Process of using photoresist treating composition containing a mixture of a hexa-alkyl disilazane, propylene glycol alkyl ether and propylene glycol alkyl ether acetate
Assignee: Clariant Finance BVI Ltd
•
Filing: 1985-10-28
•
Granted: 1987-09-08
•
Expires: 2005-10-28
Abstract
Abstract The invention provides a composition which comprises from about 3 to about 50% by weight of a hexa-alkyl disilazane and a solvent composition which comprises one or more compounds selected from the group consisting of a propylene glycol alkyl ether and a propylene glycol alkyl ether acetate.
Inventors
- 👤 Dana Durham
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 07:02
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/26; G03F7/42; G03F7/422; G03F7/004; G03F7/022; G03F7/0226; G03F7/075; G03F7/0751
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
105 words
A method of treating a photoresist coating on a substrate, which photoresist comprises a resin selected from the group consisting of novolaks and paravinyl phenols, and at least one o-quinone diazide photosensitizer, which method comprises contacting said photoresist coating for sufficient time to strip, thin, clean or promote adhesion of the coating with a mixture which comprises from about 3 to about 50% by weight of the mixture of a hexa-alkyl disilazane and from about 50 to about 97% by weight of the mixture of a solvent composition which comprises both a propylene glycol mono alkyl ether and a propylene glycol mono alkyl ether acetate.
Claim 2
Independent Claim
105 words
A method of treating a photoresist coating on a substrate, which photoresist comprises a resin selected from the group consisting of novolaks and paravinyl phenols, and at least one o-quinone diazide photosensitizer, which method comprises contacting said photoresist coating for sufficient time to strip, thin, clean or promote adhesion of the coating with a mixture which comprises from about 3 to about 50% by weight of the mixture of a hexa-alkyl disilazane and from about 50 to about 97% by weight of the mixture of a solvent composition which comprises both a propylene glycol mono alkyl ether and a propylene glycol mono alkyl ether acetate.
Claim 3
Dependent Claim
13 words
The method of claim 1 wherein said ether is propylene glycol mono-methyl ether.
Claim 4
Dependent Claim
14 words
The method of claim 1 wherein said acetate is propylene glycol mono-methyl ether acetate.
Claim 5
Independent Claim
99 words
A method for stripping a photoresist coating from a substrate, which photoresist comprises a resin selected from the group consisting of novolaks and paravinyl phenols, and at least one o-quinone diazide, said method comprising contacting said photoresist coating with a stripping composition for sufficient time to strip photoresist coating from the substrate which comprises from about 3 to about 50% by weight of the composition of a hexa-alkyl disilazane and from about 50 to about 97% by weight of the composition of a solvent composition comprises both a propylene glycol mono-alkyl ether and a propylene glycol mono-alkyl ether acetate.
Claim 6
Independent Claim
99 words
A method for stripping a photoresist coating from a substrate, which photoresist comprises a resin selected from the group consisting of novolaks and paravinyl phenols, and at least one o-quinone diazide, said method comprising contacting said photoresist coating with a stripping composition for sufficient time to strip photoresist coating from the substrate which comprises from about 3 to about 50% by weight of the composition of a hexa-alkyl disilazane and from about 50 to about 97% by weight of the composition of a solvent composition comprises both a propylene glycol mono-alkyl ether and a propylene glycol mono-alkyl ether acetate.
Claim 7
Dependent Claim
28 words
The method of claim 1 wherein both ether and acetate are present and wherein the ratio of ether to acetate is in the range of from about 10:1-1:10.
Claim 8
Dependent Claim
23 words
The method of claim 1 wherein both ether and acetate are present and wherein the ratio of ether to acetate is about 1:1.
References Cited (Backward Citations)
US3228768A
Cited
US3520683A
Cited
US3882038A
Cited
US3549368A
Cited
US3933517A
Cited
US3666473A
Cited
US3869292A
Cited
US3868254A
Cited
US3859099A
Cited
US4411983A
Cited
US4308368A
Cited
US4416976A
Cited
US4378423A
Cited
US4381340A
Cited
US4460674A
Cited
US4355094A
Cited
US4409317A
Cited
US4351895A
Cited
US4397937A
Cited
US4439516A
Cited
US4403029A
Cited
US4482661A
Cited
US4550069A
Cited
US4592787A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1990-09-07 | 1991-03-09 | 1991-09-08 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1994-09-07 | 1995-03-09 | 1995-09-08 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1998-09-07 | 1999-03-09 | 1999-09-08 | $7700.00 | Window Closed / Lapsed |