← Back to Patent Explorer
US6596583B2 Expired / Lapsed US ⏱️ 0.0 years remaining

Methods for forming and integrated circuit structures containing ruthenium and tungsten containing layers

Assignee: Mosaid Technologies Inc
•
Filing: 2001-10-29
•
Granted: 2003-07-22
•
Expires: 2021-10-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Capacitors having increased capacitance include an enhanced-surface-area (rough-surfaced) electrically conductive layer or other layers that are compatible with the high-dielectric constant materials. In one approach, an enhanced-surface-area electrically conductive layer for such capacitors is formed by processing a ruthenium oxide layer at high temperature at or above 500° C. and low pressure 75 torr or below, most desirably 5 torr or below, to produce a roughened ruthenium layer having a textured surface with a mean feature size of at least about 100 Angstroms. The initial ruthenium oxide layer may be provided by chemical vapor deposition techniques or sputtering techniques or the like. The layer may be formed over an underlying electrically conductive layer. The processing may be performed in an inert ambient or in a reducing ambient. A nitrogen-supplying ambient or nitrogen-supplying reducing ambient may be used during the processing or afterwards to passivate the ruthenium for improved compatibility with high-dielectric-constant dielectric materials. Processing in an oxidizing ambient may also be performed to passivate the roughened layer. The roughened layer of ruthenium may be used to form an enhanced-surface-area electrically conductive layer. The resulting enhanced-surface-area electrically conductive layer may form a plate of a storage capacitor in an integrated circuit, such as in a memory cell of a DRAM or the like. In another approach, a tungsten nitride layer is provided as an first electrode of such a capacitor. The capacitor, or at least the tungsten nitride layer, is annealed to increase the capacitance of the capacitor.

Inventors

  • 👤 Vishnu K. Agarwal
  • 👤 Garo Derderian
  • 👤 Gurtej S. Sandhu
  • 👤 Weimin M. Li
  • 👤 Mark Visokay
  • 👤 Cem Basceri
  • 👤 Sam Yang

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:08
CPC Classifications
H; H10; H10B; H10B12/00; H10D; H10D1/00; H10D1/60; H10D1/68; H10D1/692; H10D1/711; H10D1/712; H10D1/694; H10D1/682; H10P; H10P14/00; H10P14/60; H10P14/69; H10P14/692; H10P14/6938; H10P14/6939; H10P14/69393; H10P14/69398

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 66 words
A method of forming a capacitor, the method comprising: forming a first conductive layer containing tungsten nitride; annealing the first conductive layer at an anneal temperature sufficient to convert a tungsten nitride compound WN into a tungsten nitride compound W 2 N; forming a layer of dielectric material over the annealed first conductive layer; and forming a second conductive layer over the layer of dielectric material.
Claim 2
Independent Claim 66 words
A method of forming a capacitor, the method comprising: forming a first conductive layer containing tungsten nitride; annealing the first conductive layer at an anneal temperature sufficient to convert a tungsten nitride compound WN into a tungsten nitride compound W 2 N; forming a layer of dielectric material over the annealed first conductive layer; and forming a second conductive layer over the layer of dielectric material.
Claim 3
Dependent Claim 31 words
The method of claim 1 , wherein the anneal temperature is at least 500 C and the first conductive layer is maintained at the anneal temperature for at least 30 seconds.
Claim 4
Dependent Claim 17 words
The method of claim 1 , wherein the first conductive layer is formed conformally on a post.
Claim 5
Dependent Claim 20 words
The method of claim 1 , wherein the first conductive layer is formed conformally in a recess in a substrate.
Claim 6
Dependent Claim 13 words
The method of claim 1 , where the dielectric layer contains tantalum oxide.
Claim 7
Independent Claim 34 words
A method of increasing a capacitance of a capacitor that includes a tungsten nitride bottom electrode, the method comprising annealing the capacitor at an anneal temperature sufficient to convert WN into W 2 N.
Claim 8
Independent Claim 34 words
A method of increasing a capacitance of a capacitor that includes a tungsten nitride bottom electrode, the method comprising annealing the capacitor at an anneal temperature sufficient to convert WN into W 2 N.
Claim 9
Dependent Claim 15 words
The method of claim 6 , wherein the anneal temperature is at least 500 C.
Claim 10
Independent Claim 35 words
A method of forming a bottom electrode of a capacitor, the method comprising: applying a layer of tungsten nitride; annealing the tungsten nitride layer; and forming a dielectric layer on the annealed tungsten nitride layer.
Claim 11
Independent Claim 35 words
A method of forming a bottom electrode of a capacitor, the method comprising: applying a layer of tungsten nitride; annealing the tungsten nitride layer; and forming a dielectric layer on the annealed tungsten nitride layer.
Claim 12
Dependent Claim 41 words
The method of claim 8 , wherein the tungsten nitride layer includes a metastable tungsten nitride compound and the tungsten nitride layer is annealed at a temperature sufficient to convert at least some of the metastable compound to a stable compound.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2006-07-21 2007-01-20 2007-07-22 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2010-07-21 2011-01-20 2011-07-22 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2014-07-21 2015-01-20 2015-07-22 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag