Fabrication of high-silica glass article

Assignee: Nokia Bell Labs
•
Filing: 1986-11-20
•
Granted: 1987-11-17
•
Expires: 2006-11-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Incorporation of fluorine into a porous silica body, such as an unsintered body produced by a sol-gel method, by VAD or OVPO, reduces or eliminates bubble or pore formation upon re-heating of the glass formed by sintering of the porous material. Effective fluorine concentrations are between 0.01 and 5% by weight. The invention can be used advantageously in producing preforms and optical fiber.

Inventors

  • 👤 David W. Johnson, Jr.
  • 👤 John B. MacChesney
  • 👤 Eliezer M. Rabinovich
  • 👤 Eva M. Vogel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 21:00
CPC Classifications
C; C03; C03B; C03B37/00; C03B37/01; C03B37/012; C03B37/014; C03B37/016; C03B19/00; C03B19/12; C03B19/14; C03B19/1453; C03B37/01446; C03B2201/00; C03B2201/06; C03B2201/08; C03B2201/12; C03B2201/14; Y; Y10; Y10S; Y10S65/00; Y10S65/15; Y10S65/16; Y10S65/90; Y10S65/901

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 272 words
Method of producing an optical fiber comprising a core and a cladding surrounding the core, the core and the cladding consisting of high-silica glass, the method comprising making a high-silica glass body having a predetermined refractive index profile, with a center region of relatively high refractive index and a peripheral region of relatively low refractive index surrounding the center region, the glass body to be referred to as the preform, heating at least a part of the preform to a temperature above a sintering temperature, and drawing the optical fiber from the heated part of the preform, with the fiber core and cladding derived from the center region and peripheral region of the preform, respectively; wherein the preform is made by a process that comprises (a) making a porous high-silica body by a sol-gel process, the porous body having an inner portion and an outer portion; (b) drying the porous body including heat treatment in an atmosphere comprising chlorine to remove bound water; and (c) sintering the porous body at the sintering temperature such that the porous body is transformed into the preform, the center and peripheral regions of the preform derived, respectively, from the inner and outer portion of the porous body; the method further comprises (d) causing to be present, prior to completion of step (c), in both the inner and the outer portion of the porous body, a fluorine concentration that is effective to essentially prevent the evolution of bubbles in the heated part of the preform during the heating and fiber drawing, such that the core and the cladding of the optical fiber are essentially free of bubbles.
Claim 2
Dependent Claim 272 words
Method of producing an optical fiber comprising a core and a cladding surrounding the core, the core and the cladding consisting of high-silica glass, the method comprising making a high-silica glass body having a predetermined refractive index profile, with a center region of relatively high refractive index and a peripheral region of relatively low refractive index surrounding the center region, the glass body to be referred to as the preform, heating at least a part of the preform to a temperature above a sintering temperature, and drawing the optical fiber from the heated part of the preform, with the fiber core and cladding derived from the center region and peripheral region of the preform, respectively; wherein the preform is made by a process that comprises (a) making a porous high-silica body by a sol-gel process, the porous body having an inner portion and an outer portion; (b) drying the porous body including heat treatment in an atmosphere comprising chlorine to remove bound water; and (c) sintering the porous body at the sintering temperature such that the porous body is transformed into the preform, the center and peripheral regions of the preform derived, respectively, from the inner and outer portion of the porous body; the method further comprises (d) causing to be present, prior to completion of step (c), in both the inner and the outer portion of the porous body, a fluorine concentration that is effective to essentially prevent the evolution of bubbles in the heated part of the preform during the heating and fiber drawing, such that the core and the cladding of the optical fiber are essentially free of bubbles.
Claim 3
Dependent Claim 24 words
Method of claim 1, wherein step (a) comprises forming a gel tube and filling the interior of the gel tube with a second gel.
Claim 4
Dependent Claim 19 words
Method of claim 1, wherein the fluorine concentration is at least 0.01% by weight everywhere in the porous body.
Claim 5
Dependent Claim 32 words
Method of claim 1, wherein at least part of one or both of steps (b) and (c) is carried out in an atmosphere consisting essentially of about 97% He and 3% chlorine.
Claim 6
Dependent Claim 22 words
Method of claim 1, wherein at least part of step (c) is carried out in an atmosphere that comprises chlorine and fluorine.
Claim 7
Dependent Claim 32 words
Method of claim 1, further comprising contacting, at least during part of step (c), the porous body with chlorine or a chlorine-containing compound such that OH is removed from the porous body.
Claim 8
Dependent Claim 30 words
Method of claim 1, wherein at least some of the fluorine is caused to be present in the porous body by introducing fluorine into the porous body prior to sintering.
Claim 9
Dependent Claim 30 words
Method of claim 1, wherein at least some of the fluorine is caused to be present in the porous body by contacting the dried porous body with a fluorine-containing atmosphere.
Claim 10
Dependent Claim 37 words
Method of claim 1, wherein step (d) comprises contacting the porous body with at least one compound selected from the group consisting of the fluorinated hydrocarbon, CF 4-y Cl y (0≦y≦3), F 2 and the inorganic fluorides.
Claim 11
Dependent Claim 12 words
Method of claim 9, wherein the fluorinated hydrocarbon is tetraethylammonium fluoride hydrate.
Claim 12
Dependent Claim 35 words
Method of claim 9, wherein the inorganic fluoride is selected from the group consisting of HF, SiF 4 , NH 4 F, GeF 4 , BF 3 , PF 3 , and PF 5 .
Claim 13
Dependent Claim 6 words
Method of claim 9, wherein y=2.
Claim 14
Dependent Claim 17 words
Method of claim 1, wherein the temperature above the sintering temperature is at least about 2000° C.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-11-16 1991-05-18 1991-11-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-11-16 1995-05-18 1995-11-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-11-16 1999-05-18 1999-11-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag