← Back to Patent Explorer
US5012324A Expired / Lapsed US ⏱️ 0.0 years remaining

Flat body, particularly for use as a heat sink for electronic power components

Assignee: Doduco Solutions GmbH
•
Filing: 1988-06-27
•
Granted: 1991-04-30
•
Expires: 2008-06-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract PCT No. PCT/EP88/00564 Sec. 371 Date Feb. 24, 1989 Sec. 102(e) Date Feb. 24, 1989 PCT Filed Jun. 27, 1988 PCT Pub. No. WO89/00339 PCT Pub. Date Jan. 12, 1989.The bodies consist of a ceramic slab (1), which is covered on both sides by metal plates (2, 3), which are firmly bonded to the ceramic slab (1) throughout their contact surface without an interlayer and have marginal strips (5) which are reduced in thickness.

Inventors

  • 👤 Wolfram Martin
  • 👤 Brigitte Waibel

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 06:56
CPC Classifications
H; H10; H10W; H10W40/00; H10W40/20; H10W40/25; H10W40/255; H10W40/22; H10W40/226; F; F02; F02B; F02B1/00; F02B1/02; F02B1/04

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 68 words
A flat body, particularly for use as a heat sink for electronic power components, consisting of a ceramic slab, which is covered on both sides by metal plates which are firmly joined to the ceramic slab throughout their contact surface, characterized in that the metal plates have provided on at least two edges of the peripheral margins, a strip reduced in thickness to improve resistance to thermal shock.
Claim 2
Dependent Claim 68 words
A flat body, particularly for use as a heat sink for electronic power components, consisting of a ceramic slab, which is covered on both sides by metal plates which are firmly joined to the ceramic slab throughout their contact surface, characterized in that the metal plates have provided on at least two edges of the peripheral margins, a strip reduced in thickness to improve resistance to thermal shock.
Claim 3
Dependent Claim 22 words
A body according to claim 1, characterized in that the two metal plates are joined to the ceramic slab without an interlayer.
Claim 4
Dependent Claim 25 words
A body according to claim 1, characterized in that the metal plates attached to both sides of the ceramic slab are arranged to be coextensive.
Claim 5
Dependent Claim 22 words
A body according to claim 1, characterized in that the metal plates attached to both sides of the ceramic slab are identical.
Claim 6
Dependent Claim 16 words
A body according to claim 1, characterized in that the metal plates are made of copper.
Claim 7
Dependent Claim 18 words
A body according to claim 1, characterized in that the marginal strips of the metal plates are beveled.
Claim 8
Dependent Claim 28 words
A body according to claim 6, characterized in that the marginal strips are beveled at an angle of about 20 ° to the surface of the ceramic slab.
Claim 9
Dependent Claim 18 words
A body according to claim 1, characterized in that the marginal strips of the metal plates are stepped.
Claim 10
Dependent Claim 31 words
A body according to claim 8, characterized in that the marginal strips are stepped once and have a reduced thickness of 40% to 50% of the thickness of the metal plates.
Claim 11
Dependent Claim 32 words
A body according to claim 1, characterized in that the marginal strips have a reduced thickness and have a width which is 1 to 3 times the thickness of the metal plates.
Claim 12
Dependent Claim 25 words
A body according to claim 1, characterized in that the metal plates and the ceramic plates have a thickness of 0.5 mm to 1 mm.
Claim 13
Dependent Claim 28 words
A body according to claim 9, characterized in that the marginal strips have a reduced thickness of about 45 per cent of the thickness of the metal plates.
Claim 14
Dependent Claim 27 words
A body according to claim 10, characterized in that the marginal strips have a width which is 1.5 to 2 times the thickness of the metal plates.
Claim 15
Dependent Claim 32 words
A body according to claim 9, characterized in that the marginal strips have a reduced thickness and have a width which is 1 to 3 times the thickness of the metal plates.
Claim 16
Dependent Claim 67 words
A flat body, particularly for use as a heat sink for electronic power components, consisting of a ceramic slab which is covered on both sides by metal plates which are firmly joined to the ceramic slab throughout their contact surface, characterized in that the metal plates are smaller in planar size than said ceramic slab to define marginal strips extending about the peripheries of said metal plates.
Claim 17
Dependent Claim 67 words
A flat body, particularly for use as a heat sink for electronic power components, consisting of a ceramic slab which is covered on both sides by metal plates which are firmly joined to the ceramic slab throughout their contact surface, characterized in that the metal plates are smaller in planar size than said ceramic slab to define marginal strips extending about the peripheries of said metal plates.
Claim 18
Dependent Claim 16 words
A body according to claim 15, characterized in that peripheral edges of said plates are beveled.
Claim 19
Dependent Claim 20 words
A body according to claim 15, characterized in that at least two opposed peripheral edges of said plates are stepped.

References Cited (Backward Citations)

US3717798A Cited
US3829598A Cited
US4556899A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-04-29 1994-10-29 1995-04-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-04-29 1998-10-29 1999-04-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-04-29 2002-10-29 2003-04-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag