Abstract

Abstract A process is described for leaching ores or concentrates containing one or more metallic sulphides .with a circulating liquor so as to solubilize desired metal values therefrom, if said metal values are capable of dissolution in an acidic ferric sulphate solution (e.g. copper), or so as to render the desired metal values (e.g. gold) more accessible to subsequent processing, in each case by effecting metallic sulphide dissolution from the ore or concentrate. In this process the ore or concentrate, for example a gold ore, is leached in a leach stage using an acidic leaching medium formed by mixing recycled liquor with a make-up stream containing bacterially generated ferric ions and sulphate ions which is produced in a generator (a) which is external to the circulation path of the liquor between the leach stage and a separation stage, (b) which contains a colony of suitable bacteria, such as Thiobacillus ferro-oxidans, and (c) which is fed, as necessary, with a pyritic material, water, nutrients, sulphuric acid and an oxygen-containing gas (e.g. air). As the presence of live bacteria in the leach state is not essential to operation, the process can be used for leaching arsenopyritic and similar ores and with a recycle stream containing high levels of arsenic or other impurity which is potentially deleterious to bacterial viability. A mixture of leached solids and liquor is passed from the leach stage to the separation stage, which is included in the path of the circulating liquor where leached solids are separated from a ferrous sulphate-containing liquor. The leached solids can be treated for recovery of metal values (e.g. gold), if the metal values are not leached in the leach stage. Alternatively, if the desired metal values (e.g. copper) appear in the liquor, the leached solids are discarded and the liquor is subjected to metal recovery, e.g. cementation, before recycle.

Inventors

  • 👤 Frederick D. Pooley
  • 👤 Martin T. Errington

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 13:38
CPC Classifications
C; C22; C22B; C22B3/00; C22B3/18; C22B11/00; C22B11/04; C22B15/00; C22B15/0063; C22B15/0065; C22B15/0067; C22B15/0071; C22B3/04; C22B3/06; C22B3/08; Y; Y02; Y02P; Y02P10/00; Y02P10/20; Y10; Y10S; Y10S423/00; Y10S423/09; Y10S423/17

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 239 words
A process for recovery of gold from a gold-bearing arsenopyritic material selected from a gold-bearing arsenopyritic ore and a gold-bearing arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation stage, which process comprises: (i) supplying a pyritic material, sulphuric acid, nutrients, and an oxygen-containing gas to a generator vessel containing a colony of Thiobacillus ferro-oxidans, said pyritic material having a content of arsenic producing an arsenic content in the liquor in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, thereby to generate an aqueous acidic ferric sulphate solution containing bacterially generated ferric ions; (ii) admixing resulting aqueous acidic ferric sulphate solution with an arsenic-containing aqueous recycle stream containing ferrous ions; (iii) leaching the gold-bearing arsenopyritic material in the form of a pulp in the leach stage by admixture with the feric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids in the solids separation stage from the arsenic-containing aqueous leach liquor containing ferrous ions; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the arsenic-containing leach liquor of step (iv) in excess of the volume required to form the arsenic-containing aqueous stream of step (ii); and (vii) recycling the remainder of the arsenic-containing aqueous leach liquor of step (iv) as the arsenic-containing aqueous recycle stream of step (ii).
Claim 2
Dependent Claim 239 words
A process for recovery of gold from a gold-bearing arsenopyritic material selected from a gold-bearing arsenopyritic ore and a gold-bearing arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation stage, which process comprises: (i) supplying a pyritic material, sulphuric acid, nutrients, and an oxygen-containing gas to a generator vessel containing a colony of Thiobacillus ferro-oxidans, said pyritic material having a content of arsenic producing an arsenic content in the liquor in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, thereby to generate an aqueous acidic ferric sulphate solution containing bacterially generated ferric ions; (ii) admixing resulting aqueous acidic ferric sulphate solution with an arsenic-containing aqueous recycle stream containing ferrous ions; (iii) leaching the gold-bearing arsenopyritic material in the form of a pulp in the leach stage by admixture with the feric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids in the solids separation stage from the arsenic-containing aqueous leach liquor containing ferrous ions; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the arsenic-containing leach liquor of step (iv) in excess of the volume required to form the arsenic-containing aqueous stream of step (ii); and (vii) recycling the remainder of the arsenic-containing aqueous leach liquor of step (iv) as the arsenic-containing aqueous recycle stream of step (ii).
Claim 3
Dependent Claim 25 words
A process according to claim 1, in which the pH in the generator is controlled in the range of from about 8 to about 3.0.
Claim 4
Dependent Claim 13 words
A process according to calim 1, in which the oxygen-containing gas is air.
Claim 5
Dependent Claim 13 words
A process according to calim 1, in which the oxygen-containing gas is air.
Claim 6
Dependent Claim 49 words
A process according to claim 1, in which the leach stage is operated using a pulp of the gold-bearing material containing from about 5% to about 15% w/w solids and the residence time of the solids in the leach stage is from about 24 hours to about 96 hours.
Claim 7
Dependent Claim 36 words
A process according to claim 4, in which the pulp has a solids content of about 10% w/w solids and in which the residence time of the solids in the leach stage is about 72 hours.
Claim 8
Dependent Claim 289 words
A process for the recovery of gold from a gold-bearing arsenic-containing material selected from an arsenopyritic ore and an arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation state, which process comprises: (i) supplying to a generator vessel which is external to the path of the liquor circulating between the leach stage and solids separation stage and which contains a colony of Thiobacillus ferro-oxidans, a pyritic material that has a content of arsenic producing an arsenic content in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, as well as sulphuric acid, nutrients, and an oxygen-containing gas thereby to generate an auqeous acidic ferric sulphate solution containing bacterially generated ferric ions and having a pH in the range of from about 0.8 to about 3.0; (ii) admixing resulting aqueous ferric sulphate solution with an aqueous recycle stream containing ferric ions and dissolved arsenic values; (iii) leaching the gold-bearing asenopyritic material in a leach stage in the form of a pulp containing from about 5% to about 15% w/w solids by admixture with the mixed ferric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids from an aqueous leach liquor containing ferrous ions and dissolved arsenic values; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the aqueous leach liquor of step (iv) in excess of the volume required to form the aqueous recycle stream of step (ii); and (vii) recycling the remainder of the aqueous leach liquor of step (iv) along a path which does not include the generator vessel to form the aqueous recycle stream of step (ii).
Claim 9
Dependent Claim 289 words
A process for the recovery of gold from a gold-bearing arsenic-containing material selected from an arsenopyritic ore and an arsenopyritic concentrate in which an aqueous liquor is circulated between a leach stage and a solids separation state, which process comprises: (i) supplying to a generator vessel which is external to the path of the liquor circulating between the leach stage and solids separation stage and which contains a colony of Thiobacillus ferro-oxidans, a pyritic material that has a content of arsenic producing an arsenic content in the generator vessel which is less than the arsenic content of a recycle stream leaching the gold-bearing arsenopyritic material, as well as sulphuric acid, nutrients, and an oxygen-containing gas thereby to generate an auqeous acidic ferric sulphate solution containing bacterially generated ferric ions and having a pH in the range of from about 0.8 to about 3.0; (ii) admixing resulting aqueous ferric sulphate solution with an aqueous recycle stream containing ferric ions and dissolved arsenic values; (iii) leaching the gold-bearing asenopyritic material in a leach stage in the form of a pulp containing from about 5% to about 15% w/w solids by admixture with the mixed ferric sulphate and arsenic-containing aqueous liquor from step (ii); (iv) separating resultant leached solids from an aqueous leach liquor containing ferrous ions and dissolved arsenic values; (v) subjecting recovered solids of step (iv) to a cyanide leach step; (vi) discarding a part of the aqueous leach liquor of step (iv) in excess of the volume required to form the aqueous recycle stream of step (ii); and (vii) recycling the remainder of the aqueous leach liquor of step (iv) along a path which does not include the generator vessel to form the aqueous recycle stream of step (ii).
Claim 10
Dependent Claim 25 words
A process according to claim 6, in which the pH in the generator is controlled in the range of from about 0.8 to about 3.0.
Claim 11
Dependent Claim 49 words
A process according to claim 6, in which the leach stage is operated using a pulp of the gold-bearing material containing from about 5% to about 15% w/w solids and the residence time of the solids in the leach stage is from about 24 hours o about 96 hours.
Claim 12
Dependent Claim 36 words
A process according to claim 8, in which the pulp has a solids content of about 10% w/w solids and in which the residence time of the solids in the leach stage is about 72 hours.

References Cited (Backward Citations)

CA757602A Cited
CA869470A Cited
US2829964A Cited
US3347661A Cited
US3856913A Cited
CA1018774A Cited
GB1409486A Cited
GB2097369A Cited
US4497778A Cited
US4571387A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-04-17 1992-10-17 1993-04-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-04-17 1996-10-17 1997-04-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-04-17 2000-10-17 2001-04-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag