Abstract

Abstract A technique for enclosing microelectronic circuit elements in hermetically sealed packages comprising a planar ceramic substrate with a box-like ceramic cover sealed thereto by a fused glass coating. The glass sealant is applied to the substrate in the form of a paste which thereafter is fired at high temperature and cooled to produce a smooth glass coating. With the cover in place on the substrate, the glass coating is remelted by heat developed by infra-red radiation impinging on all sides of the package structure from heaters in an infra-red furnace. A reflective shield on top of the cover reduces the inflow of heat through that surface, and a heat sink beneath the substrate removes heat, thereby to reduce the temperature rise experienced by circuit elements in the package interior.

Inventors

  • 👤 Delip R. Bokil
  • 👤 Tanjore R. Narasimhan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 19:08
CPC Classifications
H; H10; H10W; H10W95/00; H10W76/00; H10W76/60

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 206 words
The method of packaging temperature-sensitive microelectronic devices, including hybrid integrated circuits, supported on a rigid hermetic planar substrate, comprising the steps of: applying a meltable hermetic sealing material along a closed path defined by the interface between said substrate and a hermetic box-like cover surrounding the region for said microelectronic devices; placing on said substrate said hermetic box-like cover having side walls aligned with and contacting said sealing material completely around said closed path; directing infra-red radiation towards both said substrate and said cover from all sides thereof, said radiation striking the regions of both said cover and said substrate which are adjacent the interface therebetween; shielding the top surfaces of said cover by means reflecting the radiation directed towards said top surfaces; withdrawing heat from the lower surfaces of said substrate by heat sink means; said radiation being applied simultaneously to all sides of the package structure for a time sufficient to melt said sealing material and to provide for fusion and/or bonding thereof with said substrate and said cover; and removing said infra-red radiation to permit the melted sealing material to cool in a fused and/or bonded state with both said substrate and said cover to assure effective hermetic sealing of the completed package.
Claim 2
Independent Claim 206 words
The method of packaging temperature-sensitive microelectronic devices, including hybrid integrated circuits, supported on a rigid hermetic planar substrate, comprising the steps of: applying a meltable hermetic sealing material along a closed path defined by the interface between said substrate and a hermetic box-like cover surrounding the region for said microelectronic devices; placing on said substrate said hermetic box-like cover having side walls aligned with and contacting said sealing material completely around said closed path; directing infra-red radiation towards both said substrate and said cover from all sides thereof, said radiation striking the regions of both said cover and said substrate which are adjacent the interface therebetween; shielding the top surfaces of said cover by means reflecting the radiation directed towards said top surfaces; withdrawing heat from the lower surfaces of said substrate by heat sink means; said radiation being applied simultaneously to all sides of the package structure for a time sufficient to melt said sealing material and to provide for fusion and/or bonding thereof with said substrate and said cover; and removing said infra-red radiation to permit the melted sealing material to cool in a fused and/or bonded state with both said substrate and said cover to assure effective hermetic sealing of the completed package.
Claim 3
Dependent Claim 18 words
The method of claim 1, wherein said substrate, said cover, and said sealing material are all electrically non-conductive.
Claim 4
Dependent Claim 16 words
The method of claim 2, wherein said substrate and said cover are formed of ceramic material.
Claim 5
Dependent Claim 13 words
The method of claim 3, wherein said sealing material is a glass frit.
Claim 6
Dependent Claim 54 words
The method of claim 4, wherein said glass frit first is fired at high temperature to produce a smooth glass coating in the areas to be sealed; said substrate being free of temperature-sensitive devices during the firing of said glass frit; and fabricating temperature-sensitive devices on said substrate before carrying out said radiation-sealing procedure.

References Cited (Backward Citations)

US3283124A Cited
US3404215A Cited
US3683146A Cited
US3937388A Cited
US4291815A Cited
US4291815B1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-11-13 1988-05-14 1988-11-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-11-13 1992-05-14 1992-11-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-11-13 1996-05-14 1996-11-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag