← Back to Patent Explorer
US4118467A Expired / Lapsed US ⏱️ 0.0 years remaining

Treatment of gas containing hydrogen sulfide

Assignee: Toa Oil Co Ltd
•
Filing: 1978-03-16
•
Granted: 1978-10-03
•
Expires: 1998-03-16
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An effluent alkali salt solution obtained in the desulfurization of a hydrogen sulfide-containing gas by washing with an alkali wash solution is subjected to a two stage precipitation treatment at different temperatures to recover valuable components such as a vanadium compound, chelating agent, ADA, and active alkali salts while removing inactive salts such as sulfate and thiosulfate.

Inventors

  • 👤 Masaru Sano
  • 👤 Koji Kashima

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 19:29
CPC Classifications
C; C01; C01B; C01B17/00; C01B17/02; C01B17/04; C01B17/05; B; B01; B01D; B01D53/00; B01D53/14; B01D53/1418; B01D53/1456; B01D53/1468; B01D53/34; B01D53/46; B01D53/48; B01D53/52; Y; Y02; Y02W; Y02W10/00; Y02W10/30; Y02W10/37

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 195 words
In a process for treating a hydrogen sulfide-containing gas, in which said gas is washed with an alkali wash solution to absorb said hydrogen sulfide as hydrosulfide, the solution containing hydrosulfide being oxidized using an oxidizer-anthraquinone disulfonate system to convert said hydrosulfide into elemental sulfur, said elemental sulfur being removed therefrom to obtain a salt solution comprising sulfur compounds and the disulfonate, the improvement comprising: a first stage wherein at least a portion of said salt solution is concentrated so as to form a concentrate having a sodium ion concentration of at least about 9 g.mol/Kg H 2 O, the disulfonate being allowed to precipitate from said concentrate at a temperature of about 25° to 90° C. to form a first mixture, said first mixture being separated into a first solids rich phase containing said precipitated disulfonate and a first mother liquid phase; and a second stage wherein said first liquid phase is cooled to a temperature not higher than 10° C. to allow the sulfur compounds to precipitate to form a second mixture, said second mixture being separated into a second solids rich phase containing said precipitated sulfur compounds and a second liquid phase.
Claim 2
Dependent Claim 195 words
In a process for treating a hydrogen sulfide-containing gas, in which said gas is washed with an alkali wash solution to absorb said hydrogen sulfide as hydrosulfide, the solution containing hydrosulfide being oxidized using an oxidizer-anthraquinone disulfonate system to convert said hydrosulfide into elemental sulfur, said elemental sulfur being removed therefrom to obtain a salt solution comprising sulfur compounds and the disulfonate, the improvement comprising: a first stage wherein at least a portion of said salt solution is concentrated so as to form a concentrate having a sodium ion concentration of at least about 9 g.mol/Kg H 2 O, the disulfonate being allowed to precipitate from said concentrate at a temperature of about 25° to 90° C. to form a first mixture, said first mixture being separated into a first solids rich phase containing said precipitated disulfonate and a first mother liquid phase; and a second stage wherein said first liquid phase is cooled to a temperature not higher than 10° C. to allow the sulfur compounds to precipitate to form a second mixture, said second mixture being separated into a second solids rich phase containing said precipitated sulfur compounds and a second liquid phase.
Claim 3
Dependent Claim 20 words
The process as claimed in claim 1, further comprising recycling said first solid rich phase to said alkali wash solution.
Claim 4
Dependent Claim 57 words
The process as claimed in claim 1, further comprising washing said first solids rich phase with water in an amount sufficient to dissolve said precipitated disulfonate to form a third mixture, separating said third mixture into a third solids rich phase and a third liquid phase, and recycling said third liquid phase to said alkali wash solution.
Claim 5
Dependent Claim 21 words
The process as claimed in 1, 2 or 3, further comprising recycling said second liquid phase to said alkali wash solution.
Claim 6
Dependent Claim 18 words
The process as claimed in claim 1, wherein said separation of said first mixture is conducted by centrifuge.
Claim 7
Dependent Claim 28 words
The process as claimed in claim 1, wherein said precipitation in said first stage is effected at a temperature in the range of from 30° to 40° C.
Claim 8
Dependent Claim 28 words
The process as claimed in claim 1, wherein said precipitation in said second stage is effected at a temperature in the range of from 0° to 5° C.

References Cited (Backward Citations)

US3928535A Cited
US3972989A Cited
US3959452A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-10-02 1982-04-03 1982-10-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-10-02 1986-04-03 1986-10-03 $3760.00 Window Closed / Lapsed