Silicon nitride based composite with improved fracture toughness
Assignee: Valenite LLC
•
Filing: 1990-10-11
•
Granted: 1993-10-05
•
Expires: 2010-10-11
Abstract
Abstract Composite materials, articles and cutting tools are prepared by densification to form a body comprising whiskers of hard refractory transition metal carbides, nitrides or carbonitrides uniformly distributed in a two-phase silicon nitride matrix. A first phase comprises silicon nitride grains and the second phase is an intergranular phase formed from one or more suitable densification aids. Optionally, dispersoid particles and/or polycrystalline fibers may also be incorporated. The preferred composite article or cutting tool has a fracture toughness equal to or greater than about 3.5 MPa.m 1/2 .
Inventors
- 👤 II Joseph G. Baldoni
- 👤 Sergej-Tomislav Buljan
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 21:12
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/71; C04B35/78; C04B35/80; C04B35/515; C04B35/58; C04B35/584; C04B35/593; C04B35/5935; C04B2235/00; C04B2235/02; C04B2235/30; C04B2235/32; C04B2235/3217; C04B2235/3224; C04B2235/3225; C04B2235/50; C04B2235/52; C04B2235/5208; C04B2235/5216; C04B2235/522; C04B2235/5224; C04B2235/524; C04B2235/5244; C04B2235/526; C04B2235/5264; C04B2235/5276; C04B2235/70; C04B2235/74; C04B2235/77; C04B2235/80; C04B2235/85; C04B2235/96; Y; Y10; Y10T; Y10T407/00; Y10T407/27; Y10T409/00; Y10T409/30; Y10T409/303752; Y10T82/00; Y10T82/10
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
204 words
A method for continuous or interrupted machine cutting of cast iron stock comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .
Claim 2
Independent Claim
204 words
A method for continuous or interrupted machine cutting of cast iron stock comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .
Claim 3
Independent Claim
210 words
A method for continuous or interrupted machine cutting of high nickel alloy stock comprising at least 50% nickel comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions, thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .
Claim 4
Independent Claim
210 words
A method for continuous or interrupted machine cutting of high nickel alloy stock comprising at least 50% nickel comprising the step of milling, turning, or boring with a shaped tool of a densified abrasion and fracture resistant composite material comprising: about 5-60% by volume of one or more first dispersoid materials selected from the group consisting of whiskers of carbides, nitrides, and carbonitrides of titanium, hafnium, tantalum, niobium, and tungsten, and solid solutions, thereof; and optionally, one or more other dispersoid materials selected from the group consisting of particles and polycrystalline fibers of carbides, nitrides, and carbonitrides of titanium, zirconium, hafnium, vanadium, niobium, tantalum, chromium, molybdenum, and tungsten, and silicon carbide, titanium diboride, hafnium diboride, and alumina, and mixtures and solid solutions thereof; wherein the combined dispersoid materials comprise about 5-70% by volume of the densified composite material; the remainder of the densified composite material being a two-phase matrix comprising a first phase of silicon nitride grains and a second, continuous intergranular phase formed from one or more suitable densification aids; wherein the dispersoid materials are substantially uniformly distributed in the two-phase matrix, and the densified composite material has a density greater than about 98% or theoretical and a fracture toughness greater than or equal to 3.5 MPa.m 1/2 .
References Cited (Backward Citations)
JPS5247803A
Cited
US4433979A
Cited
US4388085A
Cited
US4440707A
Cited
US4416670A
Cited
US4409004A
Cited
US4406667A
Cited
US4421528A
Cited
US4421525A
Cited
US4424066A
Cited
US4425141A
Cited
US4426209A
Cited
US4406670A
Cited
US4406669A
Cited
US4507224A
Cited
US4449989A
Cited
US4469489A
Cited
US4441894A
Cited
US4543345A
Cited
JPS60200863A
Cited
US4818635A
Cited
US4610917A
Cited
US4978643A
Cited
US4990470A
Cited
US4946808A
Cited
US5023214A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1996-10-04 | 1997-04-05 | 1997-10-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2000-10-04 | 2001-04-05 | 2001-10-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2004-10-04 | 2005-04-05 | 2005-10-05 | $7700.00 | Window Closed / Lapsed |