Claims Analysis
Total Claims: 19
Claim 1
Independent Claim
402 words
A method for fabricating a vertical bipolar transistor, which comprises the steps of: i) implanting a first impurity of a second conductivity type into a portion of a surface of a first conductivity type semiconductor substrate and annealing the implanted first impurity of the second conductivity type to form a first buried layer; ii) implanting a second impurity of the second conductivity type into an upper peripheral portion of said first buried layer, and activating the implanted second impurity of the second conductivity type; iii) defining an active region by growing an epitaxial layer of the first conductivity type on said semiconductor substrate having said first buried layer at a surface portion thereof, and out-diffusing the activated second impurity of the upper peripheral portion of said first buried layer, to form a second buried layer of the second conductivity type, said second buried layer having a higher impurity concentration than that of said first buried layer, both said first buried layer and said second buried layer defining a portion of said epitaxial layer as said active region; iv) forming a base region of the second conductivity type by implanting a third impurity of the second conductivity type into a first upper portion of said active region and annealing the implanted third impurity; and v) completing a fabrication of the vertical bipolar transistor by forming an emitter region, a base contact region and a collector contact region at upper portions of said active region, wherein the step v) comprises the substeps of: a) forming an isolating oxide film on a portion of said active region as well as on an upper portion of said epitaxial layer except said active region; b) forming the emitter region of the first conductivity type at a first upper portion of said base region, and the collector contact region of the first conductivity type at a second upper portion of said active region, said collector contact region having a higher impurity concentration than that of said epitaxial layer; c) forming the base contact region of the first conductivity type at a second upper portion of said base region, said base contact region having a higher impurity concentration than that of said base region; and d) forming a base electrode on a surface of said base region, an emitter electrode on a surface of said emitter region and a collector electrode on a surface of said collector contact region.
Claim 2
Independent Claim
402 words
A method for fabricating a vertical bipolar transistor, which comprises the steps of: i) implanting a first impurity of a second conductivity type into a portion of a surface of a first conductivity type semiconductor substrate and annealing the implanted first impurity of the second conductivity type to form a first buried layer; ii) implanting a second impurity of the second conductivity type into an upper peripheral portion of said first buried layer, and activating the implanted second impurity of the second conductivity type; iii) defining an active region by growing an epitaxial layer of the first conductivity type on said semiconductor substrate having said first buried layer at a surface portion thereof, and out-diffusing the activated second impurity of the upper peripheral portion of said first buried layer, to form a second buried layer of the second conductivity type, said second buried layer having a higher impurity concentration than that of said first buried layer, both said first buried layer and said second buried layer defining a portion of said epitaxial layer as said active region; iv) forming a base region of the second conductivity type by implanting a third impurity of the second conductivity type into a first upper portion of said active region and annealing the implanted third impurity; and v) completing a fabrication of the vertical bipolar transistor by forming an emitter region, a base contact region and a collector contact region at upper portions of said active region, wherein the step v) comprises the substeps of: a) forming an isolating oxide film on a portion of said active region as well as on an upper portion of said epitaxial layer except said active region; b) forming the emitter region of the first conductivity type at a first upper portion of said base region, and the collector contact region of the first conductivity type at a second upper portion of said active region, said collector contact region having a higher impurity concentration than that of said epitaxial layer; c) forming the base contact region of the first conductivity type at a second upper portion of said base region, said base contact region having a higher impurity concentration than that of said base region; and d) forming a base electrode on a surface of said base region, an emitter electrode on a surface of said emitter region and a collector electrode on a surface of said collector contact region.
Claim 3
Dependent Claim
25 words
The method for fabricating a vertical bipolar transistor as claimed in claim 1, wherein said emitter region and said collector contact region are simultaneously formed.
Claim 4
Dependent Claim
41 words
The method for fabricating a vertical bipolar transistor as claimed in claim 1, further comprising the step of: forming a subcollector region of the first conductivity type in said active region therein above said first buried layer after the step iii).
Claim 5
Dependent Claim
87 words
The method for fabricating a vertical bipolar transistor as claimed in claim 3, wherein said subcollector region is formed by implanting an impurity of the first conductivity type at an energy of between approximately 0.5 MeV and 1.5 MeV and at a dosage of approximately 5×10 12 atoms/cm 2 to 5×10 13 atoms/cm 2 , and annealing the implanted first impurity of the first conductivity type at a temperature of between 900° C. and 1000° C. and for 60 minutes to 100 minutes in a nitrogen atmosphere.
Claim 6
Dependent Claim
29 words
The method for fabricating a vertical bipolar transistor as claimed in claim 1, wherein the first conductivity type is a P-type and the second conductivity type is an N-type.
Claim 7
Dependent Claim
89 words
The method for fabricating a vertical bipolar transistor as claimed in claim 1, wherein said first buried layer is formed by implanting the first impurity of the second conductivity type at an energy of between approximately 20 KeV and 60 KeV and at a dosage of approximately 1×10 15 atoms/cm 2 to 1×10 16 atoms/cm 2 , and annealing the implanted first impurity of the second conductivity type at a temperature of between 1150° C. and 1250° C. and for 200 minutes to 300 minutes in an oxygen atmosphere.
Claim 8
Dependent Claim
62 words
The method for fabricating a vertical bipolar transistor as claimed claim 1, wherein the second impurity of the second conductivity type is a phosphorus and said second buried layer is formed by implanting the phosphorus at an energy of between approximately 20 KeV and 50 KeV and at a dosage of approximately 5×10 15 atoms/cm 2 to 5×10 16 atoms/cm 2 .
Claim 9
Dependent Claim
45 words
The method for fabricating a vertical bipolar transistor as claimed in claim 7, wherein said second buried layer is formed by annealing the implanted phosphorus at a temperature of between 1000° C. and 1150° C. and for 30 minutes to 60 minutes to be activated.
Claim 10
Dependent Claim
51 words
The method for fabricating a vertical bipolar transistor as claimed in claim 8, wherein said second buried layer is formed by out-diffusing the activated phosphorus at the same time as growing said epitaxial layer of the first conductivity type on said first buried layer as well as on said semiconductor substrate.
Claim 11
Dependent Claim
84 words
The method for fabricating a vertical bipolar transistor as claimed in claim 1, wherein said base region is formed by implanting the third impurity of the second conductivity type at an energy of between approximately 20 KeV and 30 KeV and at a dosage of approximately 5×10 13 atoms/cm 2 to 1×10 14 atoms/cm 2 , and annealing the implanted third impurity of the second conductivity type at a temperature of between 900° C. and 1000° C. and for 30 minutes to 60 minutes.
Claim 12
Independent Claim
390 words
A method for fabricating a vertical bipolar transistor, which comprises the steps of: i) implanting a first impurity of a second conductivity type into a portion of a surface of a first conductivity type semiconductor substrate and annealing the implanted first impurity of the second conductivity type to form a first buried layer; ii) implanting a second impurity of the second conductivity type into an upper peripheral portion of said first buried layer, and activating the implanted second impurity of the second conductivity type; iii) defining an active region by growing an epitaxial layer of the first conductivity type on said semiconductor substrate having said first buried layer at a surface portion thereof at the same time as out-diffusing the activated second impurity of the upper peripheral portion of said first buried layer, to form a second buried layer of the second conductivity type, said second buried layer having higher impurity concentration than that of said first buried layer, both said first buried layer and said second buried layer defining a portion of said epitaxial layer as said active region; iv) forming a subcollector region of the first conductivity type at said active region above said first buried layer; v) forming an isolating oxide film on a portion of said active region and on said epitaxial layer except said active region; vi) forming a base region of the second conductivity type by implanting a third impurity of the second conductivity type into a first upper portion of said active region, and annealing the implanted third impurity of the second conductivity type; vii) forming an emitter region of the first conductivity type at a first upper portion of said base region at the same time as forming a collector contact region of the first conductivity type at a second upper portion of said active region, said collector contact region having a higher impurity concentration than that of said epitaxial layer; viii) forming a base contact region of the first conductivity type at a second upper portion of said base region, said base contact region having a higher impurity concentration than that of said base region; and ix) forming a base electrode on a surface of said base contact region, an emitter electrode on a surface of said emitter region and a collector electrode on a surface of said collector contact region.
