US4663430A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for the preparation of high molecular weight polyarylene sulphide in the absence of water
Assignee: Bayer AG
•
Filing: 1986-01-02
•
Granted: 1987-05-05
•
Expires: 2006-01-02
Abstract
Abstract This invention relates to a process for the preparation of high molecular weight, optionally branched polyarylene sulphides. These may be prepared from alkali metal sulphides and aromatic halogen compounds in a polar organic solvent in the absence of water.
Inventors
- 👤 Edgar Ostlinning
- 👤 Karsten Idel
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 14:50
CPC Classifications
C; C08; C08G; C08G75/00; C08G75/02; C08G75/0204; C08G75/025; C08G75/0254; C08G75/0231
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
270 words
Process for the preparation of high molecular weight polyarylene sulphide having a viscosity of from 0.3×10 3 to 5×10 6 Pascal units which comprises reacting in the absence of water (a) 0-100 mol-% of at least one aromatic dihalogen compound corresponding to the formula ##STR3## and 100-0 mol-% of at least one aromatic dihalogen compound corresponding to the formula ##STR4## wherein X represents halogens in the meta- or para-position to each other and R 1 , which is identical or different, represents hydrogen, alkyl, cycloalkyl, aryl, alkylaryl or arylalkyl and two groups R 1 in the ortho-position to each other are linked together to form an aromatic or heterocyclic ring and one group R 1 is invariably different from hydrogen and (b) 0-5 mol-% based on the sum of components (a) and (b), of an aromatic trihalogen or tetrahalogen compound corresponding to the formula ArX.sub.n (III) wherein Ar represents an aromatic or heterocyclic group, X represents chlorine or bromine and n represents 3 or 4, and (c) alkali metal sulphide alone or together with alkali metal hydroxide, the molar ratio of (a+b):c is within the range of 0.85:1 to 1.15:1, and (d) in an organic solvent which is an N-alkyllactam having a boiling point above 200° C., characterized in that the molar ratio of alkali metal sulphide (c) to organic solvent (d) is within the range of 1:2 to 1:15 and the alkali metal sulphide is dehydrated either solvent-free or in a polar organic solvent with or without the aid of an inert H 2 O carrier before addition of the aromatic halogen compounds of formulae I, II or III.
Claim 2
Dependent Claim
270 words
Process for the preparation of high molecular weight polyarylene sulphide having a viscosity of from 0.3×10 3 to 5×10 6 Pascal units which comprises reacting in the absence of water (a) 0-100 mol-% of at least one aromatic dihalogen compound corresponding to the formula ##STR3## and 100-0 mol-% of at least one aromatic dihalogen compound corresponding to the formula ##STR4## wherein X represents halogens in the meta- or para-position to each other and R 1 , which is identical or different, represents hydrogen, alkyl, cycloalkyl, aryl, alkylaryl or arylalkyl and two groups R 1 in the ortho-position to each other are linked together to form an aromatic or heterocyclic ring and one group R 1 is invariably different from hydrogen and (b) 0-5 mol-% based on the sum of components (a) and (b), of an aromatic trihalogen or tetrahalogen compound corresponding to the formula ArX.sub.n (III) wherein Ar represents an aromatic or heterocyclic group, X represents chlorine or bromine and n represents 3 or 4, and (c) alkali metal sulphide alone or together with alkali metal hydroxide, the molar ratio of (a+b):c is within the range of 0.85:1 to 1.15:1, and (d) in an organic solvent which is an N-alkyllactam having a boiling point above 200° C., characterized in that the molar ratio of alkali metal sulphide (c) to organic solvent (d) is within the range of 1:2 to 1:15 and the alkali metal sulphide is dehydrated either solvent-free or in a polar organic solvent with or without the aid of an inert H 2 O carrier before addition of the aromatic halogen compounds of formulae I, II or III.
Claim 3
Dependent Claim
15 words
Process according to claim 1 wherein the reaction temperature is from 170° to 270° C.
Claim 4
Dependent Claim
14 words
Process according to claim 1 wherein the polar organic solvent is N-methylcaprolactam or N-ethylcaprolactam.
Claim 5
Dependent Claim
14 words
Process according to claim 1 wherein (d) further comprises, N,N-dialkylcarboxylic acid amide as cosolvent.
Claim 6
Dependent Claim
11 words
Process according to claim 1 wherein toluene is the inert carrier.
References Cited (Backward Citations)
US3354129A
Cited
DE1620923A1
Cited
US4232142A
Cited
US4064114A
Cited
EP0065689A1
Cited
US4433138A
Cited
US4371671A
Cited
EP0073525A1
Cited
US4368321A
Cited
EP0086487A1
Cited
EP0100536A2
Cited
US4595748A
Cited
US4598144A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1990-05-04 | 1990-11-03 | 1991-05-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1994-05-04 | 1994-11-03 | 1995-05-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1998-05-04 | 1998-11-03 | 1999-05-05 | $7700.00 | Window Closed / Lapsed |