Abstract
Abstract Described is a flexible adhesive formulation for bonding a semiconductor device to a flexible substrate and a flexible card containing a semiconductor device which can be processed in a computer.
Inventors
- 👤 My N. Nguyen
- 👤 Yuan Y. Chien
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 05:43
CPC Classifications
C; C07; C07C; C07C261/00; C07C261/02; C08; C08G; C08G59/00; C08G59/18; C08G59/40; C08G59/4007; C08K; C08K5/00; C08K5/0008; C08K5/0016; C09; C09J; C09J179/00; C09J179/04; G; G06; G06K; G06K19/00; G06K19/06; G06K19/067; G06K19/07; G06K19/077; G06K19/07745; H; H01; H01B; H01B1/00; H01B1/20; H01B1/22; H10; H10W; H10W20/00; H10W20/40; H10W40/00; H10W40/20; H10W40/25; H10W40/251; H10W70/00; H10W70/60; H10W70/699; H10W72/00; H10W72/071; H10W72/073; H10W72/07331; H10W72/07337; H10W72/30; H10W72/321; H10W72/325; H10W72/351; H10W72/352; H10W72/353; H10W72/354
Claims Analysis
Total Claims: 24
Claim 1
Independent Claim
90 words
A method of making a cyanate ester flexible which comprises reacting the cyanate ester with at least one flexibilizer having a glass transition temperature less than about 25° C., and comprising at least one member from the group consisting of compounds containing hydroxyl groups having a molecular weight of about 200 to 5000, compounds containing amine and compounds containing epoxide reactive functional groups, or mixtures thereof, to produce a formulation having a viscosity of about 5 to 50 poise and a radius of curvature of about 1 meter or more.
Claim 2
Independent Claim
90 words
A method of making a cyanate ester flexible which comprises reacting the cyanate ester with at least one flexibilizer having a glass transition temperature less than about 25° C., and comprising at least one member from the group consisting of compounds containing hydroxyl groups having a molecular weight of about 200 to 5000, compounds containing amine and compounds containing epoxide reactive functional groups, or mixtures thereof, to produce a formulation having a viscosity of about 5 to 50 poise and a radius of curvature of about 1 meter or more.
Claim 3
Independent Claim
92 words
A method of making a cyanate ester flexible which comprises reacting the cyanate ester with at least one flexibilizer having a glass transition temperature less than about 25° C. comprising at least one polyhydroxyl polymer compound having a molecular weight of about 200 to about 5000 from the group of polyhydroxyl polymer compounds within at least one of the following formulas: HO--(CH.sub.2).sub.m --CO--O--(CH.sub.2).sub.n OH, and HO--(CH.sub.2).sub.m --O--C--O--R--C--O--(CH.sub.2).sub.n --OH to produce a formulation having a viscosity of about 5 to 50 poise and a radius of curvature of about 1 meter or more.
Claim 4
Independent Claim
92 words
A method of making a cyanate ester flexible which comprises reacting the cyanate ester with at least one flexibilizer having a glass transition temperature less than about 25° C. comprising at least one polyhydroxyl polymer compound having a molecular weight of about 200 to about 5000 from the group of polyhydroxyl polymer compounds within at least one of the following formulas: HO--(CH.sub.2).sub.m --CO--O--(CH.sub.2).sub.n OH, and HO--(CH.sub.2).sub.m --O--C--O--R--C--O--(CH.sub.2).sub.n --OH to produce a formulation having a viscosity of about 5 to 50 poise and a radius of curvature of about 1 meter or more.
Claim 5
Dependent Claim
23 words
A method according to claim 2 wherein said polyhydroxyl polymer compound is one from the group consisting of polyhydroxyl polyesters and polyhydroxyl polyethers.
Claim 6
Dependent Claim
17 words
A method according to claim 2 wherein said cyanate ester further includes a metal containing co-curing catalyst.
Claim 7
Independent Claim
70 words
A method of rendering a cyanate ester flexible which comprises adding to the cyanate ester at least one polyhydroxyl polymer compound having a glass transition temperature less than about 25° C. and a molecular weight range of about 200 to about 5000 within at least one of the following formulas: HO--(CH.sub.2).sub.m --CO--O--(CH.sub.2).sub.n --OH and HO--(CH.sub.2).sub.m --O--C--O--R--C--O--(CH.sub.2).sub.m --OH or mixtures thereof, and grafting such polymer to the cyanate ester molecular structure.
Claim 8
Independent Claim
70 words
A method of rendering a cyanate ester flexible which comprises adding to the cyanate ester at least one polyhydroxyl polymer compound having a glass transition temperature less than about 25° C. and a molecular weight range of about 200 to about 5000 within at least one of the following formulas: HO--(CH.sub.2).sub.m --CO--O--(CH.sub.2).sub.n --OH and HO--(CH.sub.2).sub.m --O--C--O--R--C--O--(CH.sub.2).sub.m --OH or mixtures thereof, and grafting such polymer to the cyanate ester molecular structure.
Claim 9
Dependent Claim
18 words
A method according to claim 1 wherein said cyanate ester is reacted with an amine reactive functional group.
Claim 10
Dependent Claim
18 words
A method according to claim 1 wherein said cyanate ester is reacted with an epoxide reactive functional group.
Claim 11
Dependent Claim
19 words
A method according to claim 1 wherein said method comprises reacting cyanate ester with an amine reactive functional group.
Claim 12
Dependent Claim
19 words
A method according to claim 1 wherein said method comprises reacting cyanate ester with an epoxide reactive functional group.
Claim 13
Independent Claim
78 words
A method of making a cyanate ester flexible which comprises reacting 4 to 16 wt. % cyanate ester with 6 to 24 wt. % of at least one flexibilizer having a glass transition temperature less than about 25° C. containing one reactive functional group from the group of hydroxyl, amine and epoxide reactive functional groups, or mixtures thereof, wherein flexibilizers containing hydroxyl reactive functional groups have a molecular weight in the range of about 200 to about 5000.
Claim 14
Independent Claim
78 words
A method of making a cyanate ester flexible which comprises reacting 4 to 16 wt. % cyanate ester with 6 to 24 wt. % of at least one flexibilizer having a glass transition temperature less than about 25° C. containing one reactive functional group from the group of hydroxyl, amine and epoxide reactive functional groups, or mixtures thereof, wherein flexibilizers containing hydroxyl reactive functional groups have a molecular weight in the range of about 200 to about 5000.
Claim 15
Dependent Claim
32 words
A method according to claim 1 wherein said cyanate ester comprises an adhesive formulation suitable for bonding a semiconductor device to a substrate and further comprises a thermally and/or electrically conductive filler.
Claim 16
Dependent Claim
11 words
A method according to claim 2 wherein said filler comprises silver.
Claim 17
Dependent Claim
15 words
A method according to claim 2 wherein said adhesive formulation further comprises a curing catalyst.
Claim 18
Dependent Claim
14 words
A method according to claim 3 wherein said adhesive formulation further comprises an alkylphenol.
Claim 19
Dependent Claim
32 words
A method according to claim 1 wherein said cyanate ester comprises an adhesive formulation suitable for bonding a semiconductor device to a substrate and further comprises a thermally and/or electrically conductive filler.
Claim 20
Dependent Claim
11 words
A method according to claim 15 wherein said filler comprises silver.
Claim 21
Dependent Claim
15 words
A method according to claim 15 wherein said adhesive formulation further comprises a curing catalyst.
Claim 22
Dependent Claim
32 words
A method according to claim 5 wherein said cyanate ester comprises an adhesive formulation suitable for bonding a semiconductor device to a substrate further comprising adding a thermally and/or electrically conductive filler.
Claim 23
Dependent Claim
11 words
A method according to claim 18 wherein said filler comprises silver.
Claim 24
Dependent Claim
12 words
A method according to claim 18 further comprising adding a curing catalyst.
References Cited (Backward Citations)
US1743167A
Cited
US2895270A
Cited
US3586926A
Cited
US3595900A
Cited
US3658623A
Cited
US4280885A
Cited
US4369302A
Cited
US4375498A
Cited
US4401776A
Cited
JPS58153338A
Cited
DE3423385A1
Cited
US4552690A
Cited
US4754001A
Cited
US4740343A
Cited
US4699888A
Cited
US4608434A
Cited
US4604452A
Cited
US4732702A
Cited
US4740830A
Cited
US4709008A
Cited
US4740584A
Cited
US5037691A
Cited
US4861823A
Cited
US5162574A
Cited
US4839442A
Cited
US4940848A
Cited
US4918157A
Cited
US4785075A
Cited
US4847233A
Cited
US4983683A
Cited
US4831086A
Cited
US4902752A
Cited
US5037692A
Cited
US5036646A
Cited
US5215860A
Cited
JPH02285968A
Cited
US4931545A
Cited
US5186880A
Cited
JPH0369883A
Cited
US5002818A
Cited
US4999699A
Cited
US5068309A
Cited
US5149863A
Cited
US5056296A
Cited
US5143785A
Cited
US5150195A
Cited
US5155066A
Cited
WO1992008247A1
Cited
US5261157A
Cited
US5114003A
Cited
US5330684A
Cited
WO1993017059A1
Cited
WO1993016921A1
Cited
WO1993016987A1
Cited
US5195299A
Cited
US5399907A
Cited
US5195299B1
Cited
US5250600A
Cited
WO1993024564A1
Cited
US5325654A
Cited
WO1994006844A1
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1999-02-05 | 1999-08-07 | 2000-02-06 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2003-02-05 | 2003-08-07 | 2004-02-06 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2007-02-05 | 2007-08-07 | 2008-02-06 | $7700.00 | Window Closed / Lapsed |