← Back to Patent Explorer
US5200388A Expired / Lapsed US ⏱️ 0.0 years remaining

Metalorganic chemical vapor deposition of superconducting films

Assignee: Oki Electric Industry Co Ltd
•
Filing: 1990-06-22
•
Granted: 1993-04-06
•
Expires: 2010-06-22
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An oxide superconducting film is formed by CVD. The starting material gas sources are Ba(DPM) 2 , Ba(DPM) 2 ·(THF) n or Ba(DPM) 2 ·(DMF) n ; Cu(DPM) 2 , Cu(DPM) 2 ·(THF) n or Cu(DPM) 2 ·(DMF) n ; and M(DPM) 3 , M(DPM) 3 ·(THF) n or M(DPM) 3 ·(DMF) n , where DPM is 2,2,6,6-tetramethyl-3,5-heptaneodianate represented by the chemical formula: CH.sub.3 C(CH.sub.3).sub.2 COCHCOC(CH.sub.3).sub.2 CH.sub.3 THF is tetrahydrofuran represented by the chemical formula: ##STR1## DMF is dimethylformamide represented by the chemical formula: HCON(CH.sub.3).sub.2 M is an element chosen from the list: Y, La, Nd, Pm, Sm, Eu, Er, Gd, Tb, Dy, Ho, Tm, Yb and Lu, and n is any integer. The starting gas sources are introduced into a growth tank after gasification together with at least one of the gases O 2 , O 3 , or N 2 O, and the oxide film being formed on a substrate placed in said growth tank.

Inventors

  • 👤 Hitoshi Abe
  • 👤 Tomohiro Nakamori

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 06:57
CPC Classifications
C; C23; C23C; C23C16/00; C23C16/22; C23C16/30; C23C16/40; C23C16/408; H; H10; H10N; H10N60/00; H10N60/01; H10N60/0268; H10N60/0296; H10N60/0436; H10N60/0464; Y; Y10; Y10S; Y10S505/00; Y10S505/725; Y10S505/73; Y10S505/734

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 219 words
A process for forming a superconducting film on a substrate using chemical vapor deposition wherein the superconducting film exhibits a zero resistance at a temperature of at least 80° K., said process comprising the steps of: (a) heating said substrate upon which said superconducting film is to be formed; (b) providing the following source materials: (1) one of the compounds Ba(DPM) 2 ·(THF).sub.η or Ba(DPM) 2 ·(DMF).sub.η, (2) one of the compounds Cu(DPM) 2 ·(THF).sub.η or Cu(DPM) 2 ·(DMF).sub.η, and (3) one of the compounds M(DPM) 3 ·(THF).sub.η or M(DPM) 3 ·(DMF).sub.η, where DPM is 2, 2, 6, 6-tetramethyl-3,5-heptaneodianate represented by the chemical formula CH.sub.3 c(CH.sub.3).sub.2 COCHCOC(CH.sub.3).sub.2 CH.sub.3 where THF is tetrahydrofuran represented by the chemical formula: ##STR5## where DMF is dimethylformamide represented by the chemical formula CHON(CH 3 ) 2 where M is an element chosen from the list: Y, La, Nd, Pm, Sm, Eu, Er, Gd, Tb, Dy, Ho, Tm, Yb or Lu, and where n is any integer; (c) gasifying said source materials to form first gases; (d) introducing said first gases into a growth tank; and (e) simultaneously introducing at least one of the following second gases O 2 , O 3 , or N 2 O to said tank whereby an oxide superconducting film is formed on said substrate located in said growth tank.
Claim 2
Dependent Claim 219 words
A process for forming a superconducting film on a substrate using chemical vapor deposition wherein the superconducting film exhibits a zero resistance at a temperature of at least 80° K., said process comprising the steps of: (a) heating said substrate upon which said superconducting film is to be formed; (b) providing the following source materials: (1) one of the compounds Ba(DPM) 2 ·(THF).sub.η or Ba(DPM) 2 ·(DMF).sub.η, (2) one of the compounds Cu(DPM) 2 ·(THF).sub.η or Cu(DPM) 2 ·(DMF).sub.η, and (3) one of the compounds M(DPM) 3 ·(THF).sub.η or M(DPM) 3 ·(DMF).sub.η, where DPM is 2, 2, 6, 6-tetramethyl-3,5-heptaneodianate represented by the chemical formula CH.sub.3 c(CH.sub.3).sub.2 COCHCOC(CH.sub.3).sub.2 CH.sub.3 where THF is tetrahydrofuran represented by the chemical formula: ##STR5## where DMF is dimethylformamide represented by the chemical formula CHON(CH 3 ) 2 where M is an element chosen from the list: Y, La, Nd, Pm, Sm, Eu, Er, Gd, Tb, Dy, Ho, Tm, Yb or Lu, and where n is any integer; (c) gasifying said source materials to form first gases; (d) introducing said first gases into a growth tank; and (e) simultaneously introducing at least one of the following second gases O 2 , O 3 , or N 2 O to said tank whereby an oxide superconducting film is formed on said substrate located in said growth tank.
Claim 3
Dependent Claim 15 words
A process according to claim 1 further including radiating said growth tank with electromagnetic radiation.
Claim 4
Dependent Claim 21 words
A process according to claim 1 further including ozonizing said second gas by means of RF heating coil or UV lamp.
Claim 5
Dependent Claim 32 words
A process according to claim 1, wherein the growth of the superconductor film in said CVD method is carried out under conditions to permit formation of one molecular layer at a time.
Claim 6
Dependent Claim 19 words
The process of claim 1 wherein said superconduct film exhibits a zero resistance between 80° K. and 91° K.

References Cited (Backward Citations)

US4501602A Cited
US4626449A Cited
JPS61141420A Cited
US4751149A Cited
US4812325A Cited
WO1989003594A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-04-05 1996-10-05 1997-04-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-04-05 2000-10-05 2001-04-06 $3760.00 Window Closed / Lapsed