Patent US4649032A successfully refreshed from Google Patents.
US4649032A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for the selective removal of hydrogen sulfide from gaseous streams
Assignee: Mobil Oil AS
•
Filing: 1985-01-11
•
Granted: 1987-03-10
•
Expires: 2005-01-11
Abstract
Abstract The invention relates to a process for the selective removal of hydrogen sulfide from a gaseous stream additionally containing carbon dioxide by contacting the gaseous stream with a polyvalent metal chelate solution for a time sufficient to allow the polyvalent metal chelate to oxidize the hydrogen sulfide to elemental sulfur without allowing the polyvalent metal chelate solution to absorb appreciable amounts of carbon dioxide. The pH of the metal chelate solution should be greater than 7 and the contact time between the polyvalent metal chelate and the gaseous stream is between 0.006 and 0.08 second.
Inventors
- 👤 Earl S. Snavely, Jr.
- 👤 Timothy A. Jones
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 20:43
CPC Classifications
B; B01; B01D; B01D53/00; B01D53/34; B01D53/46; B01D53/48; B01D53/52; C; C01; C01B; C01B17/00; C01B17/02; C01B17/04; C01B17/05
Claims Analysis
Total Claims: 65
Claim 1
Independent Claim
80 words
A process for the selective removal of hydrogen sulfide from a gaseous stream, additionally containing carbon dioxide, by contacting the gaseous stream with a polyvalent metal chelate solution, wherein the pH of said polyvalent metal chelate solution is greater than 7 and is constant because the net absorption-desorption of said carbon dioxide in said solution is zero, said contacting being for a time sufficient to allow the polyvalent metal chelate solution to oxidize the hydrogen sulfide to elemental sulfur precipitate.
Claim 2
Dependent Claim
80 words
A process for the selective removal of hydrogen sulfide from a gaseous stream, additionally containing carbon dioxide, by contacting the gaseous stream with a polyvalent metal chelate solution, wherein the pH of said polyvalent metal chelate solution is greater than 7 and is constant because the net absorption-desorption of said carbon dioxide in said solution is zero, said contacting being for a time sufficient to allow the polyvalent metal chelate solution to oxidize the hydrogen sulfide to elemental sulfur precipitate.
Claim 3
Dependent Claim
30 words
The process of claim 1, wherein said gaseous stream is contacted with said solution in a static mixer and said hydrogen sulfide is oxidized to sulfur in said static mixer.
Claim 4
Dependent Claim
11 words
The process of claim 1, wherein the polyvalent metal is iron.
Claim 5
Dependent Claim
11 words
The process of claim 1, wherein the chelate is ethylenediaminetetraacetic acid.
Claim 6
Dependent Claim
11 words
The process of claim 1, wherein the chelate is N-hydroxylethyl-ethylenediaminetriacetic acid.
Claim 7
Dependent Claim
25 words
The process of claim 1, wherein the contact time between the gaseous stream and the metal chelate is from about 0.006 to about 0.08 second.
Claim 8
Dependent Claim
15 words
The process of claim 1, wherein said solution contains carbonates, bicarbonates, hydroxide, or mixtures thereof.
Claim 9
Dependent Claim
18 words
The process of claim 1, wherein the polyvalent metal chelate solution has a pH between 7.5 and 11.
Claim 10
Dependent Claim
19 words
The process of claim 1, wherein at least 80% of the hydrogen sulfide in the gaseous stream is removed.
Claim 11
Dependent Claim
25 words
The process of claim 1, wherein after oxidizing the hydrogen sulfide, the polyvalent metal chelate is regenerated by passing an oxygen-containing gas through said solution.
Claim 12
Dependent Claim
11 words
The process of claim 10, wherein said oxygen-containing gas is air.
Claim 13
Dependent Claim
38 words
The process of claim 2, further comprising separating a gas phase of reduced hydrogen sulfide content from a liquid phase containing a reduced metal chelate solution having dispersed therein sulfur particles immediately after contact in said static mixer.
Claim 14
Dependent Claim
20 words
The process of claim 12, comprising regenerating said reduced metal chelate by passing an oxygen-containing gas through said liquid phase.
Claim 15
Dependent Claim
31 words
The process of claim 13, wherein said oxygen-containing gas is bubbled through said liquid phase, and said sulfur particles are carried to the surface of the liquid phase by said bubbles.
Claim 16
Dependent Claim
42 words
The process of claim 10, wherein said oxygen-containing gas is passed through said solution by forming a low pressure area below the surface of said solution and inducing said gas into said low pressure area to disperse said gas in said solution.
Claim 17
Dependent Claim
34 words
The process of claim 15, wherein said dispersed gas and said solution are subjected to a shearing force to intimately mix said gas in said solution and finely divide said gas into minute bubbles.
Claim 18
Dependent Claim
38 words
The process of claim 16, wherein said low pressure area is formed by movement of a rotating means below the surface of said solution and wherein said low pressure area communicates with a supply of said oxygen-containing gas.
Claim 19
Dependent Claim
14 words
The process of claim 17, wherein said supply of oxygen-containing gas is the atmosphere.
Claim 20
Dependent Claim
49 words
The process of claim 17, wherein a disperser means is provided below the surface of said solution, said disperser means surrounding and being circumferentially spaced from said rotating means, said gas and liquid being sheared by passing said dispersed gas and liquid through fluid openings in said disperser means.
Claim 21
Dependent Claim
23 words
The process of claim 1, wherein said gaseous stream contains a major proportion of carbon dioxide and a minor proportion of hydrogen sulfide.
Claim 22
Dependent Claim
25 words
The process of claim 20, wherein said gaseous stream comprises greater than 75% by weight carbon dioxide and less than 5% by weight hydrogen sulfide.
Claim 23
Dependent Claim
44 words
The process of claim 12, wherein said separating takes place in a separator means immediately following said static mixer, said static mixer and separator means forming a static mixer-separator train, said gaseous stream being fed to a plurality of first stage static mixer-separator trains.
Claim 24
Dependent Claim
44 words
The process of claim 22, wherein at least one additional static mixer-separator train follows each of said plurality of first stage static mixer-separator trains, said gas phase from said separator means being conveyed to the following static mixer in said additional static mixer-separator trains.
Claim 25
Dependent Claim
37 words
The process of claim 23, wherein said polyvalent metal chelate solution is fed to the static mixers of said plurality of first stage static mixer-separator trains and to the static mixers of said additional static mixer-separator trains.
Claim 26
Dependent Claim
55 words
The process of claim 23, wherein the liquid phase from each of said separators from the plurality of first stage static mixer-separator trains and the separators from said additional static mixer-separator trains is conveyed to a regenerator, said reduced metal chelate being oxidized by passing an oxygen-containing gas through said liquid phase in said regenerator.
Claim 27
Dependent Claim
31 words
The process of claim 25, wherein said oxygen-containing gas is bubbled through said liquid phase and said sulfur particles are carried to the surface of said liquid phase by said bubbles.
Claim 28
Dependent Claim
30 words
The process of claim 26, further comprising separating the sulfur particles from said liquid phase and melting the sulfur particles and separating said molten sulfur from any residual liquid phase.
Claim 29
Dependent Claim
36 words
The process of claim 10, further comprising adding an oxidizing adjunct selected from the group consisting of hydroquinones, anthraquinones, naphthaquinones, and mixtures thereof to said solution to increase the efficiency of regenerating the polyvalent metal chelate.
Claim 30
Dependent Claim
15 words
The process of claim 28, wherein said anthraquinone comprises 2-7 anthraquinone disulfonic acid disodium salt.
Claim 31
Dependent Claim
43 words
The process of claim 28, wherein said polyvalent metal chelate solution consists essentially of chelated iron, pH adjusting agents selected from the group consisting of carbonates, bicarbonates, hydroxides or mixtures thereof, and said oxidizing adjunct for increasing the regeneration of said chelated iron.
Claim 32
Dependent Claim
19 words
The process of claim 10, wherein said regenerated polyvalent metal chelate is recycled for contact with said gaseous stream.
Claim 33
Dependent Claim
15 words
The process of claim 31, wherein said recycled polyvalent metal chelate is devoid of oxygen.
Claim 34
Dependent Claim
17 words
The process of claim 31, wherein said polyvalent metal chelate comprises about 6% molar excess of chelate.
Claim 35
Dependent Claim
11 words
The process of claim 33, wherein said polyvalent metal is iron.
Claim 36
Dependent Claim
17 words
The process of claim 10, wherein said elemental sulfur is separated from said regenerated polyvalent metal chelate.
Claim 37
Dependent Claim
26 words
The process of claim 10, wherein an insufficient amount of oxygen-containing gas is passed through said polyvalent metal chelate solution to oxidize all of said solution.
Claim 38
Dependent Claim
72 words
A process for the selective removal of hydrogen sulfide from a gaseous stream, additionally containing carbon dioxide, comprising the step of contacting the gaseous stream with a polyvalent metal chelate solution having a pH value greater than 7, for a time from about 0.006 to about 0.08 seconds, wherein the pH of the polyvalent metal chelate solution is constant because the net absorption-desorption of the carbon dioxide in the solution is zero.
