Abstract

Abstract A method of forming oxide from nitride, in which the oxidation is enhanced by illuminating the nitride material with UV light. This method produces a rapid growth of oxide and allows for the monitoring of the oxide thickness in situ. The method comprises the steps of (i) placing the nitride material on an illuminating holder; (ii) dipping the nitride material and the illuminating holder in an electrolyte; and (iii) illuminating the nitride material with a light having an energy larger than the energy gap of the nitride material. The nitride material can be connected to a conductive electrode located in the electrolyte via a galvanometer to monitor a photo current generated by the oxidation of the nitride material so as to monitor the thickness of the oxide formed on the nitride material in situ. A metal coating can be coated on the nitride material to define the oxide forming region. The pH value of the electrolyte is in a range of approximately 3 to 10, and is preferably about 3.5.

Inventors

  • 👤 Lung-Han Peng
  • 👤 Yi-Chien Hsu
  • 👤 Chin-Yuan Chen
  • 👤 Jin-Kuo Ho
  • 👤 Chao-Nien Huang

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 18:34
CPC Classifications
C; C01; C01G; C01G1/00; C01G1/02; C01B; C01B13/00; C01B13/14; C01B13/32; C01B13/322; C01B13/324; C01P; C01P2002/00; C01P2002/70; C01P2002/72

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 66 words
A method of oxidizing a nitride material at room temperature comprising the steps of: (i) placing the nitride material on an illuminating holder; (ii) dipping the nitride material and the illuminating holder in an electrolyte having a pH value approximately ranged from 3 to 10; and (iii) illuminating the nitride material with a light having an energy larger than the energy gap of the nitride material.
Claim 2
Independent Claim 66 words
A method of oxidizing a nitride material at room temperature comprising the steps of: (i) placing the nitride material on an illuminating holder; (ii) dipping the nitride material and the illuminating holder in an electrolyte having a pH value approximately ranged from 3 to 10; and (iii) illuminating the nitride material with a light having an energy larger than the energy gap of the nitride material.
Claim 3
Dependent Claim 36 words
A method of oxidizing a nitride material as claimed in claim 1 further comprising a step of coating a metal coating on the nitride material to define a region of forming oxide prior to step (i).
Claim 4
Dependent Claim 63 words
A method of oxidizing a nitride material as claimed in claim 1 further comprising a step of connecting the nitride material to a conductive electrode located in the electrolyte via a galvanometer after step (iii) to monitor a photo current generated by oxidation of the nitride material so as to monitor a thickness of the oxide formed on the nitride material in situ.
Claim 5
Dependent Claim 19 words
A method of oxidizing a nitride material as claimed in claim 1 wherein the nitride material is gallium nitride.
Claim 6
Dependent Claim 22 words
A method of oxidizing a nitride material as claimed in claim 1 wherein the light illuminating the nitride material is UV light.
Claim 7
Dependent Claim 43 words
A method of oxidizing a nitride material as claimed in claim 2 wherein the metal coating is dual-layer including an inner layer and an outer layer, in which a work function of the outer layer is larger than that of the inner layer.
Claim 8
Dependent Claim 34 words
A method of oxidizing a nitride material as claimed in claim 1 wherein the electrolyte is one of KOH, H 2 O 2 , H 2 SO 4 or H 3 PO 4 .
Claim 9
Dependent Claim 19 words
A method of oxidizing a nitride material as claimed in claim 1 wherein the pH value is around 3.5.
Claim 10
Dependent Claim 59 words
A method of oxidizing a nitride material as claimed in claim 5 wherein the light source is one of a 308-nm XeCl excimer laser, a 248-nm KrF excimer laser, a 193-nm ArF excimer laser, a 157-nm F 2 excimer laser, a N 2 molecular laser, He—Cd molecular laser, a quarter-wavelength YAG laser, a deuterium lamp or a xenon lamp.
Claim 11
Dependent Claim 36 words
A method of oxidizing a nitride material as claimed in claim 6 wherein the outer layer of the dual-layer metal coating is one of Re, Pt, Ru, Rh, Pd, Au, Ir, Ni or a composition thereof.
Claim 12
Dependent Claim 35 words
A method of oxidizing a nitride material as claimed in claim 6 wherein the inner layer of dual-layer metal coating is one of Ti, V, Cr, Zr, Mo, Hf, Ta, W or a composition thereof.

References Cited (Backward Citations)

US5787104A Cited
JPH08203862A Cited
US5895223A Cited
JPH11229199A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2004-02-20 2004-08-21 2005-02-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2008-02-20 2008-08-21 2009-02-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2012-02-20 2012-08-21 2013-02-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag