Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
122 words
The method of stress releasing metallization in a very large scale integrated circuit (VLSI) comprising: providing semiconductor device structures in and on a semiconductor substrate within the central area of said VLSI circuit; depositing a metal line in a wavy pattern on said VLSI circuit wherein said metal line connects said semiconductor device structures to a bonding pad on the periphery of said VLSI circuit whereby: the topography of a layer underlying said metal line is shaped into a pattern comprising a repeating wave formation; and said metal line is deposited on top of said repeating wave formation pattern; and said wavy pattern of said metal line acts to release compressive stress in said substrate and tensile stress in said metal line.
Claim 2
Independent Claim
122 words
The method of stress releasing metallization in a very large scale integrated circuit (VLSI) comprising: providing semiconductor device structures in and on a semiconductor substrate within the central area of said VLSI circuit; depositing a metal line in a wavy pattern on said VLSI circuit wherein said metal line connects said semiconductor device structures to a bonding pad on the periphery of said VLSI circuit whereby: the topography of a layer underlying said metal line is shaped into a pattern comprising a repeating wave formation; and said metal line is deposited on top of said repeating wave formation pattern; and said wavy pattern of said metal line acts to release compressive stress in said substrate and tensile stress in said metal line.
Claim 3
Dependent Claim
40 words
The method of claim 1 wherein said topography of said layer underlying said metal line is shaped into said pattern comprising a repeating wave formation using one or more of the group consisting of silicon oxide, phosphosilicate glass, and polysilicon.
Claim 4
Dependent Claim
51 words
The method of claim 1 wherein said topography of said layer underlying said metal line is shaped into said pattern comprising a repeating wave formation using multiple contact openings to a large contact wherein said multiple contact openings provide substantially the same contact area as provided by said needed large contact.
Claim 5
Dependent Claim
19 words
The method of claim 1 wherein said repeating wave formation has a wavelength of between 1 to 10 microns.
Claim 6
Dependent Claim
25 words
The method of claim 1 wherein said wavy pattern is used for said metal lines only in the said periphery area of said integrated circuit.
Claim 7
Dependent Claim
31 words
The method of claim 1 wherein said wavy pattern is used for said metal lines both in the said periphery area and within the said central area of said integrated circuit.
Claim 8
Dependent Claim
17 words
The method of claim 1 wherein the thickness of said metal line is smaller than its width.
Claim 9
Dependent Claim
44 words
The method of claim 1 wherein said metal line is also deposited in a snaky pattern as well as said wavy pattern on said integrated circuit by use of an appropriate metal layer mask wherein said snaky pattern comprises a horizontally repeating wave pattern.
Claim 10
Independent Claim
116 words
The method of stress releasing metallization in a very large scale integrated circuit ( VLSI ) comprising: providing semiconductor device structures in and on a semiconductor substrate within the central area of said VLSI circuit wherein said device structures comprise at least one dielectric or passivation layer; depositing a metal line in a snaky pattern on said VLSI circuit wherein said metal line connects said semiconductor device structures to a bonding pad on the periphery of said VLSI circuit whereby an appropriate metal layer mask having a horizontally repeating wave pattern is used; and said snaky pattern of said metal line acts to release compressive stress in said substrate and tensile stress in said metal line.
Claim 11
Independent Claim
116 words
The method of stress releasing metallization in a very large scale integrated circuit ( VLSI ) comprising: providing semiconductor device structures in and on a semiconductor substrate within the central area of said VLSI circuit wherein said device structures comprise at least one dielectric or passivation layer; depositing a metal line in a snaky pattern on said VLSI circuit wherein said metal line connects said semiconductor device structures to a bonding pad on the periphery of said VLSI circuit whereby an appropriate metal layer mask having a horizontally repeating wave pattern is used; and said snaky pattern of said metal line acts to release compressive stress in said substrate and tensile stress in said metal line.
Claim 12
Dependent Claim
17 words
The method of claim 9 wherein the thickness of said metal line is larger than its width.
Claim 13
Dependent Claim
33 words
The method of claim 9 wherein said snaky metal structures also result in stress release in all said dielectric or passivation layers of said VLSI circuit to prevent stress-induced cracks, voids, extension leakage.
Claim 14
Dependent Claim
19 words
The method of claim 9 wherein said repeating wave pattern has a wavelength of between 1 to 10 microns.
Claim 15
Dependent Claim
25 words
The method of claim 9 wherein said snaky pattern is used for said metal lines only in the said periphery area of said integrated circuit.
Claim 16
Dependent Claim
31 words
The method of claim 9 wherein said snaky pattern is used for said metal lines both in the said periphery area and within the said central area of said integrated circuit.
Claim 17
Independent Claim
140 words
The method of stress releasing metallization in very a large scale integrated circuit (VLSI) wherein large contacts are needed comprising: providing semiconductor device structures in and on a semiconductor substrate; providing multiple contact openings to said large contact through a said dielectric layer wherein the combined areas of said multiple contact openings provide substantially the same contact area as provided by said needed large contact and the resulting topography of said dielectric layer in which said multiple contact openings are made is a repeating wave pattern; depositing metal lines on top of said repeating wave pattern whereby contact is made to said semiconductor device structures in and on said semiconductor substrate through said multiple contact openings; and said repeating wave pattern of said metal lines acts to release compressive stress in said substrate and tensile stress in said metal line.
Claim 18
Independent Claim
140 words
The method of stress releasing metallization in very a large scale integrated circuit (VLSI) wherein large contacts are needed comprising: providing semiconductor device structures in and on a semiconductor substrate; providing multiple contact openings to said large contact through a said dielectric layer wherein the combined areas of said multiple contact openings provide substantially the same contact area as provided by said needed large contact and the resulting topography of said dielectric layer in which said multiple contact openings are made is a repeating wave pattern; depositing metal lines on top of said repeating wave pattern whereby contact is made to said semiconductor device structures in and on said semiconductor substrate through said multiple contact openings; and said repeating wave pattern of said metal lines acts to release compressive stress in said substrate and tensile stress in said metal line.
Claim 19
Dependent Claim
35 words
The method of claim 15 wherein said wavy pattern of said metal lines also results in stress release in all dielectric or passivation layers of said VLSI circuit to prevent stress-induced cracks, voids, extension leakage.
Claim 20
Dependent Claim
44 words
The method of claim 15 wherein said metal line is also deposited in a snaky pattern as well as said wavy pattern on said integrated circuit by use of an appropriate metal layer mask wherein said snaky pattern comprises a horizontally repeating wave pattern.
Claim 21
Dependent Claim
25 words
The method of claim 17 wherein said repeating wave pattern for both wavy and snaky patterns has a wavelength of between 1 to 10 microns.