Abstract

Abstract The instant invention is directed to shear thickening fluids which comprise a water-swellable material (clay), present in a sufficient concentration so as to be capable of forming a stiff paste upon interaction with the water used, and water wherein the clay and water are kept separated by an intervening hydrocarbon-surfactant composition. The intervening oil phase prevents the interaction between the water and the clay phases and results in a stable, nonreacting, pumpable composite until such time as the oil envelope is ruptured by application of a sufficiently high shear force. Upon such rupture, the materials interact rapidly forming a semi-rigid stiff paste. Various well-control problems, such as oil and gas with blowouts, can be controlled by use of the above-described composite. The composite is pumped down the well pipe. Exiting the orifices of the drill bit or a nozzle supplies the shear force needed to rupture the oil envelope thereby permitting the interaction between the clay and the water resulting in the formation of a stiff paste which can stop or prevent unwanted flow in or near the wellbore.

Inventors

  • 👤 Charles R. Dawson
  • 👤 Norman N. Li
  • 👤 Dennis E. O'Brien

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 12:07
CPC Classifications
C; C09; C09K; C09K8/00; C09K8/50; C09K8/502; C09K8/516

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 134 words
A method for treating a well penetrating a subterranean formation by blocking off unwanted flow paths comprising introducing into said well a shear thickening composite stable to pumping comprising a water swellable material, capable of rapidly forming a high strength paste when mixed with water, an oil-surfactant phase and water wherein the water swellable material, present in sufficient quantity so as to form a paste having a strength of at least 2000 lb/100 ft 2 , and the water are kept separated by the intervening oil-surfactant phase, subjecting said shear thickening composite to shear forces sufficient to mix the water swellable material and the water, and mixing the water swellable material and the water causing the water swellable material to thicken rapidly into a high strength semi-rigid paste which blocks off unwanted flow paths.
Claim 2
Independent Claim 134 words
A method for treating a well penetrating a subterranean formation by blocking off unwanted flow paths comprising introducing into said well a shear thickening composite stable to pumping comprising a water swellable material, capable of rapidly forming a high strength paste when mixed with water, an oil-surfactant phase and water wherein the water swellable material, present in sufficient quantity so as to form a paste having a strength of at least 2000 lb/100 ft 2 , and the water are kept separated by the intervening oil-surfactant phase, subjecting said shear thickening composite to shear forces sufficient to mix the water swellable material and the water, and mixing the water swellable material and the water causing the water swellable material to thicken rapidly into a high strength semi-rigid paste which blocks off unwanted flow paths.
Claim 3
Dependent Claim 29 words
The method of claim 1 wherein the high shear mixing consists of passing the shear thickening fluid through the orifices of a drill bit or nozzle in the well.
Claim 4
Dependent Claim 14 words
The method of claim 1 wherein the waterswellable material is bentonite or attapulgite clay.
Claim 5
Dependent Claim 33 words
The method of claim 1 wherein the shear thickneing composite is 100 parts by weight (pbw) clay, 150 to 400 pbw water, 50 to 150 pbw oil and 5 to 50 pbw surfactant.
Claim 6
Dependent Claim 142 words
The method of claim 4 wherein the clay is montmorillonite clay or attapulgite clay, the oil is mineral oil, C 6 to C 1000 paraffinic oil, motor oil and substituted paraffinic oil wherein the substitutents are selected from the group consisting of halogens, amines, sulfates, nitrates, carboxylates and hydroxyls and the surfactant is the product obtained by the reaction of the polyamine ##STR5## wherein R 3 , R 4 , R 5 , R 6 , R 7 , R 8 , R 9 and y are chosen from the group consisting of hydrogen, C 1 to C 20 alkyl, C 6 to C 20 aryl, C 7 to C 20 alkaryl radicals and substituted derivatives thereof, and x is an integer of from 1 to 100 with polyalkenyl succinic anhydrides, reaction proceding at the R 3 , R 4 substituted nitrogen.
Claim 7
Dependent Claim 98 words
The method of claim 5 wherein the surfactant is represented by the general formula: ##STR6## wherein n varies from 10 to 60, preferably 10 to 30, most preferably 15-17, x varies from 1 to 100, preferably 3 to 10, R 5 , R 6 , R 7 , R 8 and R 9 are hydrogen C 1 to C 20 alkyl, C 6 to C 20 aryl, C 7 to C 20 alkaryl radical and substituted derivative thereof, and y is selected from the group consisting of hydrogen and oxygen containing hydrocarbyl radicals having up to 10 carbons.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-08-08 1987-02-07 1987-08-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-08-08 1991-02-07 1991-08-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-08-08 1995-02-07 1995-08-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag