), titanium nitride (TiN), physical vapor deposition Ti/N 2 -stuffed, TiSiN, WSiN, or a combination thereof.
Claim 17
Dependent Claim
22 words
The process of claim 10 wherein the physical vapor deposited copper layer is deposited at a temperature less than about 400° C.
Claim 18
Dependent Claim
21 words
The process of claim 10 wherein the chemical vapor deposited copper layer is deposited at a temperature below about 400° C.
Claim 19
Dependent Claim
24 words
The process of claim 10 wherein the chemical vapor deposited copper and physical vapor deposited copper layers intermix to form an intermixed copper layer.
Claim 20
Dependent Claim
18 words
The process of claim 10, wherein forming the physical vapor deposited copper layer comprises sputtering the copper layer.