Polysilicon photoconductor for integrated circuits
Assignee: United States Department of Energy
•
Filing: 1989-02-23
•
Granted: 1990-08-14
•
Expires: 2009-02-23
Abstract
Abstract A photoconductive element of polycrystalline silicon is provided with intrinsic response time which does not limit overall circuit response. An undoped polycrystalline silicon layer is deposited by LPCVD to a selected thickness on silicon dioxide. The deposited polycrystalline silicon is then annealed at a selected temperature and for a time effective to obtain crystal sizes effective to produce an enhanced current output. The annealed polycrystalline layer is subsequently exposed and damaged by ion implantation to a damage factor effective to obtain a fast photoconductive response.
Inventors
- 👤 Robert B. Hammond
- 👤 Douglas R. Bowman
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-08 05:09
CPC Classifications
H; H10; H10F; H10F71/00; H10F71/121; H10F30/00; H10F30/10; H10F39/00; H10F39/10; H10F77/00; H10F77/10; H10F77/16; H10F77/162; H10F77/164; H10F77/1642; Y; Y02; Y02E; Y02E10/00; Y02E10/50; Y02E10/546; Y02E10/547; Y02P; Y02P70/00; Y02P70/50
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
182 words
A process for producing at least one photoconductive element on a bulk silicon substrate comprising: a. forming a silicon dioxide layer on said bulk silicon substrate at each location selected for a photoconductive element; b. depositing at each of said selected locations a layer of polycrystalline silicon, which is insulatively separated from said bulk silicon by said silicon dioxide layer and which serves as a sensing element; c. annealing said deposits of polycrystalline silicon, said anneal being effective to increase output current of a photoconductive element and being carried out at a temperature in the range of from about 1000° to about 1200° C. for a time period of about one hour; d. providing electrically conductive means which contact each of said polycrystalline silicon deposits and which define an optical access gas above each of said polycrystalline silicon deposits; e. subjecting each of said polycrystalline silicon deposits to damage consisting of ion implantation which is effective to adjust response time of the photoconductive element, said response time being proportional to the damage caused to the polycrystalline silicon deposits by said ion implantation.
Claim 2
Dependent Claim
182 words
A process for producing at least one photoconductive element on a bulk silicon substrate comprising: a. forming a silicon dioxide layer on said bulk silicon substrate at each location selected for a photoconductive element; b. depositing at each of said selected locations a layer of polycrystalline silicon, which is insulatively separated from said bulk silicon by said silicon dioxide layer and which serves as a sensing element; c. annealing said deposits of polycrystalline silicon, said anneal being effective to increase output current of a photoconductive element and being carried out at a temperature in the range of from about 1000° to about 1200° C. for a time period of about one hour; d. providing electrically conductive means which contact each of said polycrystalline silicon deposits and which define an optical access gas above each of said polycrystalline silicon deposits; e. subjecting each of said polycrystalline silicon deposits to damage consisting of ion implantation which is effective to adjust response time of the photoconductive element, said response time being proportional to the damage caused to the polycrystalline silicon deposits by said ion implantation.
Claim 3
Dependent Claim
27 words
The process of claim 1 where said deposits of polycrystalline silicon are deposited by an LPCVD process and the thickness of each deposit is about 0.5 micron.
Claim 4
Dependent Claim
13 words
The process of claim 1 where said annealing temperature is about 1.150° C.
References Cited (Backward Citations)
US4155785A
Cited
JPS5654058A
Cited
US4370175A
Cited
US4454526A
Cited
US4412900A
Cited
JPS59111368A
Cited
US4531143A
Cited
US4821091A
Cited
JPH09574A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-08-13 | 1994-02-12 | 1994-08-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-08-13 | 1998-02-12 | 1998-08-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-08-13 | 2002-02-12 | 2002-08-14 | $7700.00 | Window Closed / Lapsed |