← Back to Patent Explorer
US4485204A Expired / Lapsed US ⏱️ 0.0 years remaining

Polyester blends comprising a desiccant and a rubbery block copolymer

Assignee: Phillips Petroleum Co
•
Filing: 1981-08-26
•
Granted: 1984-11-27
•
Expires: 2001-08-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Blends of a polyester with a desiccant and one or more of a poly(mono-1-olefin); a rubbery diene/monovinylarene block copolymer; or a poly(mono-1-olefin) and a rubbery block copolymer, optionally with a resinous poly(monovinylarene). Any of these blends can further employ an oil as an additional component.

Inventors

  • 👤 Lester G. Nabors

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 09:34
CPC Classifications
C; C08; C08J; C08J11/00; C08J11/04; C08J11/06; C08K; C08K3/00; C08K3/18; C08K3/20; C08K3/22; C08L; C08L67/00; C08L67/02; C08J2367/00; C08J2367/02; Y; Y02; Y02W; Y02W30/00; Y02W30/50; Y02W30/62

Claims Analysis

Total Claims: 25
Claim 1
Independent Claim 51 words
The polyester composition consisting essentially of (a) about 50 to 90 weight percent polyalkylene terephthalate polyester, (b) rubbery block copolymer, and (c) desiccant, wherein said desiccant is selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; optionally further with (f) light mineral oil.
Claim 2
Dependent Claim 51 words
The polyester composition consisting essentially of (a) about 50 to 90 weight percent polyalkylene terephthalate polyester, (b) rubbery block copolymer, and (c) desiccant, wherein said desiccant is selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; optionally further with (f) light mineral oil.
Claim 3
Dependent Claim 53 words
The polyester composition consisting essentially of (a) about 50 to 90 weight percent polyalkylene terephthalate polyester, (b) rubbery block copolymer, (c) desiccant, wherein said desiccant is selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; and (d) poly(mono-1-olefin); optionally further with (f) light mineral oil.
Claim 4
Dependent Claim 53 words
The polyester composition consisting essentially of (a) about 50 to 90 weight percent polyalkylene terephthalate polyester, (b) rubbery block copolymer, (c) desiccant, wherein said desiccant is selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; and (d) poly(mono-1-olefin); optionally further with (f) light mineral oil.
Claim 5
Dependent Claim 55 words
The polyester composition consisting essentially of (a) about 25 to 75 weight percent polyalkylene terephthalate polyester, (b) rubbery block copolymer (c) desiccant, wherein said desiccant is selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; (d) poly(mono-1-olefin), and (e) poly(monovinylarene); optionally further with (f) light mineral oil.
Claim 6
Dependent Claim 55 words
The polyester composition consisting essentially of (a) about 25 to 75 weight percent polyalkylene terephthalate polyester, (b) rubbery block copolymer (c) desiccant, wherein said desiccant is selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; (d) poly(mono-1-olefin), and (e) poly(monovinylarene); optionally further with (f) light mineral oil.
Claim 7
Dependent Claim 16 words
The composition according to claim 1, 2, or 3 further including said (f) light mineral oil.
Claim 8
Dependent Claim 31 words
The composition of claim 1 employing about 5 to 40 weight percent (b), and about 3 to 20 weight percent (c); and where present about 0.5 to 5 weight percent (f).
Claim 9
Dependent Claim 30 words
The composition of claim 5 employing about 70-85 weight percent (a), about 10-20 weight percent (b), and about 5-10 weight percent (c); and where present about 1-2 weight percent (f).
Claim 10
Dependent Claim 39 words
The composition of claim 2 employing (a), about 3 to 30 weight percent (b), about 3 to 20 weight percent (c), and about 3 to 25 weight percent (d); and where present about 0.5 to 5 weight percent (f).
Claim 11
Dependent Claim 44 words
The composition of claim 7 employing about 60 to 80 weight percent (a), about 10 to 20 weight percent (b), about 5 to 10 weight percent (c), and about 5 to 10 percent (d); and where present about 1 to 2 weight percent (f).
Claim 12
Dependent Claim 46 words
The composition of claim 3 employing (a), about 3 to 30 weight percent (b), about 3 to 30 weight percent (c), about 10 to 35 weight percent (d), and about 3 to 30 weight percent (e); and where included about 0.5 to 5 weight percent (f).
Claim 13
Dependent Claim 52 words
The composition of claim 9 employing about 35 to 50 weight percent (a), about 10 to 20 weight percent (b), about 10 to 20 weight percent (c), about 20 to 25 weight percent (d), and about 5 to 10 weight percent (e); and where employed about 1 to 2 weight percent (f).
Claim 14
Dependent Claim 28 words
The composition of claim 1, 2, 3, 5, 6, 7, 8, 9, or 10 wherein said (a) is polyethylene terephthalate, and said (c) desiccant is a calcium oxide.
Claim 15
Dependent Claim 34 words
The composition of claim 1, 2, 3, 5, 6, 7, 8, 9, or 10, wherein said (b) is a butadiene/styrene block copolymer, said (a) is polyethylene terephthalate, and said (c) is a calcium oxide.
Claim 16
Dependent Claim 29 words
The composition of claim 2, 3, 7, 8, 9, or 10, wherein said (a) is polyethylene terephthalate, said (d) is a polyethylene, and said (c) is a calcium oxide.
Claim 17
Dependent Claim 36 words
The composition of claim 2, 3, 7, 8, 9, or 10 wherein said (a) is polyethylene terephthalate, said (b) is a butadiene/styrene block copolymer, said (d) is a polyethylene, and said (c) is a calcium oxide.
Claim 18
Dependent Claim 39 words
The composition of claim 3, 9, or 10, wherein said (a) is a polyethylene terephthalate, said (b) is a butadiene/styrene block copolymer, said (c) is a calcium oxide, said (d) is a polyethylene, and said (e) is a polystyrene.
Claim 19
Dependent Claim 21 words
The composition of any of claims 5, 6, 7, 8, 9, or 10, wherein said (a) is a PET bottle regrind.
Claim 20
Dependent Claim 74 words
A polyester blend composition consisting of: (a) about 50 to 90 weight percent polyalkylene terephthalate, (b) about 5 to 40 weight percent rubbery block copolymer of a hydrocarbon conjugated diene with a monovinylarene, and (c) about 3 to 20 weight percent of a desiccant selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; and optionally (f) about 0.5 to 5 weight percent of light mineral oil.
Claim 21
Dependent Claim 74 words
A polyester blend composition consisting of: (a) about 50 to 90 weight percent polyalkylene terephthalate, (b) about 5 to 40 weight percent rubbery block copolymer of a hydrocarbon conjugated diene with a monovinylarene, and (c) about 3 to 20 weight percent of a desiccant selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide; and optionally (f) about 0.5 to 5 weight percent of light mineral oil.
Claim 22
Dependent Claim 86 words
A polyester blend composition consisting of: (a) about 50 to 90 weight percent polyalkylene terephthalate, (b) about 3 to 30 weight percent of a rubbery block copolymer of a hydrocarbon conjugated diene with a monovinylarene, (c) about 3 to 20 weight percent of a desiccant selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide, and (d) about 3 to 25 weight percent of a poly(mono-1-olefin); and optionally (f) about 0.5 to 5 weight percent of light mineral oil.
Claim 23
Dependent Claim 86 words
A polyester blend composition consisting of: (a) about 50 to 90 weight percent polyalkylene terephthalate, (b) about 3 to 30 weight percent of a rubbery block copolymer of a hydrocarbon conjugated diene with a monovinylarene, (c) about 3 to 20 weight percent of a desiccant selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide, and (d) about 3 to 25 weight percent of a poly(mono-1-olefin); and optionally (f) about 0.5 to 5 weight percent of light mineral oil.
Claim 24
Dependent Claim 94 words
A polyester blend composition consisting of: (a) about 25 to 75 weight percent polyalkylene terephthalate, (b) about 3 to 30 weight percent of a rubbery block copolymer of a hydrocarbon conjugated diene with a monovinylarene, (c) about 3 to 20 weight percent desiccant selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide, (d) about 10 to 35 weight percent of a poly(mono-1-olefin), and (e) about 3 to 20 weight percent of a polymonovinylarene; and optionally (f) about 0.5 to 5 weight percent of light mineral oil.
Claim 25
Dependent Claim 94 words
A polyester blend composition consisting of: (a) about 25 to 75 weight percent polyalkylene terephthalate, (b) about 3 to 30 weight percent of a rubbery block copolymer of a hydrocarbon conjugated diene with a monovinylarene, (c) about 3 to 20 weight percent desiccant selected from the group consisting of calcium oxide, magnesium oxide, strontium oxide, barium oxide, and aluminum oxide, (d) about 10 to 35 weight percent of a poly(mono-1-olefin), and (e) about 3 to 20 weight percent of a polymonovinylarene; and optionally (f) about 0.5 to 5 weight percent of light mineral oil.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-11-27 1988-05-28 1988-11-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-11-27 1992-05-28 1992-11-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-11-27 1996-05-28 1996-11-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag