Abstract
Abstract A method of modifying the reflectivity and emissivity of a surface of a material comprises the steps of irradiating the surface with a beam of coherent pulsed radiation at a power sufficient to generate a surface plasma and scanning said beam across said surface. Successive pulses of radiation are caused to overlap and chemical change at the surface is promoted by provision of a localized atmosphere. The surface produced has features on a scale of less than 50 microns and is restricted to a depth of less than 10-3 cm. The body of the material is not affected.
Inventors
- 👤 Walter W. Duley
- 👤 Grant Kinsman
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-30 08:32
CPC Classifications
C; C21; C21D; C21D1/00; C21D1/06; C21D1/09; B; B23; B23K; B23K26/00; B23K26/12; B23K26/123; B23K26/352; B23K26/356; B23K35/00; B23K35/22; B23K35/38; B41; B41M; B41M5/00; B41M5/26; B41M5/262
Claims Analysis
Total Claims: 20
Claim 1
Independent Claim
88 words
A method of modifying the reflectivity of a surface of a material comprising the steps of: irradiating the surface with a beam of coherent pulsed radiation, said pulsed radiation being at a power level sufficient to melt the surface and thereby to generate a surface plasma so that the shock wave associated with the surface plasma produces a roughening of said surface; and repeatedly scanning said beam across said surface to form successive closely spaced lines on said surface as a result of said roughening of said surface.
Claim 2
Independent Claim
88 words
A method of modifying the reflectivity of a surface of a material comprising the steps of: irradiating the surface with a beam of coherent pulsed radiation, said pulsed radiation being at a power level sufficient to melt the surface and thereby to generate a surface plasma so that the shock wave associated with the surface plasma produces a roughening of said surface; and repeatedly scanning said beam across said surface to form successive closely spaced lines on said surface as a result of said roughening of said surface.
Claim 3
Dependent Claim
16 words
A method according to claim 1 including the step of promoting chemical change at said surface.
Claim 4
Dependent Claim
20 words
A method according to claim 2 wherein the chemical change is promoted by providing a localised atmosphere at said surface.
Claim 5
Dependent Claim
19 words
A method according to claim 3 wherein said localised atmosphere is selected from the group comprising oxygen and nitrogen.
Claim 6
Dependent Claim
26 words
A method according to claim 1 wherein said beam scans said surface at a rate to cause successive pulses of radiation to overlap on said surface.
Claim 7
Dependent Claim
17 words
A method according to claim 1 wherein said beam is inclined to the surface of the material.
Claim 8
Dependent Claim
23 words
A method according to claim 6 wherein said beam scans said surface at a rate to cause successive pulses of radiation to overlap.
Claim 9
Independent Claim
116 words
A method of reducing the average reflectivity of a surface of a material comprising the steps of: irradiating said surface with a beam of coherent pulsed radiation, said pulsed radiation being at a power level sufficient to melt the surface and thereby to generate a surface plasma so that the shock wave associated with the surface plasma produces a roughening of said surface; and repeatedly scanning said beam across selected areas of said surface to form successive closely spaced lines on said selected areas of said surface thereby to reduce the reflectivity of said selected areas, the average reflectivity thereby being reduced as a function of the reflectivity and the surface area of the selected areas.
Claim 10
Independent Claim
116 words
A method of reducing the average reflectivity of a surface of a material comprising the steps of: irradiating said surface with a beam of coherent pulsed radiation, said pulsed radiation being at a power level sufficient to melt the surface and thereby to generate a surface plasma so that the shock wave associated with the surface plasma produces a roughening of said surface; and repeatedly scanning said beam across selected areas of said surface to form successive closely spaced lines on said selected areas of said surface thereby to reduce the reflectivity of said selected areas, the average reflectivity thereby being reduced as a function of the reflectivity and the surface area of the selected areas.
Claim 11
Dependent Claim
19 words
A method according to claim 8 wherein said selected areas are arranged in a random pattern on said surface.
Claim 12
Dependent Claim
16 words
A method according to claim 8 including the step of promoting chemical change at said surface.
Claim 13
Dependent Claim
20 words
A method according to claim 10 wherein the chemical change is promoted by providing a localised atmosphere at said surface.
Claim 14
Dependent Claim
19 words
A method according to claim 11 wherein said localised atmosphere is selected from the group comprising oxygen and nitrogen.
Claim 15
Dependent Claim
26 words
A method according to claim 8 wherein said beam scans said surface at a rate to cause successive pulses of radiation to overlap on said surface.
Claim 16
Dependent Claim
17 words
A method according to claim 8 wherein said beam is inclined to the surface of the material.
Claim 17
Dependent Claim
23 words
A method according to claim 14 wherein said beam scans said surface at a rate to cause successive pulses of radiation to overlap.
Claim 18
Independent Claim
114 words
A method of changing the signature of a surface when interrogated by laser radiation comprising the steps of treating selected areas of said surface to reduce the reflectivity of said selected areas wherein the reflectivity of said selected areas is reduced by irradiating the surface with a beam of coherent pulsed radiation, said radiation being at a power level sufficient to melt the surface and thereby to generate a surface plasma so that the shock wave associated with the surface plasma produces a roughening of said surface and repeatedly scanning said beam across said selected areas to form successive closely spaced lines on said surface as a result of said roughening of said surface.
Claim 19
Independent Claim
114 words
A method of changing the signature of a surface when interrogated by laser radiation comprising the steps of treating selected areas of said surface to reduce the reflectivity of said selected areas wherein the reflectivity of said selected areas is reduced by irradiating the surface with a beam of coherent pulsed radiation, said radiation being at a power level sufficient to melt the surface and thereby to generate a surface plasma so that the shock wave associated with the surface plasma produces a roughening of said surface and repeatedly scanning said beam across said selected areas to form successive closely spaced lines on said surface as a result of said roughening of said surface.
Claim 20
Dependent Claim
19 words
A method according to claim 16 wherein said selected areas are arranged to alter the silhouette of said surface.
References Cited (Backward Citations)
US3003493A
Cited
US3112114A
Cited
US3229095A
Cited
US3357319A
Cited
US3473000A
Cited
US3569660A
Cited
US3604890A
Cited
US3832948A
Cited
US3700850A
Cited
US3663793A
Cited
US4108659A
Cited
US3935419A
Cited
US3932726A
Cited
US4288528A
Cited
US4214249A
Cited
US3965327A
Cited
US3945825A
Cited
JPS5150851A
Cited
US4028523A
Cited
US4160894A
Cited
US4087672A
Cited
US4045318A
Cited
US4117177A
Cited
US4139409A
Cited
US4152575A
Cited
US4200875A
Cited
GB2045669A
Cited
EP0036680A1
Cited
US4395616A
Cited
US4408602A
Cited
JPS57169612A
Cited
US4377735A
Cited
US4377736A
Cited
US4412231A
Cited
US4454179A
Cited
US4600686A
Cited
US4417948A
Cited
US4500771A
Cited
US4535218A
Cited
US4578329A
Cited
US4414059A
Cited
US4535998A
Cited
US4547649A
Cited
DE3425263A1
Cited
DE3411797A1
Cited
US4634645A
Cited
US4656079A
Cited
US4670639A
Cited
US4707584A
Cited
JPS62214142A
Cited
US4769257A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-11-19 | 1994-05-21 | 1994-11-20 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-11-19 | 1998-05-21 | 1998-11-20 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-11-19 | 2002-05-21 | 2002-11-20 | $7700.00 | Window Closed / Lapsed |