Abstract

Abstract Disclosed is a method for making self-aligned metal contacts on semiconductor devices, with a submicronic spacing between regions controlled by the contacts. On a semiconductor body supporting at least one raised pattern, a double layer of SiO 2 and Si 3 N 4 is deposited by an isotropic method. A double ionic etching of Si 3 N 4 by SF 6 and of SiO 2 by CHF 3 is done to insulate the sidewalls on the flanks of the pattern. A sub-etching by HF/NH 4 F/H 2 O creates a cap beneath each sidewall. The metal contacts, deposited by evaporation, are self-aligned and separated by a space "d" equal to the thickness of the insulating layers.

Inventors

  • 👤 Philippe Collot
  • 👤 Paul Schmidt

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 04:14
CPC Classifications
H; H10; H10W; H10W20/00; H10W20/01; H10W20/031; H10W20/069; H10D; H10D30/00; H10D30/01; H10D30/051; H10P; H10P50/00; H10P50/20; H10P50/28; H10P50/282; H10P50/283; H10D62/00; H10D62/80; H10D62/85; Y; Y10; Y10S; Y10S148/00; Y10S148/14

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 250 words
A method for self-alignment of metal electron contacts on a semiconductor device comprising at least one raised pattern on a semiconductor body, said method comprising the following operations: depositing by an isotropic method, on free surfaces of the body and of the pattern, including a lateral surface and flanks of said pattern, of a first insulating layer of silica SiO 2 and then a second insulating layer of silicon nitride Si 3 N 4 with well-controlled thicknesses, anisotropic, reactive ion etching, by SF 6 , of the second layer in its parts deposited on the free surfaces of the body and on top of the pattern, portions of said second layer deposited on the flanks of the pattern remaining unetched, anisotropic, reactive ion etching, by CHF 3 , of the first layer, with the exception of its portions deposited on the flanks of the pattern, which are masked by the corresponding portions of the second layer; selective and isotropic chemical etching, by a buffered solution of HF/NH 4 F/H 2 O, of the first layer, this etching operation creating a sub-etching in the portions of the first layer that are partially masked by the corresponding portions of the second layer not etched by said selective solution, self-aligned metallization, by a directional method, of the metal electrode contacts of the semiconductor device, the juxtaposed portions of the first and second insulating layers on the flanks of the pattern constituting sidewalls between regions of the semiconductor device controlled by two neighboring metallizations.
Claim 2
Independent Claim 250 words
A method for self-alignment of metal electron contacts on a semiconductor device comprising at least one raised pattern on a semiconductor body, said method comprising the following operations: depositing by an isotropic method, on free surfaces of the body and of the pattern, including a lateral surface and flanks of said pattern, of a first insulating layer of silica SiO 2 and then a second insulating layer of silicon nitride Si 3 N 4 with well-controlled thicknesses, anisotropic, reactive ion etching, by SF 6 , of the second layer in its parts deposited on the free surfaces of the body and on top of the pattern, portions of said second layer deposited on the flanks of the pattern remaining unetched, anisotropic, reactive ion etching, by CHF 3 , of the first layer, with the exception of its portions deposited on the flanks of the pattern, which are masked by the corresponding portions of the second layer; selective and isotropic chemical etching, by a buffered solution of HF/NH 4 F/H 2 O, of the first layer, this etching operation creating a sub-etching in the portions of the first layer that are partially masked by the corresponding portions of the second layer not etched by said selective solution, self-aligned metallization, by a directional method, of the metal electrode contacts of the semiconductor device, the juxtaposed portions of the first and second insulating layers on the flanks of the pattern constituting sidewalls between regions of the semiconductor device controlled by two neighboring metallizations.
Claim 3
Dependent Claim 28 words
A method according to claim 1 wherein the first and second insulating layers have a submicronic total thickness and the sidewalls have a thickness "d" which is submicronic.
Claim 4
Dependent Claim 27 words
A method according to claim 1, wherein at least one thin-layer metallization is provided as an additional coating of metal in order to finish its electrical resistance.
Claim 5
Independent Claim 275 words
A method for self-alignment of metal electrode contacts on a semiconductor device wherein one of said contacts is a Schottky type gate and said semiconductor device includes at least one raised pattern on a semiconductor body, said method comprising the steps of: metaling said Schottky type gate contact; depositing by an isotropic method, on free surfaces of the body and of the pattern, including a lateral surface and flanks of said pattern, of a first insulating layer of silica SiO 2 and subsequently a second insulating layer of silicon nitride Si 3 N 4 with well-controlled thicknesses; anisotropic, reactive ion etching, by SF 6 , of the second layer and its parts deposited on the free surfaces of the body and on top of the pattern, portions of said layer deposited on the flanks of the pattern remaining unetched; anisotropic, reactive ion etching, by CHF 3 ,f of the first layer, with the exception of its portion deposited on the flanks of the pattern, which are masked by the corresponding portions of the second layer; selective and isotropic chemical etching, by buffered solution of HF/NH 4 F/H 2 O, of the first layer, said etching operation creating a sub-etching in the portions of the first layer that are partially masked by the corresponding portions of the second layer not etched by said selective solution; self-aligned metallization, by a directional method, of the metal electrode contacts not including said Schottky type contact, of the semiconductor device, the juxtaposed portions of the first and second insulating layers on the flanks of the pattern constituting side walls between regions of the semiconductor device controlled by two neighboring metallizations.
Claim 6
Independent Claim 275 words
A method for self-alignment of metal electrode contacts on a semiconductor device wherein one of said contacts is a Schottky type gate and said semiconductor device includes at least one raised pattern on a semiconductor body, said method comprising the steps of: metaling said Schottky type gate contact; depositing by an isotropic method, on free surfaces of the body and of the pattern, including a lateral surface and flanks of said pattern, of a first insulating layer of silica SiO 2 and subsequently a second insulating layer of silicon nitride Si 3 N 4 with well-controlled thicknesses; anisotropic, reactive ion etching, by SF 6 , of the second layer and its parts deposited on the free surfaces of the body and on top of the pattern, portions of said layer deposited on the flanks of the pattern remaining unetched; anisotropic, reactive ion etching, by CHF 3 ,f of the first layer, with the exception of its portion deposited on the flanks of the pattern, which are masked by the corresponding portions of the second layer; selective and isotropic chemical etching, by buffered solution of HF/NH 4 F/H 2 O, of the first layer, said etching operation creating a sub-etching in the portions of the first layer that are partially masked by the corresponding portions of the second layer not etched by said selective solution; self-aligned metallization, by a directional method, of the metal electrode contacts not including said Schottky type contact, of the semiconductor device, the juxtaposed portions of the first and second insulating layers on the flanks of the pattern constituting side walls between regions of the semiconductor device controlled by two neighboring metallizations.

References Cited (Backward Citations)

EP0111706A1 Cited
US4587710A Cited
US4735680A Cited
JPS63257231A Cited
US4908326A Cited
US4925807A Cited
US4886765A Cited
US5015598A Cited
US5015599A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-04-05 1996-10-05 1997-04-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-04-05 2000-10-05 2001-04-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-04-05 2004-10-05 2005-04-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag