Claim 1
Independent Claim
87 words
A method for making a medical device having immobilized heparin on a blood-contacting surface comprising: (a) providing immobilized free amine groups on a blood-contacting surface; (b) admixing heparin with sufficient periodate to react with not more than two sugar units per heparin molecule in a buffer solution having a pH in the range of about 4.5-8, and allowing the admixture to react for at least 3 hours while protected from light; and (c) applying the reacted admixture to the immobilized amine groups without stopping the periodate-heparin reaction.
Claim 2
Independent Claim
87 words
A method for making a medical device having immobilized heparin on a blood-contacting surface comprising: (a) providing immobilized free amine groups on a blood-contacting surface; (b) admixing heparin with sufficient periodate to react with not more than two sugar units per heparin molecule in a buffer solution having a pH in the range of about 4.5-8, and allowing the admixture to react for at least 3 hours while protected from light; and (c) applying the reacted admixture to the immobilized amine groups without stopping the periodate-heparin reaction.
Claim 3
Dependent Claim
19 words
The method of claim 1 wherein the mobilized amine groups are provided by an immobilized coating of a polyalkyleneimine.
Claim 4
Dependent Claim
24 words
The method of claim 1 wherein the reacted admixture is stored for 2 to 14 days prior to application to the immobilized amine groups.
Claim 5
Dependent Claim
11 words
The method of claim 1 wherein the periodate is sodium periodate.
Claim 6
Dependent Claim
18 words
The method of claim 4 wherein the weight ratio of heparin to periodate is about 30:1 or less.
Claim 7
Dependent Claim
24 words
The method of claim 1 further comprising mixing the reacted admixture with a mild reducing agent prior to applying to the immobilized amine groups.
Claim 8
Dependent Claim
12 words
The method of claim 6 wherein the reducing agent is sodium cyanoborohydride.
Claim 9
Dependent Claim
20 words
The method of claim 7 wherein the pH of the reducing agent and reacted admixture is adjusted to about 4.6.
Claim 10
Independent Claim
107 words
A method for applying a heparin coating to a surface comprising: (a) attaching a polyalkyleneimine to the surface; (b) preparing a heparin solution by the steps comprising: (1) admixing heparin with a periodate in a buffered aqueous solution at a weight ratio of heparin to periodate of about 30:1; (2) reacting the admixture for at least 3 hours while protected from light; and (3) adding a cyanoborohydride to the reacted admixture; (c) applying the heparin solution to the attached polyalkyleneimine on the surface; (d) incubating the surface and applied heparin such that the heparin and the polyalkyleneimine are bonded; and (e) rinsing the incubated surface with water.
Claim 11
Independent Claim
107 words
A method for applying a heparin coating to a surface comprising: (a) attaching a polyalkyleneimine to the surface; (b) preparing a heparin solution by the steps comprising: (1) admixing heparin with a periodate in a buffered aqueous solution at a weight ratio of heparin to periodate of about 30:1; (2) reacting the admixture for at least 3 hours while protected from light; and (3) adding a cyanoborohydride to the reacted admixture; (c) applying the heparin solution to the attached polyalkyleneimine on the surface; (d) incubating the surface and applied heparin such that the heparin and the polyalkyleneimine are bonded; and (e) rinsing the incubated surface with water.
Claim 12
Dependent Claim
28 words
The method of claim 9 wherein the polyalkyleneimine is attached to the surface by applying a silane to the surface and covalently bonding the polyalkyleneimine to the silane.