Claim 39
Dependent Claim
72 words
A process for the selective removal of hydrogen sulfide from a gaseous stream, additionally containing carbon dioxide, comprising the step of contacting the gaseous stream with a polyvalent metal chelate solution having a pH value greater than 7, for a time from about 0.006 to about 0.08 seconds, wherein the pH of the polyvalent metal chelate solution is constant because the net absorption-desorption of the carbon dioxide in the solution is zero.
Claim 40
Dependent Claim
43 words
The process of claim 37, wherein the contact time is limited to a time sufficient to allow the polyvalent metal chelate to oxidize the hydrogen sulfide to elemental sulfur, but below that time allowing the metal chelate solution to absorb any carbon dioxide.
Claim 41
Dependent Claim
23 words
The process of claim 37, wherein the polyvalent metal is selected from the group consisting of iron, copper, manganese, or any combination thereof.
Claim 42
Dependent Claim
22 words
The process of claim 37, wherein the gaseous stream is contacted with the polyvalent metal chelate solution in the absence of oxygen.
Claim 43
Dependent Claim
18 words
The process of claim 37, wherein the polyvalent metal chelate solution has a pH between 7.5 and 11.
Claim 44
Dependent Claim
25 words
The process of claim 37, wherein the gaseous stream comprises greater than 75 wt % carbon dioxide and less than 5 wt % hydrogen sulfide.
Claim 45
Dependent Claim
100 words
The process of claim 37, further comprising the steps of: (a) separating a gas phase of reduced hydrogen sulfide content from a liquid phase containing reduced metal chelate solution having dispersed therein elemental sulfur particles; (b) passing a sufficient amount of an oxygen-containing gas through the liquid phase to simultaneously regenerate the reduced metal chelate and to separate the elemental sulfur particles from the chelate solution by flotation; (c) recovering elemental sulfur particles; and (d) recycling the regenerated metal chelate solution to be utilized in the initial step, wherein the gaseous stream is contacted with the polyvalent metal chelate solution.
Claim 46
Dependent Claim
37 words
The process of claim 43, wherein less than 100% regeneration of the metal chelate is obtained to insure the absence of oxygen in the area where the gaseous stream is contacted with the polyvalent metal chelate solution.
Claim 47
Dependent Claim
15 words
The process of claim 43, wherein the elemental sulfur recovered is substantially pure elemental sulfur.
Claim 48
Dependent Claim
79 words
A process for the selective removal of hydrogen sulfide from a gaseous stream additionally containing carbon dioxide, comprising the step of contacting the gaseous stream with a basic polyvalent metal chelate solution for a time sufficient to allow the polyvalent metal chelate to oxidize at least 80% of the hydrogen sulfide to elemental sulfur precipitate, wherein the pH of the polyvalent metal chelate solution is constant because the net absorption-desorption of the carbon dioxide in the solution is zero.
Claim 49
Dependent Claim
79 words
A process for the selective removal of hydrogen sulfide from a gaseous stream additionally containing carbon dioxide, comprising the step of contacting the gaseous stream with a basic polyvalent metal chelate solution for a time sufficient to allow the polyvalent metal chelate to oxidize at least 80% of the hydrogen sulfide to elemental sulfur precipitate, wherein the pH of the polyvalent metal chelate solution is constant because the net absorption-desorption of the carbon dioxide in the solution is zero.
Claim 50
Dependent Claim
43 words
The process of claim 46, wherein the contact time is limited to a time sufficient to allow the polyvalent metal chelate to oxidize the hydrogen sulfide to elemental sulfur, but below that time allowing the metal chelate solution to absorb any carbon dioxide.
Claim 51
Dependent Claim
23 words
The process of claim 46, wherein the polyvalent metal is selected from the group consisting of iron, copper, manganese, or any combination thereof.
Claim 52
Dependent Claim
22 words
The process of claim 46, wherein the gaseous stream is contacted with the polyvalent metal chelate solution in the absence of oxygen.
Claim 53
Dependent Claim
39 words
The process of claim 46, wherein the contact time between the gaseous stream and the metal chelate is from about 0.006 to about 0.08 seconds, and wherein the polyvalent metal chelate solution has a pH between 7.5 and 11.
Claim 54
Dependent Claim
25 words
The process of claim 46, wherein the gaseous stream comprises greater than 75 wt % carbon dioxide and less than 5 wt % hydrogen sulfide.
Claim 55
Dependent Claim
101 words
The process of claim 46, further comprising the steps of: (a) separating a gas phase of reduced hydrogen sulfide content from a liquid phase containing reduced metal chelate solution having dispersed therein elemental sulfur particles; (b) passing a sufficient amount of an oxygen-containing gas through the liquid phase to simultaneously regenerate the reduced metal chelate and to separate the elemental sulfur particles from the chelate solution by flotation; (c) recovering the separated elemental sulfur particles; and (d) recycling the regenerated metal chelate solution to be utilized in the initial step of contacting the gaseous stream with the polyvalent metal chelate solution.
Claim 56
Dependent Claim
37 words
The process of claim 52, wherein less than 100% regeneration of the reduced metal chelate is achieved to insure the absence of oxygen in the area where the gaseous stream is contacted with the polyvalent metal chelate.
Claim 57
Dependent Claim
16 words
The process of claim 52, wherein the recovered elemental sulfur particles are substantially pure elemental sulfur.
Claim 58
Dependent Claim
165 words
A process for the continuous removal of hydrogen sulfide from a gaseous stream additionally containing carbon dioxide, comprising the steps of: (a) contacting the gaseous stream with a polyvalent metal chelate solution having a pH value between 7.5 and 11, wherein the contact time is sufficient to allow the polyvalent metal chelate to oxidize the hydrogen sulfide to elemental sulfur precipitate, and wherein the pH of said polyvalent metal chelate solution is constant because the net absorption-desorption of said carbon dioxide in said solution is zero; (b) separating a gas phase of reduced hydrogen sulfide content from a liquid phase containing reduced metal chelate solution having dispersed therein elemental sulfur particles; (c) passing a sufficient amount of an oxygen-containing gas through the liquid phase to simultaneously regenerate the reduced metal chelate and to separate the elemental sulfur particles from the chelate solution by flotation; (d) recovering the separated elemental sulfur particles; and (e) recycling the regenerated metal chelate solution to be utilized in step (a).
Claim 59
Dependent Claim
165 words
A process for the continuous removal of hydrogen sulfide from a gaseous stream additionally containing carbon dioxide, comprising the steps of: (a) contacting the gaseous stream with a polyvalent metal chelate solution having a pH value between 7.5 and 11, wherein the contact time is sufficient to allow the polyvalent metal chelate to oxidize the hydrogen sulfide to elemental sulfur precipitate, and wherein the pH of said polyvalent metal chelate solution is constant because the net absorption-desorption of said carbon dioxide in said solution is zero; (b) separating a gas phase of reduced hydrogen sulfide content from a liquid phase containing reduced metal chelate solution having dispersed therein elemental sulfur particles; (c) passing a sufficient amount of an oxygen-containing gas through the liquid phase to simultaneously regenerate the reduced metal chelate and to separate the elemental sulfur particles from the chelate solution by flotation; (d) recovering the separated elemental sulfur particles; and (e) recycling the regenerated metal chelate solution to be utilized in step (a).
Claim 60
Dependent Claim
23 words
The process of claim 55, wherein the polyvalent metal is selected from the group consisting of iron, copper, manganese, or any combination thereof.
Claim 61
Dependent Claim
22 words
The process of claim 55, wherein the gaseous stream is contacted with the polyvalent metal chelate solution in the absence of oxygen.
Claim 62
Dependent Claim
25 words
The process of claim 55, wherein the contact time between the gaseous stream and the metal chelate is from about 0.006 to about 0.08 seconds.
Claim 63
Dependent Claim
25 words
The process of claim 55, wherein the gaseous stream comprises greater than 75 wt % carbon dioxide and less than 5 wt % hydrogen sulfide.
Claim 64
Dependent Claim
37 words
The process of claim 55, wherein less than 100% regeneration of the reduced metal chelate is achieved to insure the absence of oxygen in the area where the gaseous stream is contacted with the polyvalent metal chelate.
Claim 65
Dependent Claim
15 words
The process of claim 55, wherein the recovered elemental sulfur is substantially pure elemental sulfur.
References Cited (Backward Citations)
GB448270A
Cited
US2747962A
Cited
US3077488A
Cited
US3071433A
Cited
US3226320A
Cited
US3580950A
Cited
US3491880A
Cited
US3752877A
Cited
US3642431A
Cited
US3642448A
Cited
US3647069A
Cited
US4036942A
Cited
US4085192A
Cited
US4009251A
Cited
US3933993A
Cited
US3993563A
Cited
US3959452A
Cited
US4125597A
Cited
US4234560A
Cited
US4118467A
Cited
US4309285A
Cited
US4402930A
Cited
US4414194A
Cited
US4388293A
Cited
US4400368A
Cited
US4499059A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1990-03-09 | 1990-09-08 | 1991-03-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1994-03-09 | 1994-09-08 | 1995-03-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1998-03-09 | 1998-09-08 | 1999-03-10 | $7700.00 | Window Closed / Lapsed |