Abstract

Abstract A scratch reducing shadow mask for providing vapor deposition patterns of bonding metals onto a surface of a die. The shadow mask comprises a top surface and a bottom surface which define a plurality of vias for permitting vaporized bonding metals to pass through the mask. Mask bottom surface comprises a plurality of recessed regions to minimize the contact area of the mask with the die during the vapor deposition process.

Inventors

  • 👤 Thomas J. Dunaway
  • 👤 Richard K. Spielberger

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 17:58
CPC Classifications
H; H10; H10P; H10P72/00; H10P72/04; H10P72/0402; Y; Y10; Y10S; Y10S438/00; Y10S438/942; Y10S438/944

Claims Analysis

Total Claims: 18
Claim 1
Independent Claim 246 words
A method of manufacturing a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, comprising: a) providing a shadow mask having a top surface and a bottom surface; b) obtaining and transferring applicable dimensions of the semiconductor die to the shadow mask in order to define a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; and c) obtaining and transferring applicable dimensions of the semiconductor die in order to form the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the forming step comprising forming the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process.
Claim 2
Independent Claim 246 words
A method of manufacturing a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, comprising: a) providing a shadow mask having a top surface and a bottom surface; b) obtaining and transferring applicable dimensions of the semiconductor die to the shadow mask in order to define a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; and c) obtaining and transferring applicable dimensions of the semiconductor die in order to form the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the forming step comprising forming the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process.
Claim 3
Dependent Claim 11 words
The method of claim 1 wherein the forming step comprises etching.
Claim 4
Dependent Claim 24 words
The method of claim 1 wherein the forming step comprises providing projections extending annularly from the vias at the bottom surface of the mask.
Claim 5
Dependent Claim 11 words
The method of claim 3 wherein the forming step comprises etching.
Claim 6
Dependent Claim 19 words
The method of claim 1 wherein the providing step comprises providing a mask formed of a material comprising molybdenum.
Claim 7
Independent Claim 250 words
A method of manufacturing a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, comprising: a) providing a shadow mask having a top surface and a bottom surface; b) obtaining and transferring applicable dimensions of the semiconductor die to the shadow mask in order to define a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; and c) obtaining and transferring applicable dimensions of the semiconductor die to the shadow mask in order to etch the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the etching step comprising etching the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process.
Claim 8
Independent Claim 250 words
A method of manufacturing a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, comprising: a) providing a shadow mask having a top surface and a bottom surface; b) obtaining and transferring applicable dimensions of the semiconductor die to the shadow mask in order to define a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; and c) obtaining and transferring applicable dimensions of the semiconductor die to the shadow mask in order to etch the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the etching step comprising etching the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process.
Claim 9
Dependent Claim 19 words
The method of claim 6 wherein the providing step comprises providing a mask formed of a material comprising molybdenum.
Claim 10
Independent Claim 288 words
A method of manufacturing and using a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, the method comprising: (a) providing a shadow mask having a top surface and a bottom surface; (b) defining a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; (c) forming the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the forming step comprising forming the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process; (d) positioning the mask over the die so that the plurality of vias are aligned with the input/output interconnect locations of the die and so that the recessed regions are located over the active regions of the die; (e) causing a vaporized bonding metal to pass through the vias and deposit onto the input/output interconnect locations of the die; and (f) removing the mask from the die.
Claim 11
Independent Claim 288 words
A method of manufacturing and using a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, the method comprising: (a) providing a shadow mask having a top surface and a bottom surface; (b) defining a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; (c) forming the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the forming step comprising forming the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process; (d) positioning the mask over the die so that the plurality of vias are aligned with the input/output interconnect locations of the die and so that the recessed regions are located over the active regions of the die; (e) causing a vaporized bonding metal to pass through the vias and deposit onto the input/output interconnect locations of the die; and (f) removing the mask from the die.
Claim 12
Dependent Claim 11 words
The method of claim 8 wherein the forming step comprises etching.
Claim 13
Dependent Claim 24 words
The method of claim 8 wherein the forming step comprises providing projections extending annularly from the vias at the bottom surface of the mask.
Claim 14
Dependent Claim 11 words
The method of claim 10 wherein the forming step comprises etching.
Claim 15
Dependent Claim 19 words
The method of claim 8 wherein the providing step comprises providing a mask formed of a material comprising molybdenum.
Claim 16
Independent Claim 288 words
A method of manufacturing and using a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, the method comprising: (a) providing a shadow mask having a top surface and a bottom surface; (b) defining a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; (c) etching the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the etching step comprising etching the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process; (d) positioning the mask over the die so that the plurality of vias are aligned with the input/output interconnect locations of the die and so that the recessed regions are located over the active regions of the die; (e) causing a vaporized bonding metal to pass through the vias and deposit onto the input/output interconnect locations of the die; and (f) removing the mask from the die.
Claim 17
Independent Claim 288 words
A method of manufacturing and using a yield-enhancing shadow mask for providing vapor deposition patterns of bonding metals onto input/output interconnect locations of a semiconductor die while preventing damage to active regions of the die, the method comprising: (a) providing a shadow mask having a top surface and a bottom surface; (b) defining a plurality of vias in the shadow mask located in alignment with the input/output interconnect locations of the die for permitting vaporized bonding metals to pass through the mask and deposit onto the input/output interconnect locations; (c) etching the mask bottom surface so that it comprises a plurality of recessed regions which minimize the contact area of the mask with the die during the process of vapor deposition, the recessed regions being formed so that they surround substantially full-mask-thickness walls which define the vias aligned with the input/output interconnect locations of the die and which provide damming action to retain the vapor deposit to within a limited distance of the input/output interconnect locations of the die as defined by the vias, the etching step comprising etching the recessed regions in the mask so that they are formed over active regions of the die in order to avoid damage to the active regions from contact with the mask, thus increasing the yield of reliable die during the production process; (d) positioning the mask over the die so that the plurality of vias are aligned with the input/output interconnect locations of the die and so that the recessed regions are located over the active regions of the die; (e) causing a vaporized bonding metal to pass through the vias and deposit onto the input/output interconnect locations of the die; and (f) removing the mask from the die.
Claim 18
Dependent Claim 19 words
The method of claim 13 wherein the providing step comprises providing a mask formed of a material comprising molybdenum.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-08-18 1996-02-17 1996-08-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-08-18 2000-02-17 2000-08-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-08-18 2004-02-17 2004-08-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag