Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
239 words
A process for recovery of gold from a gold-bearing arsenopyritic material selected from a gold-bearing arsenopyritic ore and a gold-bearing arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation stage, which process comprises: (i) supplying a pyritic material, sulphuric acid, nutrients, and an oxygen-containing gas to a generator vessel containing a colony of Thiobacillus ferro-oxidans, said pyritic material having a content of arsenic producing an arsenic content in the liquor in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, thereby to generate an aqueous acidic ferric sulphate solution containing bacterially generated ferric ions; (ii) admixing resulting aqueous acidic ferric sulphate solution with an arsenic-containing aqueous recycle stream containing ferrous ions; (iii) leaching the gold-bearing arsenopyritic material in the form of a pulp in the leach stage by admixture with the feric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids in the solids separation stage from the arsenic-containing aqueous leach liquor containing ferrous ions; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the arsenic-containing leach liquor of step (iv) in excess of the volume required to form the arsenic-containing aqueous stream of step (ii); and (vii) recycling the remainder of the arsenic-containing aqueous leach liquor of step (iv) as the arsenic-containing aqueous recycle stream of step (ii).
Claim 2
Dependent Claim
239 words
A process for recovery of gold from a gold-bearing arsenopyritic material selected from a gold-bearing arsenopyritic ore and a gold-bearing arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation stage, which process comprises: (i) supplying a pyritic material, sulphuric acid, nutrients, and an oxygen-containing gas to a generator vessel containing a colony of Thiobacillus ferro-oxidans, said pyritic material having a content of arsenic producing an arsenic content in the liquor in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, thereby to generate an aqueous acidic ferric sulphate solution containing bacterially generated ferric ions; (ii) admixing resulting aqueous acidic ferric sulphate solution with an arsenic-containing aqueous recycle stream containing ferrous ions; (iii) leaching the gold-bearing arsenopyritic material in the form of a pulp in the leach stage by admixture with the feric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids in the solids separation stage from the arsenic-containing aqueous leach liquor containing ferrous ions; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the arsenic-containing leach liquor of step (iv) in excess of the volume required to form the arsenic-containing aqueous stream of step (ii); and (vii) recycling the remainder of the arsenic-containing aqueous leach liquor of step (iv) as the arsenic-containing aqueous recycle stream of step (ii).
Claim 3
Dependent Claim
25 words
A process according to claim 1, in which the pH in the generator is controlled in the range of from about 8 to about 3.0.
Claim 4
Dependent Claim
13 words
A process according to calim 1, in which the oxygen-containing gas is air.
Claim 5
Dependent Claim
13 words
A process according to calim 1, in which the oxygen-containing gas is air.
Claim 6
Dependent Claim
49 words
A process according to claim 1, in which the leach stage is operated using a pulp of the gold-bearing material containing from about 5% to about 15% w/w solids and the residence time of the solids in the leach stage is from about 24 hours to about 96 hours.
Claim 7
Dependent Claim
36 words
A process according to claim 4, in which the pulp has a solids content of about 10% w/w solids and in which the residence time of the solids in the leach stage is about 72 hours.
Claim 8
Dependent Claim
289 words
A process for the recovery of gold from a gold-bearing arsenic-containing material selected from an arsenopyritic ore and an arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation state, which process comprises: (i) supplying to a generator vessel which is external to the path of the liquor circulating between the leach stage and solids separation stage and which contains a colony of Thiobacillus ferro-oxidans, a pyritic material that has a content of arsenic producing an arsenic content in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, as well as sulphuric acid, nutrients, and an oxygen-containing gas thereby to generate an auqeous acidic ferric sulphate solution containing bacterially generated ferric ions and having a pH in the range of from about 0.8 to about 3.0; (ii) admixing resulting aqueous ferric sulphate solution with an aqueous recycle stream containing ferric ions and dissolved arsenic values; (iii) leaching the gold-bearing asenopyritic material in a leach stage in the form of a pulp containing from about 5% to about 15% w/w solids by admixture with the mixed ferric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids from an aqueous leach liquor containing ferrous ions and dissolved arsenic values; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the aqueous leach liquor of step (iv) in excess of the volume required to form the aqueous recycle stream of step (ii); and (vii) recycling the remainder of the aqueous leach liquor of step (iv) along a path which does not include the generator vessel to form the aqueous recycle stream of step (ii).
Claim 9
Dependent Claim
289 words
A process for the recovery of gold from a gold-bearing arsenic-containing material selected from an arsenopyritic ore and an arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation state, which process comprises: (i) supplying to a generator vessel which is external to the path of the liquor circulating between the leach stage and solids separation stage and which contains a colony of Thiobacillus ferro-oxidans, a pyritic material that has a content of arsenic producing an arsenic content in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, as well as sulphuric acid, nutrients, and an oxygen-containing gas thereby to generate an auqeous acidic ferric sulphate solution containing bacterially generated ferric ions and having a pH in the range of from about 0.8 to about 3.0; (ii) admixing resulting aqueous ferric sulphate solution with an aqueous recycle stream containing ferric ions and dissolved arsenic values; (iii) leaching the gold-bearing asenopyritic material in a leach stage in the form of a pulp containing from about 5% to about 15% w/w solids by admixture with the mixed ferric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids from an aqueous leach liquor containing ferrous ions and dissolved arsenic values; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the aqueous leach liquor of step (iv) in excess of the volume required to form the aqueous recycle stream of step (ii); and (vii) recycling the remainder of the aqueous leach liquor of step (iv) along a path which does not include the generator vessel to form the aqueous recycle stream of step (ii).
Claim 10
Dependent Claim
25 words
A process according to claim 6, in which the pH in the generator is controlled in the range of from about 0.8 to about 3.0.
Claim 11
Dependent Claim
49 words
A process according to claim 6, in which the leach stage is operated using a pulp of the gold-bearing material containing from about 5% to about 15% w/w solids and the residence time of the solids in the leach stage is from about 24 hours o about 96 hours.
Claim 12
Dependent Claim
36 words
A process according to claim 8, in which the pulp has a solids content of about 10% w/w solids and in which the residence time of the solids in the leach stage is about 72 hours.