Gaseous removal of ceramic coatings

Assignee: RTX Corp
•
Filing: 1988-04-11
•
Granted: 1989-12-26
•
Expires: 2008-04-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Removal of ceramic thermal barrier coatings from metallic substrates is achieved by contacting the coated article with fluorine containing gas at an elevated temperature. The gas penetrates the ceramic to attack the interface between the substrate and ceramic causing the ceramic to spall.

Inventors

  • 👤 Charles C. McComas

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 00:26
CPC Classifications
C; C23; C23G; C23G5/00; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49718; Y10T29/49721; Y10T29/49723

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 120 words
A method for removing a ceramic coating from a metallic substrate, said coating containing at least 5% by volume of porosity, including comprising the steps of providing a metallic substrate having a porous ceramic coating, heating the coated substrate to a temperature between 1400° F. to 2000° F. while contacting the coated substrate with a gas mixture containing an amount of fluorine sufficient to attack the interface between the metallic substrate and the ceramic coating in preference to attacking the coating so as to thereby remove the ceramic coating by spallation without completely dissolving the coating and without significantly attacking the substrate, said coating removal occurring in less time than that required for complete coating dissolution under the same conditions.
Claim 2
Independent Claim 120 words
A method for removing a ceramic coating from a metallic substrate, said coating containing at least 5% by volume of porosity, including comprising the steps of providing a metallic substrate having a porous ceramic coating, heating the coated substrate to a temperature between 1400° F. to 2000° F. while contacting the coated substrate with a gas mixture containing an amount of fluorine sufficient to attack the interface between the metallic substrate and the ceramic coating in preference to attacking the coating so as to thereby remove the ceramic coating by spallation without completely dissolving the coating and without significantly attacking the substrate, said coating removal occurring in less time than that required for complete coating dissolution under the same conditions.
Claim 3
Dependent Claim 17 words
A method as in claim 1 wherein the ceramic coating consists essentially of stabilized zirconia or alumina.
Claim 4
Dependent Claim 30 words
A method as in claim 1 wherein the gas contains an amount of fluorine equivalent to that found in a mixture containing 2% to 10% by volume hydrogen fluoride gas.
Claim 5
Dependent Claim 18 words
A method as in claim 1 in which the temperature is maintained between 1600° F. and 1900° F.
Claim 6
Dependent Claim 18 words
A method as in claim 1 wherein the reaction time is from about 1 to about 4 hours.
Claim 7
Dependent Claim 17 words
A method as in claim 2 wherein the fluorine constituent is present in the form of HF.
Claim 8
Dependent Claim 19 words
A method as in claim 1 wherein the gas mixture comprises 2-10 vol. % HF, with the balance hydrogen.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-12-25 1993-06-26 1993-12-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-12-25 1997-06-26 1997-12-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-12-25 2001-06-26 2001-12-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag