← Back to Patent Explorer
US5587593A Expired / Lapsed US ⏱️ 0.0 years remaining

Light-emitting semiconductor device using group III nitrogen compound

Assignee: Japan Science and Technology Agency
•
Filing: 1995-04-19
•
Granted: 1996-12-24
•
Expires: 2015-04-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A light-emitting semiconductor device includes a sapphire substrate whose main surface orientation is tilted by 1 to 4 degrees from its axis "a" <1120>, and layers epitaxially formed thereon. Tilting the surface orientation of the sapphire substrate enables uniform doping of a p-type impurity into the layers epitaxially grown thereon. As a result, the luminous intensity of the light-emitting semiconductor device is improved.

Inventors

  • 👤 Norikatsu Koide
  • 👤 Shiro Yamazaki
  • 👤 Junichi Umezaki
  • 👤 Shinya Asami

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 22:25
CPC Classifications
H; H10; H10H; H10H20/00; H10H20/80; H10H20/81; H10H20/822; H10H20/824; H10H20/825; H10H20/8252; H10H20/817

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 94 words
A light-emitting semiconductor device comprising: a sapphire substrate; an n-layer with n-type conduction of group III nitride compound semiconductor satisfying the formula Al x Ga y In 1-x-y N, 0 ≦x≦1 0≦x≦1, and 0≦x+y≦1; a magnesium (Mg) doped p-layer with p-type conduction of group III nitride compound semiconductor satisfying the formula Al x Ga y In 1-x-y N, 0≦x≦1, 0≦y≦1, and 0≦x+y≦1; and wherein a plane orientation of said sapphire substrate is set at an off angle within the range of 1 to 4 degrees from an axis "a" <1120> of said sapphire substrate.
Claim 2
Dependent Claim 94 words
A light-emitting semiconductor device comprising: a sapphire substrate; an n-layer with n-type conduction of group III nitride compound semiconductor satisfying the formula Al x Ga y In 1-x-y N, 0 ≦x≦1 0≦x≦1, and 0≦x+y≦1; a magnesium (Mg) doped p-layer with p-type conduction of group III nitride compound semiconductor satisfying the formula Al x Ga y In 1-x-y N, 0≦x≦1, 0≦y≦1, and 0≦x+y≦1; and wherein a plane orientation of said sapphire substrate is set at an off angle within the range of 1 to 4 degrees from an axis "a" <1120> of said sapphire substrate.

References Cited (Backward Citations)

US4404265A Cited
US3969753A Cited
US4908074A Cited
US5006908A Cited
US5281830A Cited
US5237182A Cited
JPH04323880A Cited
DE4313798A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-12-24 2000-06-24 2000-12-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-12-24 2004-06-24 2004-12-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-12-24 2008-06-24 2008-12-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag