Patent US4148132A successfully refreshed from Google Patents.
US4148132A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of fabricating a two-phase charge coupled device
Assignee: Northrop Grumman Space and Mission Systems Corp
•
Filing: 1976-02-09
•
Granted: 1979-04-10
•
Expires: 1996-02-09
Abstract
Abstract In a charge coupled device provided with a two-phase overlapping gate structure, charge flow directionality is built into the structure by forming an asymmetrical potential well beneath each gate electrode with a single offset mask. High packing density is achieved in an array of staggered bits and with each bit being designed to have a geometry of minimum size.
Inventors
- 👤 Robert W. Bower
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 14:04
CPC Classifications
H; H10; H10D; H10D62/00; H10D62/10; H10D62/17; H10D62/213; H10D62/335; H10D84/00; H10D84/01; H10D84/0198; H10D84/02; H10D84/03; H10D84/038; H10P; H10P76/00; H10P76/40; Y; Y10; Y10S; Y10S438/00; Y10S438/981
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
336 words
A method of fabricating a two-phase charge coupled device of high component density, comprising: (a) providing a first mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to a predetermined minimum line width; (b) forming on a surface of a semiconductor substrate at least in part by means of said first mask on array of thick insulating areas separated from each other laterally by thinner insulating regions, with said thick insulating areas having corresponding lateral width and spacing substantially equal to said predetermined line width; (c) providing a second mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to said predetermined minimum line width; (d) disposing said second mask over said insulating array with its component forming areas laterally displaced from said thick insulating areas by a distance such that a portion of said component forming area overlies said thick insulating areas and the remaining portion overlies said thinner insulating regions; (e) forming on said insulating array by means of said second mask a first set of laterally spaced gate electrodes each of which covers a portion of said thick insulating areas and the remaining portion covers the adjacent portion of said thinner insulating regions, the remaining portions of said thick insulating areas and said thinner insulating regions being devoid of said gate electrodes; (f) coating with an insulating layer said first set of gate electrodes and the portions of said thinner insulating regions that are devoid of said gate electrodes; (g) removing the portions of said thick insulating areas that are devoid of said gate electrodes at least to a depth substantially below the surface of said insulating layer coating the portions of said thinner insulating regions that are devoid of said gate electrodes; and (h) depositing a second set of gate electrodes over said insulating layer referred to in clause (f) and interleaved with said first set of gate electrodes so as to overlie at least the interelectrode spaces therebetween.
Claim 2
Independent Claim
336 words
A method of fabricating a two-phase charge coupled device of high component density, comprising: (a) providing a first mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to a predetermined minimum line width; (b) forming on a surface of a semiconductor substrate at least in part by means of said first mask on array of thick insulating areas separated from each other laterally by thinner insulating regions, with said thick insulating areas having corresponding lateral width and spacing substantially equal to said predetermined line width; (c) providing a second mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to said predetermined minimum line width; (d) disposing said second mask over said insulating array with its component forming areas laterally displaced from said thick insulating areas by a distance such that a portion of said component forming area overlies said thick insulating areas and the remaining portion overlies said thinner insulating regions; (e) forming on said insulating array by means of said second mask a first set of laterally spaced gate electrodes each of which covers a portion of said thick insulating areas and the remaining portion covers the adjacent portion of said thinner insulating regions, the remaining portions of said thick insulating areas and said thinner insulating regions being devoid of said gate electrodes; (f) coating with an insulating layer said first set of gate electrodes and the portions of said thinner insulating regions that are devoid of said gate electrodes; (g) removing the portions of said thick insulating areas that are devoid of said gate electrodes at least to a depth substantially below the surface of said insulating layer coating the portions of said thinner insulating regions that are devoid of said gate electrodes; and (h) depositing a second set of gate electrodes over said insulating layer referred to in clause (f) and interleaved with said first set of gate electrodes so as to overlie at least the interelectrode spaces therebetween.
Claim 3
Dependent Claim
56 words
The invention according to claim 1, and further including, following step (c):, (i) exposing the structure thus formed to a stream of impurity ions of sufficient energy to penetrate said semiconductor surface and form an implant in the regions thereof aligned with said thinner insulating regions but without penetrating any other regions of said semiconductor surface.
Claim 4
Independent Claim
358 words
A method of fabricating a two-phase charge coupled device of high component density, comprising: (a) providing a first mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to a predetermined minimum line width; (b) forming on a surface of a semiconductor substrate at least in part by means of said mask an array of thick insulating areas separated from each other laterally by thinner insulating regions, with said thick insulating areas having corresponding lateral width and spacing substantially equal to said predetermined minimum line width; (c) providing a second mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to said predetermined minimum line width; (d) disposing said second mask over said insulating array with its component forming areas laterally displaced from said thick insulating areas by a distance such that a portion of said component forming area overlies said thick insulating areas and the remaining portion overlies said thinner insulating regions; (e) forming on said insulating array by means of said second mask a first set of laterally spaced gate electrodes each of which covers a portion of said thick insulating areas and the remaining portion covers the adjacent portion of said thinner insulating regions, the remaining portions of said thick insulating areas and said thinner insulating regions being devoid of said gate electrodes; (f) exposing the structure thus formed to a stream of impurity ions of sufficient energy to penetrate said semiconductor surface and form an implant in the regions thereof aligned with said thinner insulating regions but without penetrating any other regions of said semiconductor surface; (g) removing so much thickness of the portions of said thick insulating areas that are devoid of said gate electrodes that the remaining thickness is about the same as that of said thin insulating regions; (h) coating said first set of gate electrodes with an insulating layer; and (i) depositing a second set of gate electrodes over said insulating layer, said insulating areas, and said insulating regions and interleaved with said first set of gate electrodes so as to overlie at least the interelectrode spaces therebetween.
Claim 5
Independent Claim
358 words
A method of fabricating a two-phase charge coupled device of high component density, comprising: (a) providing a first mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to a predetermined minimum line width; (b) forming on a surface of a semiconductor substrate at least in part by means of said mask an array of thick insulating areas separated from each other laterally by thinner insulating regions, with said thick insulating areas having corresponding lateral width and spacing substantially equal to said predetermined minimum line width; (c) providing a second mask having laterally spaced component forming areas that are substantially equal in lateral width and spacing to said predetermined minimum line width; (d) disposing said second mask over said insulating array with its component forming areas laterally displaced from said thick insulating areas by a distance such that a portion of said component forming area overlies said thick insulating areas and the remaining portion overlies said thinner insulating regions; (e) forming on said insulating array by means of said second mask a first set of laterally spaced gate electrodes each of which covers a portion of said thick insulating areas and the remaining portion covers the adjacent portion of said thinner insulating regions, the remaining portions of said thick insulating areas and said thinner insulating regions being devoid of said gate electrodes; (f) exposing the structure thus formed to a stream of impurity ions of sufficient energy to penetrate said semiconductor surface and form an implant in the regions thereof aligned with said thinner insulating regions but without penetrating any other regions of said semiconductor surface; (g) removing so much thickness of the portions of said thick insulating areas that are devoid of said gate electrodes that the remaining thickness is about the same as that of said thin insulating regions; (h) coating said first set of gate electrodes with an insulating layer; and (i) depositing a second set of gate electrodes over said insulating layer, said insulating areas, and said insulating regions and interleaved with said first set of gate electrodes so as to overlie at least the interelectrode spaces therebetween.
Claim 6
Dependent Claim
51 words
The invention according to claim 3, wherein said semiconductor substrate comprises silicon of a given type semiconductivity, said thick insulating areas comprise a layer of silicon oxide and a layer of silicon nitride superimposed on said substrate in that order, and said thinner insulating regions comprise a layer of silicon oxide.
Claim 7
Dependent Claim
25 words
The invention according to claim 4, wherein said impurity ions are of the same type as is contained in the remainder of said silicon substrate.
Claim 8
Dependent Claim
35 words
The invention according to claim 3, wherein said semiconductor substrate comprises silicon of a given type semiconductivity and both said thick insulating areas and also said thinner insulating regions are formed entirely of silicon oxide.
References Cited (Backward Citations)
US3819959A
Cited
US3760202A
Cited
US3789267A
Cited
US3865652A
Cited
US3795847A
Cited
US3918997A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1982-04-09 | 1982-10-09 | 1983-04-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1986-04-09 | 1986-10-09 | 1987-04-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1990-04-09 | 1990-10-09 | 1991-04-10 | $7700.00 | Window Closed / Lapsed |