Abstract

Abstract The invention provides a non-volatile semiconductor storage apparatus wherein silicon pillars are formed by epitaxial growth thereby to suppress a dispersion in channel length and improve the quality of a gate oxide film. In production, epitaxial silicon pillars are formed by selective epitaxial growth on a p-type silicon substrate, and a gate oxide film is formed over the overall area. Polycrystalline silicon is deposited and etched back to form a first polycrystalline silicon film serving as floating gates. Ion implantation is performed to form drain regions at the tops of the epitaxial silicon pillars and form a source region on the surface of the silicon substrate. A layered insulation film is formed, and polycrystalline silicon is deposited and etched back to form a second polycrystalline silicon film which covers over the side faces of the floating gates and serves as control gates. Bit lines are formed on the drain regions.

Inventors

  • 👤 Kenji Saitoh

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 09:16
CPC Classifications
H; H10; H10B; H10B69/00; H10B20/00; H10B41/00; H10B41/30

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 262 words
A process of producing a non-volatile semiconductor apparatus, comprising steps of: forming an insulation film on a silicon substrate and forming a plurality of perforations in said insulation film; growing silicon using said insulation film as a mask to form a single crystal epitaxial layer in the form of pillars; removing entirely said insulation film to expose a surface of said silicon substrate not covered with said single crystal epitaxial layer; forming, by thermal oxidization, a first gate insulation film over an area encompassing said pillars of the single crystal epitaxial layer and a surface of said silicon substrate not covered with said single crystal epitaxial layer between said pillars; performing deposition and etching back of polycrystalline silicon to form a plurality of floating gates on side faces of said pillars of the single crystal epitaxial layer; implanting an impurity to form a diffusion layer at tops of said pillars of the single crystal epitaxial layer and the surface of said silicon substrate which is not covered with said single crystal silicon layer and said floating gates; forming a second gate insulation film on the surfaces of said floating gates; performing deposition and etching back of polycrystalline silicon to form a plurality of control gates which cover side faces of said floating gates and fill gaps between said pillars of the single crystal epitaxial layer in a direction of a row; and forming a plurality of bit lines for interconnecting said diffusion layer formed at the tops of said pillars of the single crystal epitaxial layer in a direction of a column.
Claim 2
Dependent Claim 262 words
A process of producing a non-volatile semiconductor apparatus, comprising steps of: forming an insulation film on a silicon substrate and forming a plurality of perforations in said insulation film; growing silicon using said insulation film as a mask to form a single crystal epitaxial layer in the form of pillars; removing entirely said insulation film to expose a surface of said silicon substrate not covered with said single crystal epitaxial layer; forming, by thermal oxidization, a first gate insulation film over an area encompassing said pillars of the single crystal epitaxial layer and a surface of said silicon substrate not covered with said single crystal epitaxial layer between said pillars; performing deposition and etching back of polycrystalline silicon to form a plurality of floating gates on side faces of said pillars of the single crystal epitaxial layer; implanting an impurity to form a diffusion layer at tops of said pillars of the single crystal epitaxial layer and the surface of said silicon substrate which is not covered with said single crystal silicon layer and said floating gates; forming a second gate insulation film on the surfaces of said floating gates; performing deposition and etching back of polycrystalline silicon to form a plurality of control gates which cover side faces of said floating gates and fill gaps between said pillars of the single crystal epitaxial layer in a direction of a row; and forming a plurality of bit lines for interconnecting said diffusion layer formed at the tops of said pillars of the single crystal epitaxial layer in a direction of a column.
Claim 3
Dependent Claim 47 words
A method of producing a non-volatile semiconductor apparatus as claimed in claim 1, wherein, at the growing step, said pillars of the single crystal epitaxial layer are formed with a height substantially equal to the thickness of said insulating film formed by the insulation film forming step.
Claim 4
Dependent Claim 44 words
A method of producing a non-volatile semiconductor apparatus as claimed in claim 1, wherein a distance of the gaps between said pillars of the single epitaxial layer in a direction of a column is set larger than that in a direction of a row.
Claim 5
Dependent Claim 53 words
A method of producing a non-volatile semiconductor apparatus according to claim 1, wherein said step of performing deposition and etching back of polycrystalline silicon to form a plurality of control gates which cover side faces of said floating gates forms said control gates at least 0.3 μm below the tops of said pillars.
Claim 6
Dependent Claim 45 words
Method according to claim 1, wherein said step of performing deposition and etching back of polycrystalline silicon to form a plurality of control gates which cover side faces of said floating gates forms said polycrystalline silicon along a direction of a column of said pillars.
Claim 7
Dependent Claim 73 words
Method according to claim 1, wherein said step of performing deposition and etching back of polycrystalline silicon to form a plurality of control gates which cover side faces of said floating gates forms said polycrystalline silicon along a direction of a column of said pillars, and forms a plurality of lengths of said polycrystalline silicon control gates spaced by a distance of greater than 1 μm along a row direction of said pillars.

References Cited (Backward Citations)

US5135879A Cited
US5180680A Cited
JPH06112503A Cited
US5379255A Cited
US5382540A Cited
US5460988A Cited
US5554550A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2002-04-05 2002-10-05 2003-04-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2006-04-05 2006-10-05 2007-04-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2010-04-05 2010-10-05 2011-04-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag