Abstract

Abstract A method for making printed circuit boards comprises using double treated copper foils for all inside conductor layers of multilayer packages with substrates of alloys of epoxy and polyphenylene oxide (PPO) resin to counteract the skin-effect encountered at high frequencies. Direct bonds between inside surfaces are then used without using an oxide step that introduces red/brown or black oxides.

Inventors

  • 👤 Arthur N. Woo
  • 👤 Paul K. Tom

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 11:35
CPC Classifications
H; H05; H05K; H05K1/00; H05K1/02; H05K1/03; H05K1/0313; H05K1/032; H05K1/0326; H05K1/0213; H05K1/0237; H05K1/0242; H05K3/00; H05K3/38; H05K3/382; H05K3/384; H05K2201/00; H05K2201/07; H05K2201/0707; H05K2201/0715; H05K2203/00; H05K2203/03; H05K2203/0392; H05K3/46; H05K3/4611; H05K3/4644; H05K3/4652

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 79 words
A method for fabricating a multilayer printed circuit board (PCB) package, the method comprising the steps of: bonding double-treated copper foil to a substrate of an alloy of epoxy and polyphenylene oxide (PPO) resin to form a first laminate; etching a circuit pattern in said double-treated copper foil; and direct bonding under heat and pressure the double-treated copper foil side of said first laminate to a second laminate comprised of an alloy of epoxy and polyphenylene oxide (PPO) resin.
Claim 2
Independent Claim 79 words
A method for fabricating a multilayer printed circuit board (PCB) package, the method comprising the steps of: bonding double-treated copper foil to a substrate of an alloy of epoxy and polyphenylene oxide (PPO) resin to form a first laminate; etching a circuit pattern in said double-treated copper foil; and direct bonding under heat and pressure the double-treated copper foil side of said first laminate to a second laminate comprised of an alloy of epoxy and polyphenylene oxide (PPO) resin.
Claim 3
Dependent Claim 35 words
The method of claim 1 wherein: the step of direct bonding comprises stripping developed dry film to create traces mimicking film patterns and then proceeding directly to drying said first laminate to remove excess moisture.
Claim 4
Dependent Claim 19 words
The method of claim 1, further comprising the step of: precleaning said first laminate before the step of etching.
Claim 5
Dependent Claim 81 words
The method of claim 3, wherein the step of precleaning comprises the constituent steps of: baking said first laminate in an air-circulating oven for approximately four hours at 325° F.; dipping said first laminate in a preplating cleaner; rinsing said first laminate in water; dipping the laminates in a microetch solution; rinsing said first laminate in water; dipping said first laminate in a copper conditioning bath; rinsing said first laminate in water; and drying said first laminate in an air dryer.

References Cited (Backward Citations)

US3177103A Cited
US4659425A Cited
US4917758A Cited
US4902556A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-12-06 1997-06-07 1997-12-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-12-06 2001-06-07 2001-12-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-12-06 2005-06-07 2005-12-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag