Claims Analysis
Total Claims: 20
Claim 1
Independent Claim
101 words
A delaminated stratified paper towel comprising: a first layer of chemical fiber blend; and a second layer of an anfractuous high bulk softwood fiber blend, unitary with said first layer; said first layer being constructed of a denser chemical softwood and hardwood fiber blend relative to said second layer; said second layer having approximately 30% to 43% of the anfractuous fiber and approximately 57% to 70% of long mechanical pulp fiber; wherein said first and second layers enhance a rate of absorption and water capacity as compared to a towel of equal strength not having a layer of anfractuous fiber blend.
Claim 2
Dependent Claim
101 words
A delaminated stratified paper towel comprising: a first layer of chemical fiber blend; and a second layer of an anfractuous high bulk softwood fiber blend, unitary with said first layer; said first layer being constructed of a denser chemical softwood and hardwood fiber blend relative to said second layer; said second layer having approximately 30% to 43% of the anfractuous fiber and approximately 57% to 70% of long mechanical pulp fiber; wherein said first and second layers enhance a rate of absorption and water capacity as compared to a towel of equal strength not having a layer of anfractuous fiber blend.
Claim 3
Dependent Claim
28 words
The delaminated stratified paper towel according to claim 1, wherein said second layer is a fiber blend of the anfractuous fiber and a fiber derived from chemi-thermomechanical pulp.
Claim 4
Dependent Claim
19 words
The delaminated stratified paper towel according to claim 2, wherein said anfractuous fiber is a citric acid treated fiber.
Claim 5
Dependent Claim
33 words
The delaminated stratified paper towel according to claim 1, wherein the weight of the first layer is approximately 65% of the total weight of the paper towel and the second layer, approximately 35%.
Claim 6
Dependent Claim
25 words
The delaminated stratified paper towel according to claim 4, wherein the first layer includes approximately 70% Kraft softwood and approximately 30% Kraft hardwood by weight.
Claim 7
Dependent Claim
26 words
The delaminated stratified paper towel according to claim 1, wherein the average water holding capacity of each ply of the paper towel is approximately 9.5 gm/gm.
Claim 8
Dependent Claim
27 words
The delaminated stratified paper towel according to claim 6, wherein the average water absorption time of each ply of the finished paper towel is approximately 11 seconds.
Claim 9
Dependent Claim
39 words
The delaminated stratified paper towel according to claim 1, wherein two plies of the paper towel are embossed together to an emboss depth of approximately 0.2286 cm, the water holding capacity of the paper towel being approximately 12.4 gm/gm.
Claim 10
Dependent Claim
19 words
The delaminated stratified paper towel according to claim 9, wherein the average water absorption time is approximately 0.8 seconds.
Claim 11
Dependent Claim
30 words
The delaminated stratified paper towel according to claim 1, and further including a third layer of fiber blend wherein said second layer is disposed between said first and third layers.
Claim 12
Dependent Claim
36 words
The delaminated stratified paper towel according to claim 10, wherein the total weight of the first and third layers is approximately 65% of the total weight of the paper towel and the second layer, approximately 35%.
Claim 13
Dependent Claim
27 words
The delaminated stratified paper towel according to claim 12, wherein the first and third layers include approximately 70% Kraft softwood and approximately 30% Kraft hardwood by weight.
Claim 14
Dependent Claim
19 words
The delaminated stratified paper towel according to claim 11, wherein the anfractuous fiber is a citric acid treated fiber.
Claim 15
Independent Claim
148 words
A method of forming a delaminated stratified web of paper towel material comprising: supplying a first aqueous furnish of a blend of chemical softwood and hardwood fiber directly to a wire; supplying a second aqueous furnish of an anfractuous high bulk softwood fiber blend having approximately 30% to 43% of the anfractuous fiber and approximately 57% to 70% of long mechanical pulp fiber onto the first furnish disposed on the wire; drying the first and second furnishes on a drying means to form a web of paper towel material having a predetermined dryness; creping the paper towel material off of the drying means; and embossing the paper towel material to a predetermined emboss depth; wherein the web of paper towel material has an enhanced rate of absorption and water holding capacity as compared to a towel of equal strength not having a layer of bulky anfractuous fiber blend.
Claim 16
Independent Claim
148 words
A method of forming a delaminated stratified web of paper towel material comprising: supplying a first aqueous furnish of a blend of chemical softwood and hardwood fiber directly to a wire; supplying a second aqueous furnish of an anfractuous high bulk softwood fiber blend having approximately 30% to 43% of the anfractuous fiber and approximately 57% to 70% of long mechanical pulp fiber onto the first furnish disposed on the wire; drying the first and second furnishes on a drying means to form a web of paper towel material having a predetermined dryness; creping the paper towel material off of the drying means; and embossing the paper towel material to a predetermined emboss depth; wherein the web of paper towel material has an enhanced rate of absorption and water holding capacity as compared to a towel of equal strength not having a layer of bulky anfractuous fiber blend.
Claim 17
Dependent Claim
35 words
The method of forming a delaminated stratified web of paper towel material according to claim 14, wherein said second furnish is a fiber blend of the anfractuous fiber and a fiber derived from chemi-thermomechanical pulp.
Claim 18
Dependent Claim
26 words
The method of forming a delaminated stratified web of paper towel material according to claim 15, wherein said anfractuous fiber is a citric acid treated fiber.
Claim 19
Dependent Claim
44 words
The method of forming a delaminated stratified web of paper towel material according to claim 14, wherein the weight of the layer resulting from the first furnish is approximately 65% of the weight of the paper towel material and the second layer, approximately 35%.
Claim 20
Dependent Claim
32 words
The method of forming a delaminated stratified web of paper towel material according to claim 19, wherein the first furnish includes approximately 70% Kraft softwood and approximately 30% Kraft hardwood by weight.