US5061602A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Photosensitive recording material of enhanced flexibility
Assignee: BASF SE
•
Filing: 1989-07-25
•
Granted: 1991-10-29
•
Expires: 2009-07-25
Abstract
Abstract In a photosensitive recording material suitable for producing plates or resist patterns, the photopolymerizable recording layer contains as polymeric binder a film-forming copolymer which has a multiphase morphology, one phase having a glass transistion temperature below room temperature and a further phase having a glass transition temperature above room temperature and this copolymer having been obtained by free radical copolymerization of one or more macromers with one or more further olefinically unsaturated copolymerizable organic compounds.
Inventors
- 👤 Horst Koch
- 👤 Hans Schupp
- 👤 Reinhold Schwalm
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 04:41
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/027; G03F7/032; G03F7/033; Y; Y10; Y10S; Y10S430/00; Y10S430/1053; Y10S430/1055; Y10S430/106; Y10S430/108; Y10S430/11; Y10S430/111
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
191 words
A photosensitive recording element useful in the production of a printing plate or a resist pattern comprising a dimensionally stable base and a photopolymerizable recording layer on said base, said photopolymerizable recording layer being developable with aqueous alkali or with organic solvents and containing a polymeric binder which is soluble or dispersible in aqueous alkaline media or in organic solvents, one or more low molecular weight ethylenically unsaturated photopolymerizable organic compounds and one or more free radical forming photopolymerization initiators with or without further additive and/or auxiliary substances, wherein the polymeric binder comprises one or more film-forming copolymers which have a multiphase morphology with one or more phases having a glass transition temperature below room temperature and one or more further phases having a glass transition temperature above room temperature, this or these copolymers having been obtained by free radical copolymerization of one or more macromonomers with one or more further olefinically unsaturated copolymerizable organic compounds, and wherein, in the multiphase morphology copolymer used as the polymeric binder, the continuous phase has a glass transition temperature below room temperature and the dispersed phase has a glass transition temperature above room temperature.
Claim 2
Dependent Claim
191 words
A photosensitive recording element useful in the production of a printing plate or a resist pattern comprising a dimensionally stable base and a photopolymerizable recording layer on said base, said photopolymerizable recording layer being developable with aqueous alkali or with organic solvents and containing a polymeric binder which is soluble or dispersible in aqueous alkaline media or in organic solvents, one or more low molecular weight ethylenically unsaturated photopolymerizable organic compounds and one or more free radical forming photopolymerization initiators with or without further additive and/or auxiliary substances, wherein the polymeric binder comprises one or more film-forming copolymers which have a multiphase morphology with one or more phases having a glass transition temperature below room temperature and one or more further phases having a glass transition temperature above room temperature, this or these copolymers having been obtained by free radical copolymerization of one or more macromonomers with one or more further olefinically unsaturated copolymerizable organic compounds, and wherein, in the multiphase morphology copolymer used as the polymeric binder, the continuous phase has a glass transition temperature below room temperature and the dispersed phase has a glass transition temperature above room temperature.
Claim 3
Dependent Claim
31 words
The photosensitive recording element useful in the production of a printing plate or resist pattern of claim 1, wherein the polymeric binder comprises a filmforming copolymer which has a two-phase morphology.
Claim 4
Dependent Claim
32 words
The photosensitive recording element useful in the production of a printing plate or resist pattern of claim 1, wherein the polymeric binder has an average molecular weight (weight average) of over 10,000.
Claim 5
Dependent Claim
32 words
The photosensitive recording element useful in the production of a printing plate or resist pattern of claim 2, wherein the polymeric binder has an average molecular weight (weight average) of over 10,000.
Claim 6
Dependent Claim
41 words
The photosensitive recording element useful in the production of a printing plate or resist pattern of claim 1, wherein the macromer used for preparing the copolymer used as polymeric binder has an average molecular weight (weight average) from 1,000 to 100,000.
Claim 7
Dependent Claim
41 words
The photosensitive recording element useful in the production of a printing plate or resist pattern of claim 2, wherein the macromer used for preparing the copolymer used as polymeric binder has an average molecular weight (weight average) from 1,000 to 100,000.
Claim 8
Dependent Claim
41 words
The photosensitive recording element useful in the production of a printing plate or resist pattern of claim 3, wherein the macromer used for preparing the copolymer used as polymeric binder has an average molecular weight (weight average) from 1,000 to 100,000.
References Cited (Backward Citations)
US3036914A
Cited
US3469982A
Cited
US3751259A
Cited
US3887450B1
Cited
US3887450A
Cited
US3786116A
Cited
US3953309A
Cited
US3953309B1
Cited
US4234675A
Cited
US4239849A
Cited
EP0049504A1
Cited
US4454219A
Cited
EP0128014A2
Cited
US4722885A
Cited
US4688056A
Cited
US4849307A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1994-10-28 | 1995-04-29 | 1995-10-29 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1998-10-28 | 1999-04-29 | 1999-10-29 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2002-10-28 | 2003-04-29 | 2003-10-29 | $7700.00 | Window Closed / Lapsed |