Abstract

Abstract A method for fabricating an array of ultra-small pores for use in chalcogenide memory cells. A layer of a first material is applied onto a substrate. A portion of the layer of the first material is then removed to define an upper surface with vertical surfaces extending therefrom to a lower surface in the first layer of the first material. A fixed layer of a second material is then applied onto the vertical surfaces of the first layer of the first material. The fixed layer of the second material has a first thickness. A second layer of the first material is then applied onto the fixed layer of the second material. The fixed layer of the second material is then removed to define an array of pores in the first material layers. The pores thus defined have minimum lateral dimensions ranging from approximately 50 to 500 Angstroms and cross sectional areas greater than or equal to the first thickness of the second layer squared. The pores thus defined are further equally spaced from adjacent pores by a spacing ranging from approximately 0.25 to 0.5 microns. The pores thus defined may then be used to fabricate an array of chalcogenide memory cells.

Inventors

  • 👤 Fernando Gonzalez
  • 👤 Raymond A. Turi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 10:47
CPC Classifications
H; H10; H10N; H10N70/00; H10N70/011; H10N70/061; H10N70/068; H10B; H10B63/00; H10B63/80; H10N70/20; H10N70/231; H10N70/801; H10N70/821; H10N70/826; H10N70/881; H10N70/882; H10N70/8828; Y; Y10; Y10S; Y10S257/00; Y10S257/90

Claims Analysis

Total Claims: 41
Claim 1
Independent Claim 126 words
An array of pores fabricated by a process comprising the steps of: applying a first layer of a first material onto a substrate; removing a portion of said first layer of said first material to define a cross-shaped upper surface with generally vertical surfaces extending therefrom to a lower surface in said first layer of said first material; applying a fixed layer of a second material onto said generally vertical surfaces of said first layer of said first material, said fixed layer of said second material having a first thickness; applying a second layer of said first material onto said fixed layer of said second material; and removing said fixed layer of said second material to define said array of pores in said first material layers.
Claim 2
Dependent Claim 126 words
An array of pores fabricated by a process comprising the steps of: applying a first layer of a first material onto a substrate; removing a portion of said first layer of said first material to define a cross-shaped upper surface with generally vertical surfaces extending therefrom to a lower surface in said first layer of said first material; applying a fixed layer of a second material onto said generally vertical surfaces of said first layer of said first material, said fixed layer of said second material having a first thickness; applying a second layer of said first material onto said fixed layer of said second material; and removing said fixed layer of said second material to define said array of pores in said first material layers.
Claim 3
Dependent Claim 22 words
The array of pores of claim 1, wherein said pores have a minimum lateral dimension ranging from approximately 50 to 500 Angstroms.
Claim 4
Dependent Claim 31 words
The array of pores of claim 1, wherein said pores have a cross sectional area greater than or equal to said first thickness of said layer of said second material squared.
Claim 5
Dependent Claim 47 words
The array of pores of claim 1, wherein said pores have a minimum lateral dimension ranging from approximately 50 to 500 Angstroms; and wherein said pores have a cross sectional area greater than or equal to said first thickness of said layer of said second material squared.
Claim 6
Dependent Claim 14 words
The array of pores of claim 1, wherein said upper surface is generally horizontal.
Claim 7
Dependent Claim 25 words
The array of pores of claim 5, wherein said cross shaped horizontal upper surface includes a pair of arms extending relative to a central point.
Claim 8
Dependent Claim 26 words
The array of pores of claim 6, wherein said arms of said cross shaped horizontal upper surface range in length from about 0.5 to 1 micron.
Claim 9
Dependent Claim 22 words
The array of pores of claim wherein said upper surface is surrounded by a recess defined in part by said lower surface.
Claim 10
Dependent Claim 24 words
The array of pores of claim 8, wherein said upper surface includes a plurality of arms extending laterally relative to a generally central location.
Claim 11
Dependent Claim 16 words
The array of pores of claim 1, wherein said first material is comprised of silicon nitride.
Claim 12
Dependent Claim 16 words
The array of pores of claim 1, wherein said second material is comprised of silicon dioxide.
Claim 13
Dependent Claim 26 words
The array of pores of claim 1, wherein said first material is comprised of silicone nitride and wherein said second material is comprised of silicon dioxide.
Claim 14
Dependent Claim 70 words
An array of chalcogenide memory cells, comprising: a plurality of chalcogenide memory cells positioned in a generally common plane, each said chalcogenide memory cell including: an upper electrode; a lower electrode; a dielectric layer positioned between said upper and lower electrodes and including an opening defining a pore having an L-shaped cross section; a chalcogenide element within said pore, said chalcogenide element electrically coupled to said upper and lower electrodes.
Claim 15
Dependent Claim 70 words
An array of chalcogenide memory cells, comprising: a plurality of chalcogenide memory cells positioned in a generally common plane, each said chalcogenide memory cell including: an upper electrode; a lower electrode; a dielectric layer positioned between said upper and lower electrodes and including an opening defining a pore having an L-shaped cross section; a chalcogenide element within said pore, said chalcogenide element electrically coupled to said upper and lower electrodes.
Claim 16
Dependent Claim 20 words
The array of claim 13, wherein a minimum lateral dimension of said pores ranges from about 50 to 500 Angstroms.
Claim 17
Dependent Claim 25 words
The array of claim 13, wherein pores of adjacent chalcogenide memory cells are spaced apart by a distance ranging from about 0.25 to 0.5 microns.
Claim 18
Independent Claim 98 words
A method of fabricating an array of pores comprising the acts of: (a) removing a portion of an upper surface of a substrate to define a cross-shaped protrusion having a sidewall extending therefrom; (b) disposing a layer of a first material in a conformal manner over the cross-shaped protrusion and the sidewall; (c) disposing a layer of a second material over the layer of the first material; (d) exposing an upper portion of the layer of the first material on the sidewall; and (e) removing the layer of the first material on the sidewall to create a pore.
Claim 19
Independent Claim 98 words
A method of fabricating an array of pores comprising the acts of: (a) removing a portion of an upper surface of a substrate to define a cross-shaped protrusion having a sidewall extending therefrom; (b) disposing a layer of a first material in a conformal manner over the cross-shaped protrusion and the sidewall; (c) disposing a layer of a second material over the layer of the first material; (d) exposing an upper portion of the layer of the first material on the sidewall; and (e) removing the layer of the first material on the sidewall to create a pore.
Claim 20
Dependent Claim 31 words
The method, as set forth in claim 16, wherein act (a) comprises the act of: disposing a layer of a first dielectric material over a layer of a first conductive material.
Claim 21
Dependent Claim 16 words
The method, as set forth in claim 17, wherein the first dielectric material comprises silicon nitride.
Claim 22
Dependent Claim 24 words
The method, as set forth in claim 17, wherein the layer of the first conductive material comprises a lower electrode of a memory cell.
Claim 23
Dependent Claim 28 words
The method, as set forth in claim 16, wherein act (b) comprises the act of: disposing a layer of silicon oxide over the cross-shaped protrusion and the sidewall.
Claim 24
Dependent Claim 30 words
The method, as set forth in claim 16, wherein act (c) comprises the act of: disposing a layer of a second dielectric material over the layer of the first material.
Claim 25
Dependent Claim 16 words
The method, as set forth in claim 21, wherein the second dielectric material comprises silicon nitride.
Claim 26
Dependent Claim 20 words
The method, as set forth in claim 16, wherein the first material is selectively etchable relative to the second material.
Claim 27
Dependent Claim 44 words
The method, as set forth in claim 16, wherein act (d) comprises the act of: removing a portion of the layer of the first material and a portion of the layer of the second material to expose an upper surface of the cross-shaped protrusion.
Claim 28
Dependent Claim 44 words
The method, as set forth in claim 16, wherein act (d) comprises the act of: planarizing a portion of the layer of the first material and a portion of the layer of the second material to expose an upper surface of the cross-shaped protrusion.
Claim 29
Dependent Claim 28 words
The method, as set forth in claim 16, wherein act (e) comprises the act of: removing a portion of the substrate to create the pore in the substrate.
Claim 30
Dependent Claim 19 words
The method, as set forth in claim 26, wherein act (e) comprises the act of: removing the cross-shaped protrusion.
Claim 31
Dependent Claim 23 words
The method, as set forth in claim 16, further comprising the act of: disposing a layer of a third material into the pore.
Claim 32
Dependent Claim 16 words
The method, as set forth in claim 28, wherein the third material comprises a memory material.
Claim 33
Dependent Claim 16 words
The method, as set forth in claim 29, wherein the memory material comprises a chalcogenide material.
Claim 34
Dependent Claim 28 words
The method, as set forth in claim 29, further comprising the act of: disposing a layer of a second conductive material over the layer of the memory material.
Claim 35
Dependent Claim 24 words
The method, as set forth in claim 31, wherein the layer of the second conductive material comprises an upper electrode of a memory cell.
Claim 36
Dependent Claim 19 words
The method, as set forth in claim 16, wherein acts (a) through (e) are performed in the order recited.
Claim 37
Dependent Claim 69 words
An array of memory cells comprising: a plurality of memory cells positioned on a substrate, each memory cell comprising: an upper electrode; a lower electrode; a dielectric layer disposed between the upper electrode and the lower electrode, the dielectric layer having a pore formed therein extending from the upper electrode to the lower electrode, the pore having an L-shaped cross section; and a memory element disposed within the pore.
Claim 38
Dependent Claim 69 words
An array of memory cells comprising: a plurality of memory cells positioned on a substrate, each memory cell comprising: an upper electrode; a lower electrode; a dielectric layer disposed between the upper electrode and the lower electrode, the dielectric layer having a pore formed therein extending from the upper electrode to the lower electrode, the pore having an L-shaped cross section; and a memory element disposed within the pore.
Claim 39
Dependent Claim 16 words
The array, as set forth in claim 34, wherein the memory element comprises a chalcogenide material.
Claim 40
Dependent Claim 23 words
The array, as set forth in claim 34, wherein a minimum lateral dimension of each pore ranges from about 50 to 500 Angstroms.
Claim 41
Dependent Claim 27 words
The array, as set forth in claim 34, wherein pores of adjacent memory cells are spaced apart by a distance ranging from about 0.25 to 0.5 microns.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2002-12-13 2003-06-14 2003-12-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2006-12-13 2007-06-14 2007-12-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2010-12-13 2011-06-14 2011-12-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag