US4726710A Expired / Lapsed US ⏱️ 0.0 years remaining

Co-disposal pollution control method

Assignee: WOLF RIDGE Corp A CORP OF Co
•
Filing: 1986-06-16
•
Granted: 1988-02-23
•
Expires: 2006-06-16
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Process for disposal of fossil fuel ash by addition thereto of sodium salts, preferably sodium sulfur oxide salt Na2SOx where x is 3 and/or 4, in an amount ranging from 5-85 weight percent (dry basis) and adjusting the water percentage to within the range of 6-35%, preferably 15-28%. The coefficient of permeability of the ash and sodium salt is reduced from 102 cm/sec to the "impermeable" standard of 10-6 and below. The preferred mixes also call for a smectite clay additive present in the range of from 0.1% to 5%. A flocculant in amounts of 0.01% to 1% can be substituted for about 3-5% of the water content. A principal source of the Na2SOx is sodium FGD waste, preferably from the use of Nahcolite (a natural mineral form of sodium bicarbonate) as an SOx sorbent in the Nahcolite FGD process. The resulting co-disposal process simultaneously renders the highly soluble Na2SOx (102 g/L) and ash impermeable, and suitable for geomorphologically stable landfill disposal by known techniques to heights in excess of 200'.

Inventors

  • 👤 Edward C. Rosar
  • 👤 Maurice G. Pattengill

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 14:37
CPC Classifications
C; C04; C04B; C04B28/00; C04B28/18; C04B28/184; C04B28/02; C04B28/021; C04B2111/00; C04B2111/00474; C04B2111/00767; C04B2111/00784; Y; Y02; Y02W; Y02W30/00; Y02W30/50; Y02W30/91; Y10; Y10S; Y10S106/00; Y10S106/01

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 143 words
A method of preparing waste fossil fuel ash for disposal comprising the steps of: (a) providing waste fossil fuel ash; (b) introducing a sodium sulfur oxide salt compound into said ash in the range of from about 5 to 85 weight % on a dry basis; (c) said sodium sulfur oxide salt compound being selected from Na 2 SO x , where x is 3 or 4, NaHCO 3 , and mixtures thereof; (d) said sodium sulfur oxide compound and said ash comprising an ash/sodium oxide salt composite; and (e) adjusting the water content of said composite to have from about 15 to about 28% by weight water content to produce a substantially homogenous, substantially impermeable wetted composite mass in non-pellet form having a coefficient of permeability value below about 10 -6 cm/sec suitable for substantially solid mass landfill disposal without heat sintering.
Claim 2
Independent Claim 143 words
A method of preparing waste fossil fuel ash for disposal comprising the steps of: (a) providing waste fossil fuel ash; (b) introducing a sodium sulfur oxide salt compound into said ash in the range of from about 5 to 85 weight % on a dry basis; (c) said sodium sulfur oxide salt compound being selected from Na 2 SO x , where x is 3 or 4, NaHCO 3 , and mixtures thereof; (d) said sodium sulfur oxide compound and said ash comprising an ash/sodium oxide salt composite; and (e) adjusting the water content of said composite to have from about 15 to about 28% by weight water content to produce a substantially homogenous, substantially impermeable wetted composite mass in non-pellet form having a coefficient of permeability value below about 10 -6 cm/sec suitable for substantially solid mass landfill disposal without heat sintering.
Claim 3
Dependent Claim 52 words
A method as in claim 1 which includes the added step of: (a) mixing said composite with a source of smectite clay in an amount in the range of below about 5 weight percent dry basis, in the presence of sufficient water to produce an additive-enhanced wetted composite having said water content.
Claim 4
Dependent Claim 34 words
A method as in claim 2 which includes the added step of: (a) permitting said wetted composite to swell for a holding period of time sufficient that swelling substantially ceases before disposal is completed.
Claim 5
Dependent Claim 22 words
A method as in claim 2 wherein: (a) amount of water is an amount sufficient to produce a composite of dough-like texture.
Claim 6
Dependent Claim 27 words
A method as in claim 1 wherein: (a) said wetted composite is let set for a time sufficient to achieve a penetration resistance of about 4.5 tons/sq.ft.
Claim 7
Dependent Claim 22 words
A method as in claim 2 which includes the added step of: (a) disposing of said additive-enhanced composite in a compacted landfill.
Claim 8
Dependent Claim 19 words
A method as in claim 2 wherein: (a) said ash is a mixture of fly ash and bottom ash.
Claim 9
Dependent Claim 34 words
A method as in claim 7 wherein: (a) said bottom ash is present in an amount of up to about 80% by weight of the entire ash mixture, and the balance is fly ash.
Claim 10
Dependent Claim 30 words
A method as in claim 8 wherein: (a) said bottom ash comprises ash particles of size on the order of 60% by weight less than 10 US standard sieve mesh.
Claim 11
Dependent Claim 18 words
A method as in claim 3 wherein: (a) said hold time is on the order of 0.5-8 hours.
Claim 12
Dependent Claim 34 words
A method as in claim 2 wherein: (a) at least a portion of said water content is achieved by adding water to at least one of said clay, said composite and said additive-enhanced composite.
Claim 13
Dependent Claim 41 words
A method as in claim 11 wherein: (a) a substantial portion of the water required to be added to achieve said water content is added to said clay to form a clay slurry, and said slurry is added to said composite.
Claim 14
Dependent Claim 37 words
A method as in claim 2 wherein: (a) said Na 2 SO x is introduced in said fly ash by injection of a dry sodium sorbent into the flue gas duct of an industrial or utility boiler.
Claim 15
Dependent Claim 27 words
A method as in claim 13 wherein: (a) said dry sodium sorbent is selected from Nahcolite, sodium bicarbonate, soda ash, trona, sodium sesquicarbonate, Wegscheiderite, or mixtures thereof.
Claim 16
Dependent Claim 14 words
A method as in claim 14 wherein: (a) said sodium sorbent is solution-mined Nahcolite.
Claim 17
Dependent Claim 33 words
A method as in claim 1 wherein: (a) up to about 3% of said water is replaced by a flocculant in an amount of up to 1 dry weight percent of said mix.
Claim 18
Dependent Claim 33 words
A method as in claim 2 wherein: (a) up to about 3% of said water is replaced by a flocculant in an amount of up to 1 dry weight percent of said mix.
Claim 19
Dependent Claim 23 words
A method as in claim 1 wherein: (a) said smectite clay is present in an amount of up to about 3 weight %.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-02-22 1991-08-24 1992-02-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-02-22 1995-08-24 1996-02-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-02-22 1999-08-24 2000-02-23 $7700.00 Window Closed / Lapsed