← Back to Patent Explorer
US5272735A Expired / Lapsed US ⏱️ 0.0 years remaining

Sputtering process burnable poison coating

Assignee: Combustion Engineering Inc
•
Filing: 1992-08-03
•
Granted: 1993-12-21
•
Expires: 2012-08-03
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for sputtering coating the inside surface of a fuel assembly tubular component (10,200,400,700) with absorber material such as a burnable poison or getter. The steps include supporting the e.g., cladding tube (10) in a fixture (12,14) and supporting a source tube (100) of e.g., burnable poison material coaxially within the cladding tube, thereby defining a cylindrical annulus (24) between the tubes. The annular space is evacuated and backfilled with an inert working gas (26) such as argon, to a pressure sufficient to sustain a plasma discharge. The cladding tube is positively biased (36) as an anode, and the source tube is negatively biased (34) as a cathode, such that a plasma of the working gas is established in the annular space. A circumferential magnetic field is generated around the source tube to confine and shape the plasma whereby the source tube is bombarded with ions from the plasma substantially uniformly over the length of the source tube. Burnable poison material is thereby sputtered substantially uniformly from the source tube onto the inside surface of the cladding tube, to form a burnable poison coating thereon.

Inventors

  • 👤 William J. Bryan
  • 👤 Patrick A. Perrotti

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 04:07
CPC Classifications
G; G21; G21C; G21C3/00; G21C3/02; G21C3/04; G21C3/16; G21C3/20; C; C23; C23C; C23C14/00; C23C14/04; C23C14/046; C23C14/22; C23C14/34; C23C14/35; H; H01; H01J; H01J37/00; H01J37/32; H01J37/34; H01J37/3402; H01J2237/00; H01J2237/16; H01J2237/162; Y; Y02; Y02E; Y02E30/00; Y02E30/30

