Patent US5250477A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5250477A Expired / Lapsed US ⏱️ 0.0 years remaining

Silicon nitride based composite with improved fracture toughness

Assignee: Valenite LLC
•
Filing: 1990-10-11
•
Granted: 1993-10-05
•
Expires: 2010-10-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Composite materials, articles and cutting tools are prepared by densification to form a body comprising whiskers of hard refractory transition metal carbides, nitrides or carbonitrides uniformly distributed in a two-phase silicon nitride matrix. A first phase comprises silicon nitride grains and the second phase is an intergranular phase formed from one or more suitable densification aids. Optionally, dispersoid particles and/or polycrystalline fibers may also be incorporated. The preferred composite article or cutting tool has a fracture toughness equal to or greater than about 3.5 MPa.m 1/2 .

Inventors

  • 👤 II Joseph G. Baldoni
  • 👤 Sergej-Tomislav Buljan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 21:26
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/71; C04B35/78; C04B35/80; C04B35/515; C04B35/58; C04B35/584; C04B35/593; C04B35/5935; C04B2235/00; C04B2235/02; C04B2235/30; C04B2235/32; C04B2235/3217; C04B2235/3224; C04B2235/3225; C04B2235/50; C04B2235/52; C04B2235/5208; C04B2235/5216; C04B2235/522; C04B2235/5224; C04B2235/524; C04B2235/5244; C04B2235/526; C04B2235/5264; C04B2235/5276; C04B2235/70; C04B2235/74; C04B2235/77; C04B2235/80; C04B2235/85; C04B2235/96; Y; Y10; Y10T; Y10T407/00; Y10T407/27; Y10T409/00; Y10T409/30; Y10T409/303752; Y10T82/00; Y10T82/10

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 204 words
A method for continuous or interrupted machine cutting of cast iron stock comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .
Claim 2
Independent Claim 204 words
A method for continuous or interrupted machine cutting of cast iron stock comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .
Claim 3
Independent Claim 210 words
A method for continuous or interrupted machine cutting of high nickel alloy stock comprising at least 50% nickel comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions, thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .
Claim 4
Independent Claim 210 words
A method for continuous or interrupted machine cutting of high nickel alloy stock comprising at least 50% nickel comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions, thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-10-04 1997-04-05 1997-10-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-10-04 2001-04-05 2001-10-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-10-04 2005-04-05 2005-10-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag