← Back to Patent Explorer
US5475918A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of preventing deformation of lead frames

Assignee: EEJA Ltd
•
Filing: 1994-09-16
•
Granted: 1995-12-19
•
Expires: 2014-09-16
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Based on the fact that those portions of a lead frame which are liable to undergo deformation are the to-be-nonplated portions, the to-be-nonplated portions defined around the to-be-plated portions are covered with an adhesive tape or a resin film before the lead frame is subjected to a plating treatment, whereby to prevent deformation of the lead frame from the stage preceding to the surface treating step.

Inventors

  • 👤 Tsuneo Kubota
  • 👤 Kazuhiro Taniguchi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 11:30
CPC Classifications
H; H10; H10W; H10W70/00; H10W70/40; H10W70/421; H10W70/435; H10W70/456; H10W70/457; H10W72/00; H10W72/01; H10W72/0198; C; C25; C25D; C25D5/00; C25D5/02; Y; Y10; Y10S; Y10S29/00; Y10S29/012; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49121; Y10T29/49169; Y10T29/49171; Y10T29/49172

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 121 words
A method of preventing deformation of a lead frame, which comprises: defining, on a lead frame, to-be-nonplated portions around to-be-plated portions respectively, said to be plated portions including pin tips and die pads on which chips are to be mounted; providing, on an adhesive tape or a resin film to be applied to said lead frame, covering surface portions corresponding to profile of said to-be-nonplated portions of said lead frame, and openings which locate in said covering surface portions corresponding to a profile of said to-be-plated portions of said lead frame, respectively; and applying said adhesive tape or resin film to said lead frame prior to plating treatment, followed by a plating treatment of said to-be-plated portions exposed through said opening.
Claim 2
Independent Claim 121 words
A method of preventing deformation of a lead frame, which comprises: defining, on a lead frame, to-be-nonplated portions around to-be-plated portions respectively, said to be plated portions including pin tips and die pads on which chips are to be mounted; providing, on an adhesive tape or a resin film to be applied to said lead frame, covering surface portions corresponding to profile of said to-be-nonplated portions of said lead frame, and openings which locate in said covering surface portions corresponding to a profile of said to-be-plated portions of said lead frame, respectively; and applying said adhesive tape or resin film to said lead frame prior to plating treatment, followed by a plating treatment of said to-be-plated portions exposed through said opening.
Claim 3
Dependent Claim 76 words
The method of preventing deformation of a lead frame according to claim 1, wherein the shape of said openings of said adhesive tape or resin film is the same as that of said to-be-plated portions of said lead frame; said adhesive tape or resin film being applied to said lead frame with said openings registered with said to-be-plated portions of said lead frame respectively so as to cover said to-be-nonplated portions defined around said to-be-plated portions.
Claim 4
Dependent Claim 53 words
The method of preventing deformation of a lead frame according to claim 2, wherein said adhesive tape or resin film is formed by a heat-resistant resin, which is not peeled after completion of said plating treatment but embedded in a resin molding when said lead frame is subjected to a resin molding treatment.
Claim 5
Dependent Claim 20 words
The method of preventing deformation of a lead frame according to claim 3, wherein said heat-resistant resin is a polyimide.
Claim 6
Dependent Claim 53 words
The method of preventing deformation of a lead frame according to claim 2, wherein said adhesive tape or resin film is formed by a heat-resistant resin, which is not peeled after completion of said plating treatment but embedded in a resin molding when said lead frame is subjected to a resin molding treatment.
Claim 7
Dependent Claim 20 words
The method of preventing deformation of a lead frame according to claim 5, wherein said heat-resistant resin is a polyimide.
Claim 8
Independent Claim 79 words
A method of preventing deformation of a lead frame, which comprises: covering to-be-nonplated portions of a lead frame beforehand with an adhesive tape or a resin film; and applying a plating treatment to to-be-plated portions of said lead frame; wherein said adhesive tape or resin film is formed by a heat-resistant resin, which is not peeled after completion of said plating treatment but embedded in a resin molding when said lead frame is subjected to a resin molding treatment.
Claim 9
Independent Claim 79 words
A method of preventing deformation of a lead frame, which comprises: covering to-be-nonplated portions of a lead frame beforehand with an adhesive tape or a resin film; and applying a plating treatment to to-be-plated portions of said lead frame; wherein said adhesive tape or resin film is formed by a heat-resistant resin, which is not peeled after completion of said plating treatment but embedded in a resin molding when said lead frame is subjected to a resin molding treatment.
Claim 10
Dependent Claim 20 words
The method of preventing deformation of a lead frame according to claim 7, wherein said heat-resistant resin is a polyimide.
Claim 11
Independent Claim 187 words
A method of preventing deformation of a lead frame, wherein said lead frame is prevented from being deformed in a series of treatment processes from plating treatment to resin molding provided on said lead frame having die pads, to-be-plated portions, and to-be-nonplated portions, said to-be-plated portions including pin tips which are located around said die pads, said to-be-nonplated portions being located around said to-be-plated portions, said method comprising the steps of: applying a heat-resistant adhesive tape or resin film onto said lead frame prior to plating treatment, said adhesive tape or resin film having covering surface portions corresponding to the profile of said to-be-nonplated portions, and openings corresponding to the profile of said to-be-plated portions, to thereby allow said to-be-plated portions to be exposed through said openings and to provide said lead frame with a state that said to-be-nonplated portions are covered with said covering surface portions; and providing the lead frame with said series of treatment processes from plating treatment to resin molding, said resin molding having said adhesive tape or resin film embedded therein when said lead frame is subjected to a resin molding treatment.
Claim 12
Independent Claim 187 words
A method of preventing deformation of a lead frame, wherein said lead frame is prevented from being deformed in a series of treatment processes from plating treatment to resin molding provided on said lead frame having die pads, to-be-plated portions, and to-be-nonplated portions, said to-be-plated portions including pin tips which are located around said die pads, said to-be-nonplated portions being located around said to-be-plated portions, said method comprising the steps of: applying a heat-resistant adhesive tape or resin film onto said lead frame prior to plating treatment, said adhesive tape or resin film having covering surface portions corresponding to the profile of said to-be-nonplated portions, and openings corresponding to the profile of said to-be-plated portions, to thereby allow said to-be-plated portions to be exposed through said openings and to provide said lead frame with a state that said to-be-nonplated portions are covered with said covering surface portions; and providing the lead frame with said series of treatment processes from plating treatment to resin molding, said resin molding having said adhesive tape or resin film embedded therein when said lead frame is subjected to a resin molding treatment.
Claim 13
Dependent Claim 21 words
The method of preventing deformation of a lead frame according to claim 9, wherein said resin film is formed of polyimide.

References Cited (Backward Citations)

JPS60105658A Cited
US4089733A Cited
US4033844A Cited
US4835120A Cited
US4894752A Cited
JPH02156547A Cited
JPH0335589A Cited
US5227662A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1998-12-18 1999-06-19 1999-12-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2002-12-18 2003-06-19 2003-12-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2006-12-18 2007-06-19 2007-12-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag