← Back to Patent Explorer
US5888631A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for minimizing warp in the production of electronic assemblies

Assignee: Gore Enterprise Holdings Inc
•
Filing: 1996-11-08
•
Granted: 1999-03-30
•
Expires: 2016-11-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The present invention relates to assembly techniques and the resulting products which are thermally stable, have high structural integrity, and compensate for thermal stresses that occur between the various components of the package. This is accomplished, in-part, by designing the package so that the coefficient of thermal expansion (CTE) of a stiffening ring which is mounted on the package substrate matches the CTE of the substrate and optional lid. Further, the particular adhesives used to bond the stiffening ring are chosen to match their CTE to that of the substrate, ring and lid. Moreover, the substrate is designed so that its CTE, at least in-part, matches that of the chip, and also that of the stiffening ring.

Inventors

  • 👤 Mark F. Sylvester

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 12:16
CPC Classifications
H; H05; H05K; H05K3/00; H05K3/46; H05K3/4688; H05K1/00; H05K1/02; H05K1/0271; H10; H10W; H10W40/00; H10W40/20; H10W40/25; H10W40/255; H10W70/00; H10W70/60; H10W70/67; H10W70/68; H10W70/685; H10W70/69; H05K1/0296; H05K1/0298; H05K1/18; H05K1/182; H05K1/185; H05K2201/00; H05K2201/03; H05K2201/0332; H05K2201/0335; H05K2201/0352; H05K2201/06; H05K2201/068; H05K3/4644; H05K3/4673; H05K3/4676; H10W70/681; H10W72/00; H10W72/071; H10W72/072; H10W72/07251; H10W72/20; Y; Y10; Y10T; Y10T156/00; Y10T156/10; Y10T156/1089; Y10T156/1092; Y10T428/00; Y10T428/24; Y10T428/24802; Y10T428/24917; Y10T428/24942; Y10T428/2495

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 213 words
A laminated substrate adapted for mounting a semiconductor device comprising: a plurality of dielectric and conductive layers including a core layer, said plurality of dielectric layers, conductive layers and core layer arranged in alternatingly disposed, vertically stacked dielectric and conductive layers about a plane of symmetry passing through the core layer, wherein the conductive layers and the core layer are made of copper and the dielectric layers are comprised at least in part of an expanded polytetrafluoroethylene (ePTFE), wherein the dielectric layers include first and second dielectric layers disposed respectively on opposite sides of the core layer, and the first and second dielectric layers are made of the same material, and have approximately the same thickness and the same thickness tolerance, wherein outer-most layers of the stack are conductive layers having substantially the same thickness, and the thickness of the outer-most conductive layers are thicker than any other conductive layers except for the core layer, wherein an amount of said dielectric layers have a higher elastic modulus relative to said other dielectric layers, wherein at least some of said dielectric layers having said higher elastic modulus are arranged outwardly, from said horizontal plane of symmetry, relative to said other dielectric layers such that the flexural modulus of said laminated substrate is substantially maximized.
Claim 2
Dependent Claim 213 words
A laminated substrate adapted for mounting a semiconductor device comprising: a plurality of dielectric and conductive layers including a core layer, said plurality of dielectric layers, conductive layers and core layer arranged in alternatingly disposed, vertically stacked dielectric and conductive layers about a plane of symmetry passing through the core layer, wherein the conductive layers and the core layer are made of copper and the dielectric layers are comprised at least in part of an expanded polytetrafluoroethylene (ePTFE), wherein the dielectric layers include first and second dielectric layers disposed respectively on opposite sides of the core layer, and the first and second dielectric layers are made of the same material, and have approximately the same thickness and the same thickness tolerance, wherein outer-most layers of the stack are conductive layers having substantially the same thickness, and the thickness of the outer-most conductive layers are thicker than any other conductive layers except for the core layer, wherein an amount of said dielectric layers have a higher elastic modulus relative to said other dielectric layers, wherein at least some of said dielectric layers having said higher elastic modulus are arranged outwardly, from said horizontal plane of symmetry, relative to said other dielectric layers such that the flexural modulus of said laminated substrate is substantially maximized.
Claim 3
Dependent Claim 173 words
A substrate adapted for mounting an integrated circuit chip, the substrate comprising: a centrally disposed layer of copper material having two sides and a plane of symmetry between said two sides; two layers of a first dielectric material, said first dielectric being an expanded polytetrafluoroethylene (ePTFE), each of said layers of dielectric material having a first manufacturing thickness tolerance, each of said first dielectric layers being spaced equidistantly from each other and on opposite sides of said plane of symmetry and bearing against a respective side of said centrally disposed layer; two layers of another dielectric material, said layers of said another dielectric material having a second manufacturing thickness tolerance that is less than the first manufacturing thickness tolerance, the two layers of another dielectric material being spaced equidistantly from each other and from said first dielectric material and on opposite sides of the plane of symmetry; and two layers of a metallic electrically conductive material having a third manufacturing thickness tolerance that is less than the first and second manufacturing thickness tolerances.
Claim 4
Dependent Claim 173 words
A substrate adapted for mounting an integrated circuit chip, the substrate comprising: a centrally disposed layer of copper material having two sides and a plane of symmetry between said two sides; two layers of a first dielectric material, said first dielectric being an expanded polytetrafluoroethylene (ePTFE), each of said layers of dielectric material having a first manufacturing thickness tolerance, each of said first dielectric layers being spaced equidistantly from each other and on opposite sides of said plane of symmetry and bearing against a respective side of said centrally disposed layer; two layers of another dielectric material, said layers of said another dielectric material having a second manufacturing thickness tolerance that is less than the first manufacturing thickness tolerance, the two layers of another dielectric material being spaced equidistantly from each other and from said first dielectric material and on opposite sides of the plane of symmetry; and two layers of a metallic electrically conductive material having a third manufacturing thickness tolerance that is less than the first and second manufacturing thickness tolerances.
Claim 5
Dependent Claim 18 words
The substrate according to claim 2, wherein the two layers of another dielectric further comprise bismaleimide triazine (BT)-epoxy/glass.
Claim 6
Dependent Claim 18 words
The substrate according to claim 2, wherein said two layers of metallic electrically conductive material further comprise copper.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2002-03-29 2002-09-28 2003-03-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2006-03-29 2006-09-28 2007-03-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2010-03-29 2010-09-28 2011-03-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag