Method of reducing moisture content of hermetic packages containing semiconductor devices
Assignee: Henkel Corp
•
Filing: 1992-02-28
•
Granted: 1993-03-23
•
Expires: 2012-02-28
Abstract
Abstract Described is a method of reducing the moisture content in a hermetic package containing a semiconductor device by including a small amount of cyanate ester within the package.
Inventors
- 👤 My N. Nguyen
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 14:03
CPC Classifications
H; H10; H10W; H10W76/00; H10W76/40; H10W76/42; H10W76/48
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
79 words
A method of reducing the water moisture content in a hermetic package containing a semiconductor device comprising incorporating within said package a small but effective amount of cyanate ester, reacting said cyanate ester with water to produce an imidocarbonic acid which molecularly rearranges upon formation into a stable carbamate molecular structure, exposing said package to an elevated temperature in the range of about 100° C. to 400° C. whereby said carbamate further reacts with water to produce carbon dioxide.
Claim 2
Independent Claim
79 words
A method of reducing the water moisture content in a hermetic package containing a semiconductor device comprising incorporating within said package a small but effective amount of cyanate ester, reacting said cyanate ester with water to produce an imidocarbonic acid which molecularly rearranges upon formation into a stable carbamate molecular structure, exposing said package to an elevated temperature in the range of about 100° C. to 400° C. whereby said carbamate further reacts with water to produce carbon dioxide.
Claim 3
Independent Claim
23 words
A method according to claim wherein said cyanate ester is incorporated within the package in the form of a cyanate ester-containing adhesive formulation.
Claim 4
Independent Claim
34 words
A method according to claim wherein said package includes a lid and said cyanate ester is incorporated within the package by applying the same to the backside of the package lid prior to sealing.
References Cited (Backward Citations)
US1743167A
Cited
US2895270A
Cited
US3586926A
Cited
US4280885A
Cited
US4375498A
Cited
US5150195A
Cited
US5114003A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1996-03-22 | 1996-09-21 | 1997-03-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2000-03-22 | 2000-09-21 | 2001-03-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2004-03-22 | 2004-09-21 | 2005-03-23 | $7700.00 | Window Closed / Lapsed |