Abstract

Abstract A case or cover for a hard bound book is formed by bonding the formed by bonding the cover boards to the book cover stock using a hot melt pressure sensitive adhesive composition comprising: (a) 10 to 40% by weight of a substantially radial styrene-butadiene block copolymer, the copolymer having a styrene content greater than about 35% by weight, a modulus at 300% elongation of at least 4.5 MPa and a solution viscosity less than about 1000 cps; (b) 20 to 65% by weight of a compatible tackifying resin; (c) 0.1 to 4% by weight stabilizer; and (d) the remainder (to 100%) comprising a plasticizing oil.

Inventors

  • 👤 Thomas P. Flanagan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 07:34
CPC Classifications
B; B42; B42D; B42D3/00; B42D3/02; C; C09; C09J; C09J153/00; C09J153/02; C08; C08L; C08L2666/00; C08L2666/02; Y; Y10; Y10S; Y10S412/00; Y10S412/901; Y10T; Y10T428/00; Y10T428/28; Y10T428/31504; Y10T428/31855; Y10T428/31909; Y10T428/31913; Y10T428/31917; Y10T442/00; Y10T442/20; Y10T442/2738; Y10T442/2746; Y10T442/2754

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 99 words
A case for a hard cover book formed by bonding the cover boards to the book cover stock using a hot melt pressure sensitive adhesive composition comprising: (a) 10 to 40% by weight of a substantially radial styrene-butadiene block copolymer, the copolymer having a styrene content greater than about 35% by weight, a modulus at 300% elongation of at least 4.5 MPa and a solution viscosity less than about 1000 cps; (b) 20 to 65% by weight of a compatible tackifying resin; (c) 0.1 to 4% by weight stabilizer; and (d) the remainder (to 100%) comprising a plasticizing oil.
Claim 2
Dependent Claim 99 words
A case for a hard cover book formed by bonding the cover boards to the book cover stock using a hot melt pressure sensitive adhesive composition comprising: (a) 10 to 40% by weight of a substantially radial styrene-butadiene block copolymer, the copolymer having a styrene content greater than about 35% by weight, a modulus at 300% elongation of at least 4.5 MPa and a solution viscosity less than about 1000 cps; (b) 20 to 65% by weight of a compatible tackifying resin; (c) 0.1 to 4% by weight stabilizer; and (d) the remainder (to 100%) comprising a plasticizing oil.
Claim 3
Dependent Claim 118 words
The case of claim 1 wherein the tackifier in the hot melt adhesive composition is any compatible resin or mixture thereof selected from the group consisting of (1) natural and modified rosins1 (2) glycerol and pentaerythritol esters of natural and modified rosins; (3) copolymers and terpolymers of natural terpenes; (4) polyterpene resins having a softening point, as determined by ASTM method E28-58T, of from about 80° to 150° C.; (5) phenolic modified terpene resins and hydrogenated derivatives thereof; (6) aliphatic petroleum hydrocarbon resins having a Ball and Ring softening point of from about 70° to 135° C.; (7) aromatic petroleum hydrocarbon resins and the hydrogenated derivatives thereof; and (8) alicyclic petroleum hydrocarbon resins and the hydrogenated derivatives thereof.
Claim 4
Dependent Claim 13 words
The case of claim 1 wherein the cover board is chestnut cover board.
Claim 5
Dependent Claim 32 words
The case of claim 1 wherein the cover stock is selected from the group consisting of paper cloth, woven fabric, pyroxylin, vinyl impregnated on coated stock and spun bonded high density polyethylene.
Claim 6
Dependent Claim 104 words
In a process for the production of a book case wherein the cover boards are bonded to the cover stock, the improvement which comprises using a hot melt pressure sensitive adhesive comprising: (a) 10 to 40% by weight of a substantially radial styrene-butadiene block copolymer, the copolymer having a styrene content greater than about 35% by weight, a modulus at 300% elongation of at least 4.5 MPa and a solution viscosity less than about 1000 cps; (b) 20 to 65% by weight of a compatible tackifying resin; (c) 0.1 to 4% by weight stabilizer; and (d) the remainder (to 100%) comprising a plasticizing oil.
Claim 7
Dependent Claim 104 words
In a process for the production of a book case wherein the cover boards are bonded to the cover stock, the improvement which comprises using a hot melt pressure sensitive adhesive comprising: (a) 10 to 40% by weight of a substantially radial styrene-butadiene block copolymer, the copolymer having a styrene content greater than about 35% by weight, a modulus at 300% elongation of at least 4.5 MPa and a solution viscosity less than about 1000 cps; (b) 20 to 65% by weight of a compatible tackifying resin; (c) 0.1 to 4% by weight stabilizer; and (d) the remainder (to 100%) comprising a plasticizing oil.
Claim 8
Dependent Claim 13 words
The process of claim 5 wherein the cover board is chestnut cover board.
Claim 9
Dependent Claim 32 words
The process of claim 5 wherein the cover stock is selected from the group consisting of paper cloth, woven fabric, pyroxylin, vinyl impregnated or coated stock and spun bonded high density polyethylene.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-07-30 1994-01-29 1994-07-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-07-30 1998-01-29 1998-07-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-07-30 2002-01-29 2002-07-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag