Abstract
Abstract The process of making an ingot for use as a feed stock for a coating process in which the ingot is vaporized to produce the coating material; the ingot being made by forming a billet of the alloy minus the reactive element with a rod of the reactive element of the alloy extending centrally through the billet and then shaping the billet to ingot size, the cross-sectional area of the rod having the same relation of the remainder of the area of the billet as the percentage of the reactive element in the alloy.
Inventors
- 👤 Richard C. Elam
- 👤 Nicholas E. Ulion
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 08:51
CPC Classifications
C; C23; C23C; C23C14/00; C23C14/22; C23C14/24; C23C14/28; C23C14/30; B; B22; B22F; B22F7/00; B22F7/06; Y; Y10; Y10S; Y10S29/00; Y10S29/025; Y10T; Y10T29/00; Y10T29/49; Y10T29/4998; Y10T29/49988; Y10T428/00; Y10T428/12; Y10T428/12222; Y10T428/29; Y10T428/2913; Y10T428/2927; Y10T428/2973; Y10T428/2975
Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
304 words
In the production of an ingot of a selected cross-sectional dimension for use in crucible vaporization for a coating process, the ingot being an alloy having a reactive element as one constituent, the alloy without the reactive element being workable and the reactive element being workable, the complete alloy with the reactive element therein however being much less workable, the completed ingot being fed axially through an opening in the crucible for vaporization to produce a coating vapor having the elements of the alloy in the desired proportions including the reactive element, the crucible having an opening to receive the ingot, the steps of: forming an elongated billet having the ingredients of and in the proportions of the alloy and without the reactive element included therein; making a hole from end to end of the ingot, this hole having an area related to the area of the billet substantially the same as the percentage of reactive element in the alloy; positioning a rod of the reactive element within the billet, said rod having a cross-sectional area related to the area of the billet the same as the proportion of the reactive element in the alloy, said rod extending axially of the billet from end to end; reducing the billet from its formed size to an ingot having a shape and dimension to fit the opening in the crucible so that it may be fed therethrough and the cross section of the ingot having all the ingredients of the alloy in proper proportion therein, the ratio of the cross-sectional area of the rod in the ingot to the cross-sectional area of the ingot being comparable to the desired percent of the reactive element in the remainder of the alloy; and feeding the completed ingot through said opening in the crucible for vaporization into an alloy.
Claim 2
Dependent Claim
304 words
In the production of an ingot of a selected cross-sectional dimension for use in crucible vaporization for a coating process, the ingot being an alloy having a reactive element as one constituent, the alloy without the reactive element being workable and the reactive element being workable, the complete alloy with the reactive element therein however being much less workable, the completed ingot being fed axially through an opening in the crucible for vaporization to produce a coating vapor having the elements of the alloy in the desired proportions including the reactive element, the crucible having an opening to receive the ingot, the steps of: forming an elongated billet having the ingredients of and in the proportions of the alloy and without the reactive element included therein; making a hole from end to end of the ingot, this hole having an area related to the area of the billet substantially the same as the percentage of reactive element in the alloy; positioning a rod of the reactive element within the billet, said rod having a cross-sectional area related to the area of the billet the same as the proportion of the reactive element in the alloy, said rod extending axially of the billet from end to end; reducing the billet from its formed size to an ingot having a shape and dimension to fit the opening in the crucible so that it may be fed therethrough and the cross section of the ingot having all the ingredients of the alloy in proper proportion therein, the ratio of the cross-sectional area of the rod in the ingot to the cross-sectional area of the ingot being comparable to the desired percent of the reactive element in the remainder of the alloy; and feeding the completed ingot through said opening in the crucible for vaporization into an alloy.
Claim 3
Dependent Claim
28 words
The process of claim 1 in which the reactive element is yttrium and the alloy includes chromium and aluminum with one or more of iron, nickel and cobalt.
Claim 4
Dependent Claim
167 words
In the production of an ingot for use in a coating process in which the ingot is vaporized from a crucible to form a vapor for coating, the ingot being an alloy one element of which is reactive, and in which the alloy is not readily workable whereas the reactive element alone is workable and the alloy minus the reactive element is workable, the steps of: forming an elongated billet of the ingredients of the alloy minus the reactive element and in the proportions of these ingredients in the alloy; positioning a rod of the reactive element within the billet; forming the billet to the shape and dimension of an ingot to fit in the crucible, the ratio of the cross-sectional area of the rod to the cross-sectional area of the ingot being comparable to the percentage of reactive element in the alloy; and melting the ingot in the crucible to form a vapor having the ingredients of the alloy in required proportions to form a coating.
Claim 5
Dependent Claim
167 words
In the production of an ingot for use in a coating process in which the ingot is vaporized from a crucible to form a vapor for coating, the ingot being an alloy one element of which is reactive, and in which the alloy is not readily workable whereas the reactive element alone is workable and the alloy minus the reactive element is workable, the steps of: forming an elongated billet of the ingredients of the alloy minus the reactive element and in the proportions of these ingredients in the alloy; positioning a rod of the reactive element within the billet; forming the billet to the shape and dimension of an ingot to fit in the crucible, the ratio of the cross-sectional area of the rod to the cross-sectional area of the ingot being comparable to the percentage of reactive element in the alloy; and melting the ingot in the crucible to form a vapor having the ingredients of the alloy in required proportions to form a coating.
Claim 6
Dependent Claim
37 words
The process of claim 3 in which the billet is formed by encapsulating powdered alloy, the rod is positioned in the encapsulated alloy and the billet is then reduced to ingot dimension by hot isostatic pressure technique.
Claim 7
Dependent Claim
27 words
The process of claim 3 with the additional step of forming an axial opening through the billet from end to receive the rod of the reactive element.
Claim 8
Dependent Claim
15 words
The process of claim 5 in which the opening is located centrally of the billet.
Claim 9
Dependent Claim
22 words
The process of claim 3 in which the billet with the rod therein is formed by extrusion to ingot shape and dimension.
Claim 10
Dependent Claim
24 words
The process of claim 3 in which the alloy includes chromium, aluminum, and yttrium, with one or more of iron, nickel and cobalt therein.
References Cited (Backward Citations)
US2628516A
Cited
US2595292A
Cited
US3168399A
Cited
GB933500A
Cited
US3262858A
Cited
US3271849A
Cited
US3162530A
Cited
US3565602A
Cited
US3564940A
Cited
US3667421A
Cited
US3938964A
Cited
US3892030A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-09-04 | 1982-03-06 | 1982-09-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-09-04 | 1986-03-06 | 1986-09-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-09-04 | 1990-03-06 | 1990-09-05 | $7700.00 | Window Closed / Lapsed |