Claims Analysis

Total Claims: 25
Claim 1
Independent Claim 160 words
A method for coating the inside surface of a nuclear fuel assembly tubular component with an absorptive material, comprising: supporting the component tube in a fixture; supporting a source tube of absorptive material coaxially within the component tube, thereby defining a cylindrical annular space between the tubes; evacuating the annular space and backfilling the annular space with an inert working gas to a pressure sufficient to sustain a plasma discharge; connecting a power supply to the component tube with a positive bias as an anode and to the source tube with a negative bias as a cathode, such that a plasma of the working gas is established in the annular space; establishing a circumferential magnetic field around the source tube to confine and shape the plasma; whereby the source tube is bombarded with ions from the plasma and absorptive material is thereby sputtered from the source tube onto the inside surface of the component tube to form a coating thereon.
Claim 2
Independent Claim 160 words
A method for coating the inside surface of a nuclear fuel assembly tubular component with an absorptive material, comprising: supporting the component tube in a fixture; supporting a source tube of absorptive material coaxially within the component tube, thereby defining a cylindrical annular space between the tubes; evacuating the annular space and backfilling the annular space with an inert working gas to a pressure sufficient to sustain a plasma discharge; connecting a power supply to the component tube with a positive bias as an anode and to the source tube with a negative bias as a cathode, such that a plasma of the working gas is established in the annular space; establishing a circumferential magnetic field around the source tube to confine and shape the plasma; whereby the source tube is bombarded with ions from the plasma and absorptive material is thereby sputtered from the source tube onto the inside surface of the component tube to form a coating thereon.
Claim 3
Dependent Claim 49 words
The method of claim 1, wherein the component tube has a length of at least about 12 ft and the source tube spans the length of the cladding tube; and the absorptive material is sputtered along at least about 10 ft of the length of the component tube simultaneously.
Claim 4
Dependent Claim 39 words
The method of claim 2, wherein the source tube has a prescribed non-homogenous distribution of absorptive material along its length, and the absorptive material is sputtered simultaneously onto the component tube in a prescribed, non-homogeneous distribution along its length.
Claim 5
Dependent Claim 42 words
The method of claim 3, wherein the non-homogeneous distribution on the source tube includes at least two regions of the source tube surface having a respective two different materials selected from the group consisting of gadolinium-bearing material, erbium-bearing material, and boron-bearing material.
Claim 6
Dependent Claim 62 words
The method of claim 1, wherein a first burnable poison absorptive material from a first source tube is sputtered onto the component tube, to form a first coating; the first coating is then positioned coaxially around a second source tube of a second burnable poison absorptive material, and the second material is sputtered onto the first coating to form a second coating.
Claim 7
Dependent Claim 61 words
The method of claim 1, wherein a first burnable absorptive poison material from a first source tube is sputtered onto a first longitudinal portion of the component tube to form a first coating; and a second burnable poison absorptive material from a second source tube is sputtered onto a second longitudinal portion of the component tube to form a second coating.
Claim 8
Independent Claim 41 words
The method of 1, wherein the step of backfilling includes backfilling with a reactant gas which in the presence of the plasma and the sputtered absorptive material, chemically reacts with the sputtered material to form a coating on the component tube.
Claim 9
Independent Claim 41 words
The method of 1, wherein the step of backfilling includes backfilling with a reactant gas which in the presence of the plasma and the sputtered absorptive material, chemically reacts with the sputtered material to form a coating on the component tube.
Claim 10
Independent Claim 164 words
A method for coating the inside surface of a zircaloy fuel rod cladding tube with burnable poison material, comprising: supporting the cladding tube in a fixture; supporting a source tube of burnable poison material coaxially within the cladding tube, thereby defining a cylindrical annular space between the tubes; evacuating the annular space and backfilling the annular space with an inert working gas to a pressure sufficient to sustain a plasma discharge; connecting a power supply to the cladding tube with a positive bias as an anode and to the source tube with a negative bias as a cathode, such that a plasma of the working gas is established in the annular space; establishing a circumferential magnetic field around the source tube to confine and shape the plasma; whereby the source tube is bombarded with ions from the plasma and burnable poison material is thereby sputtered from the source tube onto the inside surface of the cladding tube to form a burnable poison coating thereon.
Claim 11
Independent Claim 164 words
A method for coating the inside surface of a zircaloy fuel rod cladding tube with burnable poison material, comprising: supporting the cladding tube in a fixture; supporting a source tube of burnable poison material coaxially within the cladding tube, thereby defining a cylindrical annular space between the tubes; evacuating the annular space and backfilling the annular space with an inert working gas to a pressure sufficient to sustain a plasma discharge; connecting a power supply to the cladding tube with a positive bias as an anode and to the source tube with a negative bias as a cathode, such that a plasma of the working gas is established in the annular space; establishing a circumferential magnetic field around the source tube to confine and shape the plasma; whereby the source tube is bombarded with ions from the plasma and burnable poison material is thereby sputtered from the source tube onto the inside surface of the cladding tube to form a burnable poison coating thereon.
Claim 12
Dependent Claim 50 words
The method of claim 8, wherein the cladding tube has a length of at least about 12 ft and the source tube spans the length of the cladding tube; and the burnable poison material is sputtered along at least about 10 ft of the length of the cladding tube simultaneously.
Claim 13
Dependent Claim 13 words
The method of claim 8, wherein the burnable poison is in metallic form.
Claim 14
Dependent Claim 13 words
The method of claim 8, wherein the burnable poison is in ceramic form.
Claim 15
Dependent Claim 15 words
The method of claim 10, wherein the burnable poison material includes the elemental isotope boron-10.
Claim 16
Dependent Claim 13 words
The method of claim 10, wherein the burnable poison material is natural boron.
Claim 17
Dependent Claim 16 words
The method of claim 11, wherein the burnable poison material is zirconium diboride enriched with boron-10.
Claim 18
Dependent Claim 40 words
The method of claim 9, wherein the source tube has a prescribed non-homogenous distribution of burnable poison material along its length, and the burnable poison is sputtered simultaneously onto the cladding tube in a prescribed, non-homogeneous distribution along its length.
Claim 19
Dependent Claim 42 words
The method of claim 15, wherein the non-homogeneous distribution on the source tube includes at least two regions of the source tube surface having a respective two different materials selected from the group consisting of gadolinium-bearing material, erbium-bearing material, and boron-bearing material.
Claim 20
Dependent Claim 60 words
The method of claim 8, wherein a first burnable poison material from a first source tube is sputtered onto the cladding tube, to form a first coating; the first coating is then positioned coaxially around a second source tube of a second burnable poison material, and the second material is sputtered onto the first coating to form a second coating.
Claim 21
Dependent Claim 59 words
The method of claim 8, wherein a first burnable poison material from a first source tube is sputtered onto a first longitudinal portion of the cladding tube to form a first coating; and a second burnable poison material from a second source tube is sputtered onto a second longitudinal portion of the cladding tube to form a second coating.
Claim 22
Dependent Claim 21 words
The method of claim 8, wherein the burnable poison material is sputtered over a limited axial portion of the cladding tube.
Claim 23
Independent Claim 161 words
A method for coating the inside surface of a zircaloy fuel rod cladding tube with getter material, comprising: supporting the cladding tube in a fixture; supporting a source tube of getter material coaxially within the cladding tube, thereby defining a cylindrical annular shape between the tubes; evacuating the annular space and backfilling the annular space with an inert working gas to a pressure sufficient to sustain a plasma discharge; connecting a power supply to the cladding tube with a positive bias as an anode and to the source tube with a negative bias as a cathode, such that a plasma of the working gas is established in the annular space; establishing a circumferential magnetic field around the source tube to confine and shape the plasma; whereby the source tube is bombarded with ions from the plasma and getter material is thereby sputtered from the source tube onto the inside surface of the cladding tube to form a getter material coating thereon.
Claim 24
Independent Claim 161 words
A method for coating the inside surface of a zircaloy fuel rod cladding tube with getter material, comprising: supporting the cladding tube in a fixture; supporting a source tube of getter material coaxially within the cladding tube, thereby defining a cylindrical annular shape between the tubes; evacuating the annular space and backfilling the annular space with an inert working gas to a pressure sufficient to sustain a plasma discharge; connecting a power supply to the cladding tube with a positive bias as an anode and to the source tube with a negative bias as a cathode, such that a plasma of the working gas is established in the annular space; establishing a circumferential magnetic field around the source tube to confine and shape the plasma; whereby the source tube is bombarded with ions from the plasma and getter material is thereby sputtered from the source tube onto the inside surface of the cladding tube to form a getter material coating thereon.
Claim 25
Dependent Claim 20 words
The method of claim 20, wherein the getter material is sputtered over a limited axial portion of the cladding tube.

References Cited (Backward Citations)

US4407713A Cited
US4400256A Cited
US4376025A Cited
US4541984A Cited
US4683043A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-12-20 1997-06-21 1997-12-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-12-20 2001-06-21 2001-12-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-12-20 2005-06-21 2005-12-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag