Pinned ceramic substrate
Assignee: International Business Machines Corp
•
Filing: 1981-04-10
•
Granted: 1984-02-28
•
Expires: 2001-04-10
Abstract
Abstract Ceramic substrates are pinned using powdered metallurgy pins formed in situ on the substrate.
Inventors
- 👤 Russell E. Darrow
- 👤 Joseph Funari
- 👤 George S. Kotrch
- 👤 George C. Phillips
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 09:56
CPC Classifications
H; H05; H05K; H05K13/00; H05K13/04; H05K3/00; H05K3/22; H05K3/24; H05K3/245; H05K1/00; H05K1/02; H05K1/09; H05K1/092; H05K2201/00; H05K2201/03; H05K2201/0332; H05K2201/0364; H05K2201/0367; H05K2201/09; H05K2201/09209; H05K2201/09372; H05K2201/09481; H05K3/40; H05K3/4007; H05K3/4038; H05K3/4053; H05K3/4061; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49124; Y10T29/49147; Y10T29/49151; Y10T29/49153; Y10T29/49155; Y10T29/49165; Y10T29/49167; Y10T29/49204; Y10T29/49206; Y10T29/49208; Y10T29/49222
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
276 words
A method for making a pinned ceramic substrate having plural pins outwardly extending from at least one predetermined surface thereof, said method comprising the steps of: providing a ceramic substrate having a plurality of first holes to be pinned, said first holes inwardly extending from a predetermined first surface of said substrate, filling said first holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, providing a vaporizable carrier having a corresponding plurality of second holes inwardly extending from a predetermined second surface thereof, juxtaposing said first and second surfaces in a predetermined contacting relationship with each other, each one of said first holes being paired with a mutually exclusive one of said second holes and being in a predetermined registration relationship therewith when said first and second surfaces are in said predetermined contacting relationship, filling said second holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, and providing a heat treatment to sinter said unsintered powdered metal particles of said first and second holes and to evaporate away said binder thereof, whereby said powdered metal particles in each one of said paired first and second holes is fused to form one of said pins affixed to said substrate and said carrier is evaporated away by said heat treatment, said binders and said carrier being evaporated away within the temperature range of 250 to 400 degrees C., and said powdered metal particles being sintered at a temperature greater than 400 degrees C., and said ceramic substrate and said powdered metal particles having compatible shrinkage characteristics, and said ceramic substrate and said powdered metal particles having compatible firing and sintering temperatures, respectively.
Claim 2
Independent Claim
276 words
A method for making a pinned ceramic substrate having plural pins outwardly extending from at least one predetermined surface thereof, said method comprising the steps of: providing a ceramic substrate having a plurality of first holes to be pinned, said first holes inwardly extending from a predetermined first surface of said substrate, filling said first holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, providing a vaporizable carrier having a corresponding plurality of second holes inwardly extending from a predetermined second surface thereof, juxtaposing said first and second surfaces in a predetermined contacting relationship with each other, each one of said first holes being paired with a mutually exclusive one of said second holes and being in a predetermined registration relationship therewith when said first and second surfaces are in said predetermined contacting relationship, filling said second holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, and providing a heat treatment to sinter said unsintered powdered metal particles of said first and second holes and to evaporate away said binder thereof, whereby said powdered metal particles in each one of said paired first and second holes is fused to form one of said pins affixed to said substrate and said carrier is evaporated away by said heat treatment, said binders and said carrier being evaporated away within the temperature range of 250 to 400 degrees C., and said powdered metal particles being sintered at a temperature greater than 400 degrees C., and said ceramic substrate and said powdered metal particles having compatible shrinkage characteristics, and said ceramic substrate and said powdered metal particles having compatible firing and sintering temperatures, respectively.
Claim 3
Dependent Claim
21 words
The method according to claim 1 wherein said ceramic substrate is uncured, said ceramic substrate being cured during said heat treatment.
Claim 4
Independent Claim
297 words
A method for making a pinned ceramic substrate having plural pins outwardly extending from at least one predetermined surface thereof, said method comprising the steps of: providing a ceramic substrate having a plurality of first holes to be pinned, said first holes inwardly extending from a predetermined first surface of said substrate, filling said first holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, providing a first heat treatment to sinter said unsintered powdered metal particles of said first holes and to evaporate said binder thereof, providing a vaporizable carrier having a corresponding plurality of second holes inwardly extending from a predetermined second surface thereof, juxtaposing said first and second surfaces in a predetermined contacting relationship with each other, each one of said first holes being paired with a mutually exclusive one of said second holes and being in a predetermined registration relationship therewith when said first and second surfaces are in said predetermined contacting relationship, filling said second holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, and providing a second heat treatment to sinter said unsintered powdered metal particles of said second holes and to evaporate said binder thereof, whereby said powdered metal particles in each one of said paired first and second holes is fused to form one of said pins affixed to said substrate and said carrier is evaporated away by said second heat treatment, said binders and said carrier being evaporated away within the temperature range of 250 to 400 degrees C., and said powdered metal particles being sintered at a temperature greater than 400 degrees C., and said ceramic substrate and said powdered metal particles having compatible shrinkage characteristics, and said ceramic substrate and said powdered metal particles having compatible firing and sintering temperatures, respectively.
Claim 5
Independent Claim
297 words
A method for making a pinned ceramic substrate having plural pins outwardly extending from at least one predetermined surface thereof, said method comprising the steps of: providing a ceramic substrate having a plurality of first holes to be pinned, said first holes inwardly extending from a predetermined first surface of said substrate, filling said first holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, providing a first heat treatment to sinter said unsintered powdered metal particles of said first holes and to evaporate said binder thereof, providing a vaporizable carrier having a corresponding plurality of second holes inwardly extending from a predetermined second surface thereof, juxtaposing said first and second surfaces in a predetermined contacting relationship with each other, each one of said first holes being paired with a mutually exclusive one of said second holes and being in a predetermined registration relationship therewith when said first and second surfaces are in said predetermined contacting relationship, filling said second holes with unsintered powdered metal particles in a temporary non-elastomer paste-like binder, and providing a second heat treatment to sinter said unsintered powdered metal particles of said second holes and to evaporate said binder thereof, whereby said powdered metal particles in each one of said paired first and second holes is fused to form one of said pins affixed to said substrate and said carrier is evaporated away by said second heat treatment, said binders and said carrier being evaporated away within the temperature range of 250 to 400 degrees C., and said powdered metal particles being sintered at a temperature greater than 400 degrees C., and said ceramic substrate and said powdered metal particles having compatible shrinkage characteristics, and said ceramic substrate and said powdered metal particles having compatible firing and sintering temperatures, respectively.
Claim 6
Dependent Claim
22 words
The method according to claim 3 wherein said ceramic substrate is uncured, said ceramic substrate being cured during said first heat treatment.
Claim 7
Dependent Claim
13 words
The method according to claim 3 wherein said mold is an acetal composition.
Claim 8
Dependent Claim
22 words
The method according to claim 1 or 3 wherein said binder is a composition of diethylene glycol butyl ether and ethyl cellulose.
Claim 9
Dependent Claim
45 words
The method according to claim 1 or 3 wherein said ceramic has a composition comprising 96.0% Al 2 O 3 , 0.5% MgO, 0.5% CaO, and 3.0% SiO 2 , and wherein said powdered metal particles are from the group consisting of molybdenum and tungsten.
References Cited (Backward Citations)
US349572A
Cited
US786257A
Cited
US936403A
Cited
US930723A
Cited
US1701342A
Cited
US2412925A
Cited
US2464437A
Cited
US3049795A
Cited
US3201858A
Cited
US3216097A
Cited
US3372474A
Cited
US3374110A
Cited
US3257708A
Cited
US3540894A
Cited
US3539876A
Cited
US3518756A
Cited
US3561110A
Cited
US3768134A
Cited
US3735466A
Cited
US3846823A
Cited
US3736651A
Cited
US4024629A
Cited
US4050756A
Cited
US4092697A
Cited
US4082394A
Cited
US4067104A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-02-27 | 1987-08-29 | 1988-02-28 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-02-27 | 1991-08-29 | 1992-02-28 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-02-27 | 1995-08-29 | 1996-02-28 | $7700.00 | Window Closed / Lapsed |