Claim 13
Independent Claim
390 words
A method for fabricating a vertical bipolar transistor, which comprises the steps of: i) implanting a first impurity of a second conductivity type into a portion of a surface of a first conductivity type semiconductor substrate and annealing the implanted first impurity of the second conductivity type to form a first buried layer; ii) implanting a second impurity of the second conductivity type into an upper peripheral portion of said first buried layer, and activating the implanted second impurity of the second conductivity type; iii) defining an active region by growing an epitaxial layer of the first conductivity type on said semiconductor substrate having said first buried layer at a surface portion thereof at the same time as out-diffusing the activated second impurity of the upper peripheral portion of said first buried layer, to form a second buried layer of the second conductivity type, said second buried layer having higher impurity concentration than that of said first buried layer, both said first buried layer and said second buried layer defining a portion of said epitaxial layer as said active region; iv) forming a subcollector region of the first conductivity type at said active region above said first buried layer; v) forming an isolating oxide film on a portion of said active region and on said epitaxial layer except said active region; vi) forming a base region of the second conductivity type by implanting a third impurity of the second conductivity type into a first upper portion of said active region, and annealing the implanted third impurity of the second conductivity type; vii) forming an emitter region of the first conductivity type at a first upper portion of said base region at the same time as forming a collector contact region of the first conductivity type at a second upper portion of said active region, said collector contact region having a higher impurity concentration than that of said epitaxial layer; viii) forming a base contact region of the first conductivity type at a second upper portion of said base region, said base contact region having a higher impurity concentration than that of said base region; and ix) forming a base electrode on a surface of said base contact region, an emitter electrode on a surface of said emitter region and a collector electrode on a surface of said collector contact region.
Claim 14
Dependent Claim
86 words
The method for fabricating a vertical bipolar transistor as claimed in claim 11, wherein said subcollector region is formed by implanting an impurity of the first conductivity type at an energy of between approximately 0.5 MeV and 1.5 MeV and at a dosage of approximately 5×10 12 atoms/cm 2 to 5×10 13 atoms/cm 2 , and annealing the implanted impurity of the first conductivity type at a temperature of between 900° C. and 1000° C. and for 60 minutes to 100 minutes in a nitrogen atmosphere.
Claim 15
Dependent Claim
29 words
The method for fabricating a vertical bipolar transistor as claimed in claim 11, wherein the first conductivity type is a P-type and the second conductivity type is an N-type.
Claim 16
Dependent Claim
89 words
The method for fabricating a vertical bipolar transistor as claimed in claim 11, wherein said first buried layer is formed by implanting the first impurity of the second conductivity type at an energy of between approximately 20 KeV and 60 KeV and at a dosage of approximately 1×10 15 atoms/cm 2 to 1×10 16 atoms/cm 2 , and annealing the implanted first impurity of the second conductivity type at a temperature of between 1150° C. and 1250° C. and for 200 minutes to 300 minutes in an oxygen atmosphere.
Claim 17
Dependent Claim
63 words
The method for fabricating a vertical bipolar transistor as claimed in claim 11, wherein the second impurity of the second conductivity type is a phosphorus and said second buried layer is formed by implanting the phosphorous at an energy of between approximately 20 KeV and 50 KeV and at a dosage of approximately 5×10 15 atoms/cm 2 to 5×10 16 atoms/cm 2 .
Claim 18
Dependent Claim
49 words
The method for fabricating a vertical bipolar transistor as claimed in claim 15, wherein said second buried layer is formed by annealing the implanted phosphorous at a temperature of between 1000° C. and 1150° C. and for 30 minutes to 60 minutes in an oxygen atmosphere to be activated.
Claim 19
Dependent Claim
88 words
The method for fabricating a vertical bipolar transistor as claimed in claim 16, wherein said base region is formed by implanting the third impurity of the second conductivity type at an energy of between approximately 20 KeV and 30 KeV and at a dosage of approximately 5×10 13 atoms/cm 2 to 1×10 14 atoms/cm 2 , and annealing the implanted third impurity of the second conductivity type at a temperature of between 900° C. and 1000° C. and for 30 minutes to 60 minutes in a nitrogen atmosphere.