Abstract

Abstract A three-terminal non-volatile ferroelectric/superconductor thin film field effect transistor (FsuFET). The FSuFET is used as a non-volatile memory storage device that provides two static states and four transient states. The FSuFET includes a superconducting film epitaxially grown on a substrate layer. A ferroelectric thin film is then epitaxially grown on the superconducting layer to form the gate of the FSuFET. A drain electrode and a source electrode are then contacted to the superconducting film on either side of the ferroelectric gate. In static mode, the two polarization states of the ferroelectric gate correspond to the binary "0" and "1" states, which are switched by applying a voltage pulse of sufficient magnitude. In transient mode, the four states depend upon the polarization state of the ferroelectric gate and the conductive state (superconducting or non-superconducting) of the drain-source channel. The four states are generated at the drain of the FSuFET and consist of a positive, high pulse; a positive, low pulse; a negative, high pulse; and a negative, low pulse.

Inventors

  • 👤 He Lin
  • 👤 Alex Ignatiev
  • 👤 Nai Juan Wu

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 01:54
CPC Classifications
H; H10; H10N; H10N60/00; H10N60/20; H10N60/205; H10N60/207

Claims Analysis

Total Claims: 23
Claim 1
Independent Claim 210 words
A non-volatile memory device, comprising: a base comprising a thin film superconductor layer having a high critical temperature, a thickness of at least 10 nm, and a top surface; a thin film ferroelectric layer epitaxially deposited on said superconductor top surface, said ferroelectric layer having a first and second polarization state; a gate electrode contacted to said ferroelectric layer; a source electrode contacted to said superconductor top surface on a first side of said ferroelectric layer; and a drain electrode contacted to said superconductor top surface on a second opposite side of said ferroelectric layer, wherein a channel region is formed in said superconductor layer under said ferroelectric layer and between said drain and source electrodes, said channel region having a resistivity that is modulated by said ferroelectric layer polarization states, wherein said ferroelectric layer being at a first polarization state causes said channel region to have a first resistivity, wherein said ferroelectric layer being at a second polarization state causes said channel region to have a second resistivity that is less than said first resistivity, wherein said ferroelectric layer retains its polarization state, and wherein said polarization state is switchable between said first and second polarization states in response to an external voltage pulse applied at said gate electrode.
Claim 2
Dependent Claim 210 words
A non-volatile memory device, comprising: a base comprising a thin film superconductor layer having a high critical temperature, a thickness of at least 10 nm, and a top surface; a thin film ferroelectric layer epitaxially deposited on said superconductor top surface, said ferroelectric layer having a first and second polarization state; a gate electrode contacted to said ferroelectric layer; a source electrode contacted to said superconductor top surface on a first side of said ferroelectric layer; and a drain electrode contacted to said superconductor top surface on a second opposite side of said ferroelectric layer, wherein a channel region is formed in said superconductor layer under said ferroelectric layer and between said drain and source electrodes, said channel region having a resistivity that is modulated by said ferroelectric layer polarization states, wherein said ferroelectric layer being at a first polarization state causes said channel region to have a first resistivity, wherein said ferroelectric layer being at a second polarization state causes said channel region to have a second resistivity that is less than said first resistivity, wherein said ferroelectric layer retains its polarization state, and wherein said polarization state is switchable between said first and second polarization states in response to an external voltage pulse applied at said gate electrode.
Claim 3
Dependent Claim 20 words
The non-volatile memory device of claim 1, wherein said second resistivity is at least 5% less than said first resistivity.
Claim 4
Dependent Claim 20 words
The non-volatile memory device of claim 1, wherein said second resistivity is at least 25% less than said first resistivity.
Claim 5
Dependent Claim 21 words
The non-volatile memory device of claim 1, wherein said ferroelectric layer retains its polarization state for at least 10 6 seconds.
Claim 6
Dependent Claim 19 words
The non-volatile memory device of claim 1, wherein said ferroelectric layer has a thickness of at least 30 nm.
Claim 7
Dependent Claim 15 words
The non-volatile memory device of claim 1, wherein said superconductor layer comprises a perovskite oxide.
Claim 8
Dependent Claim 19 words
The non-volatile memory device of claim 6, wherein said superconductor layer comprises YBa 2 Cu 3 O 7-x .
Claim 9
Dependent Claim 22 words
The non-volatile memory device of claim 1, wherein said base further includes a substrate over which said superconductor layer is epitaxially deposited.
Claim 10
Dependent Claim 14 words
The non-volatile memory device of claim 8, wherein said substrate comprises a perovskite oxide.
Claim 11
Dependent Claim 32 words
The non-volatile memory device of claim 9, wherein said substrate comprises a compound selected from the group of compounds consisting of MgO, LaAlO 3 , SrTiO 3 , and NdGaO 3 .
Claim 12
Dependent Claim 48 words
The non-volatile memory device of claim 9, wherein said substrate comprises a lower layer and a buffer layer, said buffer layer comprising a thin perovskite oxide and said lower layer comprising a compound selected from the group of compounds and elements consisting of Si, Ge, InP, and GaAs.
Claim 13
Dependent Claim 23 words
The non-volatile memory device of claim 1, wherein said ferroelectric layer is a perovskite oxide with a polarization direction normal to the substrate.
Claim 14
Dependent Claim 30 words
The non-volatile memory device of claim 12, wherein said ferroelectric layer comprises a compound selected from the group consisting of PbZrTiO 3 , (Pb,La)(Zr,Ti)O 3 , and BaSrTiO 3 .
Claim 15
Dependent Claim 21 words
The non-volatile memory device of claim 13, wherein said ferroelectric layer comprises PbZr 0 .52 Ti 0 .48 O 3 .
Claim 16
Dependent Claim 19 words
The non-volatile memory device of claim 13, wherein said ferroelectric layer has a thickness of at least 30 nm.
Claim 17
Dependent Claim 25 words
The non-volatile memory device of claim 1, wherein said channel region in said superconductor layer is switchable between a superconductive state and a normal state.
Claim 18
Dependent Claim 83 words
The non-volatile memory device of claim 16, wherein said superconductor layer has a critical current density, wherein a bias current having a first density is applied through said channel region, wherein a voltage pulse applied at said gate electrode causes a transient current having a second density to be produced in said channel region, said superconductor layer being switched from said superconductive state to said normal state if the sum of said first density and said second density exceeds said critical current density.
Claim 19
Dependent Claim 52 words
The non-volatile memory device of claim 17, wherein one of four states can be generated at said drain electrode in response to said voltage pulse, said one of four states being dependent upon said polarization state of said ferroelectric layer and whether said superconductive layer is in said superconductive or normal state.
Claim 20
Dependent Claim 35 words
The non-volatile memory device of claim 18, wherein said four states are represented as a positive, high pulse signal; a positive, low pulse signal; a negative, high pulse signal; and a negative, low pulse signal.
Claim 21
Dependent Claim 26 words
The non-volatile memory device of claim 1, wherein switching said ferroelectric layer polarization state between said first state and said second state is characterized by hysteresis.
Claim 22
Dependent Claim 37 words
The non-volatile memory device of claim 20, wherein said external voltage pulse must have a magnitude of greater than or equal to approximately 0.5 volts to switch from said second polarization state to said first polarization state.
Claim 23
Dependent Claim 37 words
The non-volatile memory device of claim 21, wherein said external voltage pulse must have a magnitude of less than or equal to approximately -0.5 volts to switch from said first polarization state to said second polarization state.

References Cited (Backward Citations)

US3832700A Cited
US5168420A Cited
US5155658A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2000-11-10 2001-05-12 2001-11-11 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2004-11-10 2005-05-12 2005-11-11 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2008-11-10 2009-05-12 2009-11-11 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag