Claims Analysis
Total Claims: 18
Claim 1
Independent Claim
67 words
A method for extracting a precious metal from an ore comprising the steps of producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas; reducing the fugacity of hydrogen gas in said leaching solution by means of an oxyanion-reducing bacterium; exposing said ore to said leaching solution; and recovering said precious metal from said leaching solution.
Claim 2
Independent Claim
67 words
A method for extracting a precious metal from an ore comprising the steps of producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas; reducing the fugacity of hydrogen gas in said leaching solution by means of an oxyanion-reducing bacterium; exposing said ore to said leaching solution; and recovering said precious metal from said leaching solution.
Claim 3
Dependent Claim
18 words
The method of claim 1 wherein the producing step is carried out by means of a sulfate-reducing bacterium.
Claim 4
Dependent Claim
27 words
The method of claim 1 wherein the oxyanion-reducing bacterium is selected from the group consisting of: an acetogen, a methanogen, a sulfate-reducing bacterium, and a nitrate-reducing bacterium.
Claim 5
Dependent Claim
36 words
The method of claim 1 wherein the oxyanion-reducing bacterium is selected from the group consisting of: Desulfobacterium catecholicum (DSM 3882), Desulfovibrio simplex (DSM 4141), Desulfovibrio salexigens (DSM 2638), and Desulfomaculum kuznetsovii (DSM 6115 or VKM B-1805).
Claim 6
Dependent Claim
71 words
A process for precious metal leaching comprising the steps of biologically reducing a dissolved sulfate under anaerobic conditions to produce a bisulfide lixiviant having an approximately neutral pH and a hydrogen gas fugacity of less than 0.001 atmospheres, leaching a first portion of an ore comprising at least one precious metal by exposing said ore to said bisulfide lixiviant, and recovering said at least one precious metal from said bisulfide lixiviant.
Claim 7
Dependent Claim
71 words
A process for precious metal leaching comprising the steps of biologically reducing a dissolved sulfate under anaerobic conditions to produce a bisulfide lixiviant having an approximately neutral pH and a hydrogen gas fugacity of less than 0.001 atmospheres, leaching a first portion of an ore comprising at least one precious metal by exposing said ore to said bisulfide lixiviant, and recovering said at least one precious metal from said bisulfide lixiviant.
Claim 8
Dependent Claim
20 words
The process of claim 5 further comprising biologically oxidizing said first portion of an ore prior to said leaching step.
Claim 9
Dependent Claim
20 words
The process of claim 5 wherein said dissolved sulfate is produced by biologically oxidizing a second portion of an ore.
Claim 10
Dependent Claim
34 words
The process of claim 5 wherein said biologically reducing step and said leaching step are accomplished in an essentially completely mixed reactor and at a pH in the range of 6 to 8 units.
Claim 11
Dependent Claim
28 words
The process of claim 7 wherein said biologically oxidizing step occurs in a first heap of ore and said leaching step occurs in a second heap of ore.
Claim 12
Dependent Claim
28 words
The process of claim 9 wherein said recovering step is comprised of exposing pregnant bisulfide solution to activated carbon and eluting said precious metals from said activated carbon.
Claim 13
Independent Claim
66 words
An apparatus for extracting a precious metal from an ore comprising: means for producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas and for reducing the fugacity of hydrogen gas in said leaching solution; means for exposing said ore to said leaching solution; and means for recovering said precious metal from said leaching solution.
Claim 14
Independent Claim
66 words
An apparatus for extracting a precious metal from an ore comprising: means for producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas and for reducing the fugacity of hydrogen gas in said leaching solution; means for exposing said ore to said leaching solution; and means for recovering said precious metal from said leaching solution.
Claim 15
Dependent Claim
180 words
A process of making a product, said product comprising a precious metal that can form a complex comprising bisulfide, said complex having an aqueous solubility, said process comprising the steps of: introducing an ore of said precious metal into an anaerobic reactor environment, said reactor environment having an activity of dissolved hydrogen sulfide gas, an activity of dissolved bisulfide ions, and a fugacity of hydrogen gas; increasing said activity of dissolved hydrogen sulfide gas and said activity of dissolved bisulfide ions and reducing said fugacity of hydrogen gas, whereby the solubility of the precious metal-bisulfide complex is increased; removing the precious metal-bisulfide complex from said reactor environment; separating said precious metal from said metal-bisulfide complex; and forming said product from said precious metal; wherein said increasing step and said reducing step are accomplished by at least one step selected from the group consisting of contacting said reactor environment with a culture of an oxyanion-reducing bacterium, and contacting said reactor environment with a stream of gas comprising hydrogen sulfide gas and a fugacity of hydrogen gas of less that 0.001 atmospheres.
Claim 16
Dependent Claim
180 words
A process of making a product, said product comprising a precious metal that can form a complex comprising bisulfide, said complex having an aqueous solubility, said process comprising the steps of: introducing an ore of said precious metal into an anaerobic reactor environment, said reactor environment having an activity of dissolved hydrogen sulfide gas, an activity of dissolved bisulfide ions, and a fugacity of hydrogen gas; increasing said activity of dissolved hydrogen sulfide gas and said activity of dissolved bisulfide ions and reducing said fugacity of hydrogen gas, whereby the solubility of the precious metal-bisulfide complex is increased; removing the precious metal-bisulfide complex from said reactor environment; separating said precious metal from said metal-bisulfide complex; and forming said product from said precious metal; wherein said increasing step and said reducing step are accomplished by at least one step selected from the group consisting of contacting said reactor environment with a culture of an oxyanion-reducing bacterium, and contacting said reactor environment with a stream of gas comprising hydrogen sulfide gas and a fugacity of hydrogen gas of less that 0.001 atmospheres.
Claim 17
Dependent Claim
20 words
The process of claim 12 wherein said precious metal is selected from the group consisting of gold, silver, and platinum.
Claim 18
Dependent Claim
23 words
The process of claim 12 wherein said increasing step is accomplished by contacting said reactor environment with a culture of a sulfate-reducing bacterium.