Thermoplastic resin composition

Assignee: Daikin Industries Ltd
•
Filing: 1998-11-05
•
Granted: 2000-04-25
•
Expires: 2018-11-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A thermoplastic resin composition comprising a blend obtainable by blending 0.1 to 99% by weight of (a) a fluorine-containing polymer having a number-average molecular weight of 2000 to 1000000 and having hydroxy group or epoxy group at least at one of end portions of a main chain and side chain of the polymer, and 1 to 99.9% by weight of (b) a heat resisting thermoplastic resin having a crystalline melting point or glass transition temperature of not less than 150 DEG C. The present invention can provide a composition comprising various heat resisting thermoplastic resins and a fluorine-containing polymer having a functional group which is capable of developing an affinity with said resins and forming a uniform dispersion.

Inventors

  • 👤 Tetsuo Shimizu
  • 👤 Yoshihisa Yamamoto
  • 👤 Seitaro Yamaguchi
  • 👤 Nobuhiko Tsuda
  • 👤 Noriyasu Yamane
  • 👤 Takafumi Yamato
  • 👤 Masahiro Kumegawa
  • 👤 Takayuki Araki

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 21:37
CPC Classifications
C; C08; C08L; C08L77/00; C08L77/06; C08G; C08G59/00; C08G59/18; C08G59/20; C08G59/22; C08G59/30; C08G59/32; C08G59/3254; C08G61/00; C08G61/12; C08L101/00; C08L27/00; C08L27/02; C08L27/12; C08L27/16; C08L67/00; C08L67/02; C08L67/03; C08L69/00; C08L77/02; C08L81/00; C08L81/04; C08L2201/00

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 495 words
A thermoplastic resin composition which comprises a blend obtained by blending 0.1 to 99% by weight of (a) a fluorine-containing polymer having a functional group and a number-average molecular weight of 2000 to 1000000 and 1 to 99.9% by weight of (b) a heat resisting polyarylene sulfide resin having a crystalline melting point or glass transition temperature of not less than 150° C.; said fluorine-containing polymer (a) having a functional group that is at least one selected from fluorine-containing polymers having functional groups, in which a concentration of the functional groups at a main chain end portion and side chain portion is 2 to 2000 μmol/g per the total weight of the fluorine-containing polymer, and represented by the formula (I): ##STR6## wherein X is a structural unit of the formula --(CH 2 CX 1 X 2 )-- (wherein X 1 and X 2 are the same or different, and each is hydrogen atom, fluorine atom, --(CH 2 ) p --(O) q --R--B 1 (R is a dihydric hydrocarbon group having carbon atoms of 1 to 20 or dihydric fluorine-substituted organic group having carbon atoms of 1 to 20, B 1 is hydrogen atom, fluorine atom, hydroxy group or epoxy group, p is 0 or 1 and q is 0 or 1), --OCO--R--B 1 (R and B 1 are the same as above) or --COO--R--B 1 (R and B 1 are the same as above)); Y is a structural unit of the formula --(CF 2 CY 1 Y 2 )--(wherein Y 1 and Y 2 are the same or different, and each is hydrogen atom, fluorine atom, chlorine atom, --(CF 2 ) r --(O) s --(R f ) t --(CH 2 ) u --B 2 (R f is a dihydric fluorine-substituted organic group having carbon atoms of 1 to 14, B 2 is hydrogen atom, halogen atom, hydroxy group, epoxy group or glycidyloxy group, r is 0 or 1, s is 0 or 1, t is 0 or 1, and u is an integer of 1 to 3) or S(CF 2 ) v --B 3 (B 3 is hydrogen atom, fluorine atom or chlorine atom, and v is an integer of 1 to 10)); both A 1 and A 2 are end portions of a main chain; provided that each of X and Y may comprise two or more structural units; Y may not be present when X has the structural unit derived from CH 2 ═CHF, CH 2 ═CF 2 or fluoroalkyl-α-substituted acrylate (substituent is hydrogen atom, fluorine atom or methyl); X may not be present when Y has the structural unit derived from CH 2 ═CF 2 or CH 2 ═CHCl; at least one of A 1 and A 2 contains hydroxy group, epoxy group or glycidyl group when both of X and Y do not contain hydroxy group, epoxy group or glycidyl group; said resin composition contains only the fluorine-containing polymer represented by the formula (I) as the fluorine-containing polymer having functional group.
Claim 2
Dependent Claim 495 words
A thermoplastic resin composition which comprises a blend obtained by blending 0.1 to 99% by weight of (a) a fluorine-containing polymer having a functional group and a number-average molecular weight of 2000 to 1000000 and 1 to 99.9% by weight of (b) a heat resisting polyarylene sulfide resin having a crystalline melting point or glass transition temperature of not less than 150° C.; said fluorine-containing polymer (a) having a functional group that is at least one selected from fluorine-containing polymers having functional groups, in which a concentration of the functional groups at a main chain end portion and side chain portion is 2 to 2000 μmol/g per the total weight of the fluorine-containing polymer, and represented by the formula (I): ##STR6## wherein X is a structural unit of the formula --(CH 2 CX 1 X 2 )-- (wherein X 1 and X 2 are the same or different, and each is hydrogen atom, fluorine atom, --(CH 2 ) p --(O) q --R--B 1 (R is a dihydric hydrocarbon group having carbon atoms of 1 to 20 or dihydric fluorine-substituted organic group having carbon atoms of 1 to 20, B 1 is hydrogen atom, fluorine atom, hydroxy group or epoxy group, p is 0 or 1 and q is 0 or 1), --OCO--R--B 1 (R and B 1 are the same as above) or --COO--R--B 1 (R and B 1 are the same as above)); Y is a structural unit of the formula --(CF 2 CY 1 Y 2 )--(wherein Y 1 and Y 2 are the same or different, and each is hydrogen atom, fluorine atom, chlorine atom, --(CF 2 ) r --(O) s --(R f ) t --(CH 2 ) u --B 2 (R f is a dihydric fluorine-substituted organic group having carbon atoms of 1 to 14, B 2 is hydrogen atom, halogen atom, hydroxy group, epoxy group or glycidyloxy group, r is 0 or 1, s is 0 or 1, t is 0 or 1, and u is an integer of 1 to 3) or S(CF 2 ) v --B 3 (B 3 is hydrogen atom, fluorine atom or chlorine atom, and v is an integer of 1 to 10)); both A 1 and A 2 are end portions of a main chain; provided that each of X and Y may comprise two or more structural units; Y may not be present when X has the structural unit derived from CH 2 ═CHF, CH 2 ═CF 2 or fluoroalkyl-α-substituted acrylate (substituent is hydrogen atom, fluorine atom or methyl); X may not be present when Y has the structural unit derived from CH 2 ═CF 2 or CH 2 ═CHCl; at least one of A 1 and A 2 contains hydroxy group, epoxy group or glycidyl group when both of X and Y do not contain hydroxy group, epoxy group or glycidyl group; said resin composition contains only the fluorine-containing polymer represented by the formula (I) as the fluorine-containing polymer having functional group.
Claim 3
Dependent Claim 41 words
The composition of claim 1, wherein the fluorine-containing polymer (a) having the functional group is an elastomer having a number-average molecular weight of 2000 to 200000, and a ratio of (a)/(b) is 0.1 to 40% by weight/99.9 to 60% by weight.

References Cited (Backward Citations)

JPS6257448A Cited
JPS6381159A Cited
JPS63264672A Cited
JPS63172749A Cited
EP0275186A2 Cited
JPH03215548A Cited
JPH03263464A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2003-04-25 2003-10-25 2004-04-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2007-04-25 2007-10-25 2008-04-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2011-04-25 2011-10-25 2012-04-25 $7700.00 Window Closed / Lapsed