Abstract

Abstract A method for forming an oxide film in a semiconductor device comprises a pre-oxidation process, a main oxidation process and a post-oxidation process. N2O gas is used for the pre-oxidation process, a mixed gas of N2O gas and NH3 gas is used for the main oxidation process, and N2O gas is used for the post-oxidation process. The insulation characteristics of the oxide film are increased by introducing nitrogen, and amount of introduced nitrogen can be regulated by the controlling of amount of NH3 gas. Also, the problems encountered when NH3 gas and N2O gas are used separately for the oxidation process can be solved by using of the mixed gas of NH3 gas and N2O gas.

Inventors

  • 👤 Byung J. Cho

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 14:46
CPC Classifications
H; H10; H10P; H10P14/00; H10P14/60; H10P14/65; H10P14/6516; H10P14/6518; H10P14/6519; H10P14/63; H10P14/6302; H10P14/6304; H10P14/6306; H10P14/6529; H10P14/6322

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 67 words
A method for forming an oxide film in a semiconductor device comprising: a) initiating oxide film formation by introducing an nitrous oxide containing gas; b) controlling the oxidation rate and influx of nitrogen by introducing ammonia into said nitrous oxide containing gas; and c) halting the introducing of ammonia gas while maintaining the flow of nitrous oxide containing gas until formation of said oxide film is complete.
Claim 2
Independent Claim 67 words
A method for forming an oxide film in a semiconductor device comprising: a) initiating oxide film formation by introducing an nitrous oxide containing gas; b) controlling the oxidation rate and influx of nitrogen by introducing ammonia into said nitrous oxide containing gas; and c) halting the introducing of ammonia gas while maintaining the flow of nitrous oxide containing gas until formation of said oxide film is complete.

References Cited (Backward Citations)

US3422321A Cited
US4532022A Cited
US4581622A Cited
US4363868A Cited
US4438157A Cited
US4543707A Cited
US5403786A Cited
US4960727A Cited
US5338954A Cited
US5264396A Cited
US5296411A Cited
US5397720A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-07-30 2000-01-29 2000-07-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-07-30 2004-01-29 2004-07-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-07-30 2008-01-29 2008-07-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag