Insulation layer structure and method for making the same

Assignee: SK Hynix Inc
•
Filing: 1998-11-19
•
Granted: 2000-11-21
•
Expires: 2018-11-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A dual thickness gate insulation layer, for use with, e.g., a dual gate MOSFET (Metal Oxide Semiconductor Field Effect Transistor), is formed using a more simplified method and improves the reliability. An impurity layer is formed in the semiconductor substrate, and the impurity layer includes a first portion and a second portion. An insulation layer is grown in the semiconductor substrate, and the insulation layer includes a first layer and a second layer which are different from each other in thickness. The present invention simplifies the insulation layer fabricating steps and improves product reliability.

Inventors

  • 👤 Yun-Jun Huh
  • 👤 Nam-Hoon Cho

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:01
CPC Classifications
H; H10; H10P; H10P10/00; H10D; H10D84/00; H10D84/01; H10D84/0123; H10D84/0126; H10D84/0144; H10D84/02; H10D84/03; H10D84/038; Y; Y10; Y10S; Y10S148/00; Y10S148/043; Y10S148/163; Y10S438/00; Y10S438/981

Claims Analysis

Total Claims: 29
Claim 1
Independent Claim 120 words
A method of making a dual thickness insulation layer structure, comprising the steps of: forming an impurity layer in a substrate, the impurity layer including a first portion having a first amount of an impurity and a second portion having a second amount of the impurity, the first and second portions being formed simultaneously; and growing an insulation layer in the substrate, the insulation layer including a first layer and a second layer formed beneath the first portion and the second portion, respectively, wherein the first layer and the second layer are grown at different growth rates due to the first and second amounts of the impurity such that the first and second layers differ from each other in thickness.
Claim 2
Independent Claim 120 words
A method of making a dual thickness insulation layer structure, comprising the steps of: forming an impurity layer in a substrate, the impurity layer including a first portion having a first amount of an impurity and a second portion having a second amount of the impurity, the first and second portions being formed simultaneously; and growing an insulation layer in the substrate, the insulation layer including a first layer and a second layer formed beneath the first portion and the second portion, respectively, wherein the first layer and the second layer are grown at different growth rates due to the first and second amounts of the impurity such that the first and second layers differ from each other in thickness.
Claim 3
Dependent Claim 17 words
The method of claim 1, wherein the impurity layer delays a growth rate of the insulation layer.
Claim 4
Dependent Claim 64 words
The method of claim 1, wherein the forming step comprises the steps of: forming a pad layer on the substrate, the pad layer including a first pad portion and a second pad portion; annealing, under an atmosphere of an impurity gas, the pad layer and the substrate to form the impurity layer between the pad layer and the substrate; and removing the pad layer.
Claim 5
Dependent Claim 24 words
The method of claim 3, wherein the impurity gas is a nitrous gas selected from the group consisting of N 2 O and NO.
Claim 6
Dependent Claim 13 words
The method of claim 1, wherein the insulation layer comprises an oxide layer.
Claim 7
Dependent Claim 23 words
The method of claim 1, wherein the first portion of the impurity layer is thinner than the second portion of the impurity layer.
Claim 8
Dependent Claim 41 words
The method of claim 6, wherein the first layer of the insulation layer corresponding to the first portion of the impurity layer is thicker than the second layer of the insulation layer corresponding to the second portion of the impurity layer.
Claim 9
Dependent Claim 43 words
The method of claim 3, wherein the first pad portion of the pad layer is initially formed on the semiconductor substrate, and the first pad portion of the pad layer is selectively etched to form the second pad portion of the pad layer.
Claim 10
Dependent Claim 15 words
The method of claim 1, wherein the first amount is less than the second amount.
Claim 11
Dependent Claim 23 words
The method of claim 8, wherein a thickness of the second pad portion is less than a thickness of the first pad portion.
Claim 12
Dependent Claim 27 words
The method of claim 1, wherein the growing step includes simultaneously growing the first layer and the second layer of the insulation layer at different growth rates.
Claim 13
Independent Claim 145 words
A method of making a dual thickness insulation layer structure, comprising: forming a pad layer on a substrate, the pad layer including a first pad portion and a second pad portion; annealing, under an atmosphere of an impurity gas, the pad layer and the substrate to form an impurity layer between the pad layer and the substrate, wherein the impurity layer includes a first portion having a first amount of an impurity and a second portion having a second amount of the impurity, and the first amount of the impurity is less than the second amount of impurity; removing the pad layer; and growing an insulation layer in the substrate, the insulation layer including a first layer and a second layer formed beneath the first portion and the second portion, respectively, wherein the first layer and the second layer differ from each other in thickness.
Claim 14
Independent Claim 145 words
A method of making a dual thickness insulation layer structure, comprising: forming a pad layer on a substrate, the pad layer including a first pad portion and a second pad portion; annealing, under an atmosphere of an impurity gas, the pad layer and the substrate to form an impurity layer between the pad layer and the substrate, wherein the impurity layer includes a first portion having a first amount of an impurity and a second portion having a second amount of the impurity, and the first amount of the impurity is less than the second amount of impurity; removing the pad layer; and growing an insulation layer in the substrate, the insulation layer including a first layer and a second layer formed beneath the first portion and the second portion, respectively, wherein the first layer and the second layer differ from each other in thickness.
Claim 15
Dependent Claim 17 words
The method of claim 12, wherein the impurity layer delays a growth rate of the insulation layer.
Claim 16
Dependent Claim 24 words
The method of claim 12, wherein the impurity gas is a nitrous gas selected from the group consisting of N 2 O and NO.
Claim 17
Dependent Claim 13 words
The method of claim 12, wherein the insulation layer comprises an oxide layer.
Claim 18
Dependent Claim 23 words
The method of claim 12, wherein the first portion of the impurity layer is thinner than the second portion of the impurity layer.
Claim 19
Dependent Claim 41 words
The method of claim 12, wherein the first layer of the insulation layer corresponding to the first portion of the impurity layer is thicker than the second layer of the insulation layer corresponding to the second portion of the impurity layer.
Claim 20
Dependent Claim 43 words
The method of claim 12, wherein the first pad portion of the pad layer is initially formed on the semiconductor substrate, and the first pad portion of the pad layer is selectively etched to form the second pad portion of the pad layer.
Claim 21
Dependent Claim 28 words
The method of claim 12, wherein the first pad portion has a first thickness, and the second pad portion has a second thickness less than the first thickness.
Claim 22
Dependent Claim 32 words
The method of claim 12, wherein the step of forming the impurity layer includes simultaneously forming the first portion and the second portion of the impurity layer in a single growth step.
Claim 23
Dependent Claim 27 words
The method of claim 12, wherein the growing step includes simultaneously growing the first layer and the second layer of the insulation layer at different growth rates.
Claim 24
Independent Claim 137 words
A method of forming a dual thickness insulation layer structure, comprising the steps of: forming an impurity layer in a substrate, the impurity layer including a first portion having a first amount of an impurity and a second portion having a second amount of the impurity, wherein the first portion of the impurity layer is thinner than the second portion of the impurity layer; and growing an insulation layer in the substrate, the insulation layer including a first portion and a second portion, wherein the first and second portions of the insulation layer are located beneath the first and second portions of the impurity layer, respectively, and wherein the first and second portions of the insulation layer are grown at different growth rates, such that the first and second portions of the insulation layer have different thicknesses.
Claim 25
Independent Claim 137 words
A method of forming a dual thickness insulation layer structure, comprising the steps of: forming an impurity layer in a substrate, the impurity layer including a first portion having a first amount of an impurity and a second portion having a second amount of the impurity, wherein the first portion of the impurity layer is thinner than the second portion of the impurity layer; and growing an insulation layer in the substrate, the insulation layer including a first portion and a second portion, wherein the first and second portions of the insulation layer are located beneath the first and second portions of the impurity layer, respectively, and wherein the first and second portions of the insulation layer are grown at different growth rates, such that the first and second portions of the insulation layer have different thicknesses.
Claim 26
Dependent Claim 18 words
The method of claim 22, wherein the first and second portions of the impurity layer are formed simultaneously.
Claim 27
Dependent Claim 23 words
The method of claim 22, wherein the first portion of the insulation layer is thicker than the second portion of the insulation layer.
Claim 28
Dependent Claim 37 words
The method of claim 22, wherein the step of forming the impurity layer comprises performing an annealing step in an impurity gas atmosphere such that the first and second portions of the impurity layer are formed simultaneously.
Claim 29
Dependent Claim 59 words
The method of claim 22, wherein the step of forming the impurity layer comprises the steps of: forming a pad layer on the substrate, the pad layer including a first pad portion and a second pad portion; annealing the pad layer and the substrate in an impurity gas atmosphere to form the impurity layer; and removing the pad layer.

References Cited (Backward Citations)

US4151010A Cited
US4651406A Cited
US4851370A Cited
US5497021A Cited
US5360769A Cited
US5881085A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2003-11-21 2004-05-22 2004-11-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2007-11-21 2008-05-22 2008-11-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2011-11-21 2012-05-22 2012-11-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag