Thin film device and method for manufacturing thin film device

Assignee: Western Digital Technologies Inc
•
Filing: 2000-05-12
•
Granted: 2002-06-18
•
Expires: 2020-05-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract As an electrically conductive layer or a lower layer of conductor layers to be patterned, a conductor layer which is dry-etchable with an oxygen-containing gas is provided. A dry etching process of the conductor layer with the oxygen-containing gas is performed highly selectively to a ground film.

Inventors

  • 👤 Tadashi Kimura
  • 👤 Isao Muragishi
  • 👤 Hiroyoshi Sekiguchi
  • 👤 Masaya Sakaguchi
  • 👤 Hiroyasu Tsuji
  • 👤 Satoru Mitani

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 12:09
CPC Classifications
B; B82; B82Y; B82Y25/00; C; C23; C23F; C23F4/00; B82Y10/00; G; G11; G11B; G11B5/00; G11B5/127; G11B5/31; G11B5/3163; G11B5/33; G11B5/39; G11B5/3903; G11B5/3906; G11B5/3909; H; H01; H01F; H01F41/00; H01F41/32; H01F41/34; H10; H10D; H10D30/00; H10D30/60; H10D30/67; H10D30/6729; H10D30/6737; H10D30/6739; H10P; H10P50/00; H10P50/20; H10P50/26; H10P50/264; H10P50/266; H10P50/267; G11B2005/3996; G11B5/3109; G11B5/3116; G11B5/313

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 142 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer and a first gap film both formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: depositing a film of Ru or RuO 2 , which film is to serve as the pair of lead electrodes; forming an etching mask pattern on said film of Ru or RuO 2 ; and then performing dry etching of said film of Ru or RuO 2 with plasma of a gas containing at least oxygen.
Claim 2
Independent Claim 142 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer and a first gap film both formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: depositing a film of Ru or RuO 2 , which film is to serve as the pair of lead electrodes; forming an etching mask pattern on said film of Ru or RuO 2 ; and then performing dry etching of said film of Ru or RuO 2 with plasma of a gas containing at least oxygen.
Claim 3
Dependent Claim 71 words
The method for manufacturing a thin film device according to claim 1 , wherein forming the etching mask pattern on said film of Ru or RuO 2 includes: depositing a film of SiO 2 or SiN on said film of Ru or RuO 2 ; then forming a resist pattern on said film of SiO 2 or SiN by photolithography; and then dry etching said film of SiO 2 or SiN.
Claim 4
Dependent Claim 35 words
The method for manufacturing a thin film device according to claim 2 , wherein said film of SiO 2 or SiN is used as part of an insulating film on the pair of lead electrodes.
Claim 5
Independent Claim 201 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer and a first gap film both formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: depositing at least two conductor layers on the magnetoresistive element portion, with one of the at least two conductor layers being in contact with the magnetoresistive element and being an Ru or RuO 2 layer, wherein said at least two conductor layers are to serve as the pair of lead electrodes; forming an etching mask pattern on said at least two conductor layers; then dry etching another of said at least two conductor layers, that is separated from the magnetoresistive element portion by the Ru or RuO 2 layer, with plasma of a gas containing halogen; and then dry etching the Ru or RuO 2 layer with plasma of a gas containing at least oxygen.
Claim 6
Independent Claim 201 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer and a first gap film both formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: depositing at least two conductor layers on the magnetoresistive element portion, with one of the at least two conductor layers being in contact with the magnetoresistive element and being an Ru or RuO 2 layer, wherein said at least two conductor layers are to serve as the pair of lead electrodes; forming an etching mask pattern on said at least two conductor layers; then dry etching another of said at least two conductor layers, that is separated from the magnetoresistive element portion by the Ru or RuO 2 layer, with plasma of a gas containing halogen; and then dry etching the Ru or RuO 2 layer with plasma of a gas containing at least oxygen.
Claim 7
Dependent Claim 46 words
The method according to claim 4 , wherein said another of said at least two conductor layers comprises a layer of any of W, Ta, Rh, Cr, Al and Ir, or a layer of an alloy containing any of W, Ta, Rh, Cr, Al and Ir.
Claim 8
Independent Claim 184 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer and a first gap film both formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: forming an Ru layer on one side of the magnetoresistive element that is to be closer to the pair of lead electrodes; patterning the magnetoresistive element, and patterning the permanent magnetic domain control layer at both end portions of the magnetoresistive element in the track width direction; then depositing a film that is to serve as the pair of lead electrodes, and forming an etching mask on said film by photolithography; then dry etching said film with plasma of a halogen-containing gas; and then dry etching said Ru layer with plasma of a gas containing at least oxygen.
Claim 9
Independent Claim 184 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer and a first gap film both formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: forming an Ru layer on one side of the magnetoresistive element that is to be closer to the pair of lead electrodes; patterning the magnetoresistive element, and patterning the permanent magnetic domain control layer at both end portions of the magnetoresistive element in the track width direction; then depositing a film that is to serve as the pair of lead electrodes, and forming an etching mask on said film by photolithography; then dry etching said film with plasma of a halogen-containing gas; and then dry etching said Ru layer with plasma of a gas containing at least oxygen.
Claim 10
Independent Claim 180 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: forming an RuO 2 layer on one side of the magnetoresistive element that is to be closer to the pair of lead electrodes; patterning the magnetoresistive element, and patterning the permanent magnetic domain control layer at both end portions of the magnetoresistive element in the track width direction; then depositing a film that is to serve as the pair of lead electrodes, and forming an etching mask on said film by photolithography; then dry etching said film with plasma of a halogen-containing gas; and then dry etching said RuO 2 layer with plasma of a gas containing at least oxygen.
Claim 11
Independent Claim 180 words
A method for manufacturing a thin film device including patterning a pair of lead electrodes on a magnetoresistive element portion and on a permanent magnetic domain control layer at both end portions of a magnetoresistive element, of the magnetoresistive element portion, in a direction of track width on a lower shield layer formed on a substrate, with the pair of lead electrodes to be electrically connected in series to the magnetoresistive element, wherein patterning the pair of lead electrodes comprises: forming an RuO 2 layer on one side of the magnetoresistive element that is to be closer to the pair of lead electrodes; patterning the magnetoresistive element, and patterning the permanent magnetic domain control layer at both end portions of the magnetoresistive element in the track width direction; then depositing a film that is to serve as the pair of lead electrodes, and forming an etching mask on said film by photolithography; then dry etching said film with plasma of a halogen-containing gas; and then dry etching said RuO 2 layer with plasma of a gas containing at least oxygen.

References Cited (Backward Citations)

JPH0536032A Cited
JPH0626009A Cited
US6225133B1 Cited
US5847423A Cited
US6071787A Cited
US6218258B1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2005-06-17 2005-12-17 2006-06-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2009-06-17 2009-12-17 2010-06-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2013-06-17 2013-12-17 2014-06-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag