Method for fabricating silicon-on-insulator wafer
Assignee: SK Hynix Inc
•
Filing: 1998-12-30
•
Granted: 2000-10-24
•
Expires: 2018-12-30
Abstract
Abstract Disclosed is a method for fabricating a silicon-on-insulator wafer, particularly to a cost reductive method.
Inventors
- 👤 Sang Mun So
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 10:57
CPC Classifications
H; H10; H10P; H10P14/00; H10P14/60; H10P90/00; H10P90/19; H10P90/1904; H10P90/1906; H10P90/1914; H10P90/1916; H10P90/1922; H10W; H10W10/00; H10W10/10; H10W10/181; Y; Y10; Y10S; Y10S438/00; Y10S438/928; Y10S438/967; Y10S438/977
Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
308 words
A method for fabricating silicon-on-insulator wafer, comprising the steps of: providing a first, a second and a third silicon substrates being comprised of bulk silicon; forming a first oxide film on one side of the first silicon substrate; forming a first impurity layer within the second silicon substrate with a selected depth; forming an isolation film in one side of the second silicon substrate; forming a second oxide film having even surface on the second silicon substrate; bonding the second oxide film of the second silicon substrate and the first oxide film of the first silicon substrate; performing a first polishing, a wet-etching and a second polishing processes in sequence until the impurity layer is removed, in the other side of the second silicon substrate; forming a second impurity layer within the second silicon substrate adjoining the first isolation film; forming a second isolation film in the other side of the second silicon substrate; forming a third oxide film having even surface on the other side of the second silicon substrate; forming a fourth oxide film on the third silicon substrate; bonding a fourth oxide film of the third silicon substrate and the third oxide film of the second silicon substrate; dividing a first wafer and a second wafer by the second impurity layer as a boundary line, wherein the first wafer includes the first isolation film and a first silicon layer which is some portion of the second silicon substrate where the first isolation film is formed, and the second wafer includes the second isolation film and a second silicon layer which is some portion of the second silicon substrate where the second isolation film is formed; and polishing the first and the second silicon layers using the first and the second isolation films of the first wafer and the second wafer as a polishing stopper, respectively.
Claim 2
Independent Claim
308 words
A method for fabricating silicon-on-insulator wafer, comprising the steps of: providing a first, a second and a third silicon substrates being comprised of bulk silicon; forming a first oxide film on one side of the first silicon substrate; forming a first impurity layer within the second silicon substrate with a selected depth; forming an isolation film in one side of the second silicon substrate; forming a second oxide film having even surface on the second silicon substrate; bonding the second oxide film of the second silicon substrate and the first oxide film of the first silicon substrate; performing a first polishing, a wet-etching and a second polishing processes in sequence until the impurity layer is removed, in the other side of the second silicon substrate; forming a second impurity layer within the second silicon substrate adjoining the first isolation film; forming a second isolation film in the other side of the second silicon substrate; forming a third oxide film having even surface on the other side of the second silicon substrate; forming a fourth oxide film on the third silicon substrate; bonding a fourth oxide film of the third silicon substrate and the third oxide film of the second silicon substrate; dividing a first wafer and a second wafer by the second impurity layer as a boundary line, wherein the first wafer includes the first isolation film and a first silicon layer which is some portion of the second silicon substrate where the first isolation film is formed, and the second wafer includes the second isolation film and a second silicon layer which is some portion of the second silicon substrate where the second isolation film is formed; and polishing the first and the second silicon layers using the first and the second isolation films of the first wafer and the second wafer as a polishing stopper, respectively.
Claim 3
Dependent Claim
17 words
The method of claim 1, wherein the first and the fourth oxide films are thermal oxide films.
Claim 4
Dependent Claim
34 words
The method of claim 1, wherein any ones of BPSG film, SOG film, O 3 -TEOS oxide film and high density plasma oxide film, is deposited as the first and the fourth oxide films.
Claim 5
Dependent Claim
20 words
The method of claim 1, wherein the first and the fourth oxide films are formed with thickness of 500˜10,000 Å.
Claim 6
Dependent Claim
14 words
The method of claim 1, wherein the impurity layer is a boron ion-implanted layer.
Claim 7
Dependent Claim
32 words
The method of claim 5, wherein the impurity layer is formed by injecting boron ions with energy of 50˜200 KeV and dose of 1.0×10 15 /cm 2 ˜3.0×10 16 /cm 2 .
Claim 8
Dependent Claim
30 words
The method of claim 1, wherein the first and the second isolation films are formed with thickness of 500˜5,000 Å by a partial oxidation process or by means of trench.
Claim 9
Dependent Claim
32 words
The method of claim 1, wherein the second and the third oxide films are any ones of BPSG film, SOG film, O 3 -TEOS oxide film and high density plasma oxide film.
Claim 10
Dependent Claim
20 words
The method of claim 1, wherein the second and the third oxide films are formed with thickness of 1,000˜10,000 Å.
Claim 11
Dependent Claim
23 words
The method of claim 1, wherein the first silicon substrate and the second silicon substrate are cleaned before they are bonded each other.
Claim 12
Dependent Claim
49 words
The method of claim 10, wherein the cleaning process is performed with one of a solution that the volume ratio of NH 4 OH:H 2 O 2 :H 2 O is 1:4:20, or a solution that the volume ratio of H 2 SO 4 :H 2 O is 4:1.
Claim 13
Dependent Claim
28 words
The method of claim 1, wherein the first silicon substrate and the second silicon substrate are bonded under a vacuum condition of 7.5×10 -1 Torr 7.5×10 -4 Torr.
Claim 14
Dependent Claim
54 words
The method of claim 1, wherein the first substrate and the second silicon substrate are heat-treated at temperature of 800˜1,200° C. for 30˜120 minutes under the atmosphere of one of nitrogen N 2 or oxygen O 2 so that their bonding intensity increases, after bonding the first silicon substrate and the second silicon substrate.
Claim 15
Dependent Claim
32 words
The method of claim 1, wherein the second silicon substrate is wet-etched with an etching solution that the volume ratio of NH 4 OH:H 2 O 2 :H 2 O is 1˜2:0.01˜0.02:1˜5.
Claim 16
Dependent Claim
33 words
The method of claim 1, wherein the second impurity layer is formed by injecting hydrogen ions with energy of 10˜1,000 KeV and dose of 1.0×10 15 /cm 2 ˜1.0×10 17 /cm 2 .
Claim 17
Dependent Claim
23 words
The method of claim 1, wherein the second silicon substrate and the third silicon substrate are cleaned before they are bonded each other.
Claim 18
Dependent Claim
49 words
The method of claim 16, wherein the cleaning process is performed with one of a solution that the volume ratio of NH 4 OH:H 2 O 2 :H 2 O is 1:4:20, or a solution that the volume ratio of H 2 SO 4 :H 2 O is 4:1.
Claim 19
Dependent Claim
43 words
The method of claim 1, wherein the process for dividing the first wafer and the second wafer is performed by heat-treating at temperature of 800˜1,200° C. for 30˜120 minutes under the atmosphere of one of nitrogen N 2 or oxygen O 2 .
Claim 20
Dependent Claim
43 words
The method of claim 1, wherein the second silicon substrate is polished under the condition that the rotating velocity of chuck table is 10˜30 rpm, the pressure applied by spindle is 4˜8 psi, and the rotating velocity of the spindle is 20˜40 rpm.
Claim 21
Dependent Claim
40 words
The method of claim 1, wherein the second silicon substrate of the first and the second wafers are polished, and those wafers are heat-treated at temperature of 700˜1,200° C. for 30˜120 minutes under the atmosphere of hydrogen H 2 .
References Cited (Backward Citations)
US4601779A
Cited
US4826787A
Cited
US5523254A
Cited
JPH0749281A
Cited
US5449638A
Cited
JPH0964317A
Cited
JPH1079498A
Cited
US6010950A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 2003-10-24 | 2004-04-24 | 2004-10-24 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2007-10-24 | 2008-04-24 | 2008-10-24 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2011-10-24 | 2012-04-24 | 2012-10-24 | $7700.00 | Window Closed / Lapsed |