Patent US5200693A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5200693A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for determining characteristics of pn semiconductor structures

Assignee: SINGLETERY JAMES
•
Filing: 1991-02-26
•
Granted: 1993-04-06
•
Expires: 2011-02-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method and apparatus for determining the carrier concentration and profile depth for pn semiconductor structures, and band discontinuities for heterojunction pn structures is disclosed. A more accurate measurement of carrier concentration and profile depth is obtained by initially measuring the pn junction intercept voltage of a pn semiconductor structure to be tested before the structure is exposed to a conventional capacitance-voltage (C-V) profiling process. The pn junction intercept voltage is employed to determine the pn junction capacitance which can then be compensated for in capacitance dependent formulae used for calculating the carrier concentration and profile depth. The intercept voltage can also be used to determine band discontinuities in a heterojunction pn structure. A fixed or retractable metal contact is employed to contact the p-type layer of a pn semiconductor structure to be tested and permit this initial measurement to be obtained. In a preferred form of the invention, a C-V profiling apparatus containing an electrolyte solution which etches through the structure to be tested as capacitance and current measurements are taken is employed. In the case of the fixed metal contact, the electrolyte first etches through the contact before it begins etching through the structure being tested.

Inventors

  • 👤 James Singletery, Jr.

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 20:21
CPC Classifications
H; H10; H10P; H10P74/00; H10P74/20; H10P74/207

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 85 words
A method of determining the carrier concentration and profile depth in a pn semiconductor structure comprising the steps of: measuring the pn junction intercept voltage of said semiconductor structure to be tested; determining the pn junction capacitance, C pn , of said semiconductor structure to be tested from said measured intercept voltage; measuring the carrier concentration and profiling depth of said structure; and, determining the actual carrier concentration and profile depth from said determined pn junction capacitance and said measured carrier concentration and profiling depth.
Claim 2
Independent Claim 85 words
A method of determining the carrier concentration and profile depth in a pn semiconductor structure comprising the steps of: measuring the pn junction intercept voltage of said semiconductor structure to be tested; determining the pn junction capacitance, C pn , of said semiconductor structure to be tested from said measured intercept voltage; measuring the carrier concentration and profiling depth of said structure; and, determining the actual carrier concentration and profile depth from said determined pn junction capacitance and said measured carrier concentration and profiling depth.
Claim 3
Dependent Claim 41 words
The method of claim 1 wherein said step of measuring the carrier concentration and profiling depth comprises placing the structure to be tested in a capacitance-voltage profiling apparatus, and obtaining said carrier concentration and profile depth measurements with said profiling apparatus.
Claim 4
Dependent Claim 61 words
The method of claim 2 wherein said step of measuring the pn junction intercept voltage comprises: applying a voltage across the pn semiconductor structure to be tested to reverse bias said structure; measuring the capacitance, C mea , across said structure; and, determining the pn junction intercept voltage of said structure from the values of said applied voltage and measured capacitance.
Claim 5
Dependent Claim 145 words
The method of claim 3 wherein the step of determining the actual carrier concentration and profile depth comprises: determining the Schottky capacitance, C Schottky , of said pn semiconductor structure from said determined pn junction capacitance, C pn , and said measured capacitance, C mea , across said structure using the equation: ##EQU24## determining the actual carrier concentration, N actual , from the measured carrier concentration, N mea , the measured capacitance across said structure, C mea , and the determined Schottky capacitance, C Schottky , from the equation: ##EQU25## determining the actual profile depth, X actual , from the measured profile depth, X mea , and the determined pn junction capacitance, C pn , using the equation: ##EQU26## where ε is the permittivity of the semiconductor structure and A is the area of a contact employed to apply voltage across said pn semiconductor structure.
Claim 6
Dependent Claim 38 words
The method of claim 1 further including the step of determining conduction and valence band discontinuities from said measured pn junction intercept voltage which exist at the pn junction interface if said pn semiconductor structure is a heterostructure.
Claim 7
Dependent Claim 62 words
The method of claim 3, wherein said step of applying a voltage across the pn semiconductor structure comprises engaging a first layer of said semiconductor structure with a first ohmic contact, and engaging a second layer of said semiconductor structure with a second ohmic contact; and applying a voltage across said first and second ohmic contacts to reverse bias said semiconductor structure.
Claim 8
Dependent Claim 33 words
The method of claim 6, further comprising the step of retracting said first ohmic contact away from said first layer to permit measurement of carrier concentration and profile depth of said semiconductor structure.
Claim 9
Dependent Claim 68 words
The method of claim 6, wherein said step of measuring the carrier concentration and profiling depth further comprises: exposing said first layer and said first ohmic contact to an electrolyte solution; applying a voltage to said electrolyte solution to thereby cause said solution to etch through said first ohmic contact and said semiconductor structure; and measuring the carrier concentration and profile depth as said semiconductor structure is etched.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-04-05 1996-10-05 1997-04-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-04-05 2000-10-05 2001-04-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-04-05 2004-10-05 2005-04-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag