← Back to Patent Explorer
US5672194A Expired / Lapsed US ⏱️ 0.0 years remaining

Method and apparatus for extracting precious metals from their ores and the product thereof

Assignee: Yellowstone Environmental Science Inc
•
Filing: 1995-05-08
•
Granted: 1997-09-30
•
Expires: 2015-05-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method and apparatus for extraction of precious metals from their ores and the product thereof. Oxidized ore comprising a precious metal is exposed to a leaching solution (lixiviant) comprising a relatively high concentration (fugacity) of dissolved hydrogen sulfide gas, a relatively high concentration (activity) of bisulfide ions, and a relatively low concentration (fugacity) of dissolved hydrogen gas. The hydrogen sulfide gas and bisulfide ions are preferably added to the solution by sulfate-reducing bacteria growing in a medium comprising dissolved sulfate ions and dissolved nitrate ions, but abiotic sources may also be used. Examples of such bacteria include mesophilic, fresh-water species such as Desulfobacterium catecholicum DSM 3882 and Desulfovibrio simplex DSM 4141; mesophilic, salt-water species such as Desulfovibrio salexigens DSM 2638; and thermophilic, fresh-water species such as Desulfomaculum kuznetsovii VKM B-1805. The complexed precious metal is recovered from the lixiviant.

Inventors

  • 👤 Robert M. Hunter
  • 👤 Frank M. Stewart
  • 👤 Tamara Darsow

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 20:58
CPC Classifications
C; C22; C22B; C22B3/00; C22B3/18; C22B11/00; C22B11/04; Y; Y02; Y02P; Y02P10/00; Y02P10/20; Y10; Y10S; Y10S423/00; Y10S423/09; Y10S423/17

Claims Analysis

Total Claims: 18
Claim 1
Independent Claim 67 words
A method for extracting a precious metal from an ore comprising the steps of producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas; reducing the fugacity of hydrogen gas in said leaching solution by means of an oxyanion-reducing bacterium; exposing said ore to said leaching solution; and recovering said precious metal from said leaching solution.
Claim 2
Independent Claim 67 words
A method for extracting a precious metal from an ore comprising the steps of producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas; reducing the fugacity of hydrogen gas in said leaching solution by means of an oxyanion-reducing bacterium; exposing said ore to said leaching solution; and recovering said precious metal from said leaching solution.
Claim 3
Dependent Claim 18 words
The method of claim 1 wherein the producing step is carried out by means of a sulfate-reducing bacterium.
Claim 4
Dependent Claim 27 words
The method of claim 1 wherein the oxyanion-reducing bacterium is selected from the group consisting of: an acetogen, a methanogen, a sulfate-reducing bacterium, and a nitrate-reducing bacterium.
Claim 5
Dependent Claim 36 words
The method of claim 1 wherein the oxyanion-reducing bacterium is selected from the group consisting of: Desulfobacterium catecholicum (DSM 3882), Desulfovibrio simplex (DSM 4141), Desulfovibrio salexigens (DSM 2638), and Desulfomaculum kuznetsovii (DSM 6115 or VKM B-1805).
Claim 6
Dependent Claim 71 words
A process for precious metal leaching comprising the steps of biologically reducing a dissolved sulfate under anaerobic conditions to produce a bisulfide lixiviant having an approximately neutral pH and a hydrogen gas fugacity of less than 0.001 atmospheres, leaching a first portion of an ore comprising at least one precious metal by exposing said ore to said bisulfide lixiviant, and recovering said at least one precious metal from said bisulfide lixiviant.
Claim 7
Dependent Claim 71 words
A process for precious metal leaching comprising the steps of biologically reducing a dissolved sulfate under anaerobic conditions to produce a bisulfide lixiviant having an approximately neutral pH and a hydrogen gas fugacity of less than 0.001 atmospheres, leaching a first portion of an ore comprising at least one precious metal by exposing said ore to said bisulfide lixiviant, and recovering said at least one precious metal from said bisulfide lixiviant.
Claim 8
Dependent Claim 20 words
The process of claim 5 further comprising biologically oxidizing said first portion of an ore prior to said leaching step.
Claim 9
Dependent Claim 20 words
The process of claim 5 wherein said dissolved sulfate is produced by biologically oxidizing a second portion of an ore.
Claim 10
Dependent Claim 34 words
The process of claim 5 wherein said biologically reducing step and said leaching step are accomplished in an essentially completely mixed reactor and at a pH in the range of 6 to 8 units.
Claim 11
Dependent Claim 28 words
The process of claim 7 wherein said biologically oxidizing step occurs in a first heap of ore and said leaching step occurs in a second heap of ore.
Claim 12
Dependent Claim 28 words
The process of claim 9 wherein said recovering step is comprised of exposing pregnant bisulfide solution to activated carbon and eluting said precious metals from said activated carbon.
Claim 13
Independent Claim 66 words
An apparatus for extracting a precious metal from an ore comprising: means for producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas and for reducing the fugacity of hydrogen gas in said leaching solution; means for exposing said ore to said leaching solution; and means for recovering said precious metal from said leaching solution.
Claim 14
Independent Claim 66 words
An apparatus for extracting a precious metal from an ore comprising: means for producing a leaching solution, said solution comprising dissolved hydrogen sulfide gas and bisulfide ions, and having a fugacity of hydrogen gas and for reducing the fugacity of hydrogen gas in said leaching solution; means for exposing said ore to said leaching solution; and means for recovering said precious metal from said leaching solution.
Claim 15
Dependent Claim 180 words
A process of making a product, said product comprising a precious metal that can form a complex comprising bisulfide, said complex having an aqueous solubility, said process comprising the steps of: introducing an ore of said precious metal into an anaerobic reactor environment, said reactor environment having an activity of dissolved hydrogen sulfide gas, an activity of dissolved bisulfide ions, and a fugacity of hydrogen gas; increasing said activity of dissolved hydrogen sulfide gas and said activity of dissolved bisulfide ions and reducing said fugacity of hydrogen gas, whereby the solubility of the precious metal-bisulfide complex is increased; removing the precious metal-bisulfide complex from said reactor environment; separating said precious metal from said metal-bisulfide complex; and forming said product from said precious metal; wherein said increasing step and said reducing step are accomplished by at least one step selected from the group consisting of contacting said reactor environment with a culture of an oxyanion-reducing bacterium, and contacting said reactor environment with a stream of gas comprising hydrogen sulfide gas and a fugacity of hydrogen gas of less that 0.001 atmospheres.
Claim 16
Dependent Claim 180 words
A process of making a product, said product comprising a precious metal that can form a complex comprising bisulfide, said complex having an aqueous solubility, said process comprising the steps of: introducing an ore of said precious metal into an anaerobic reactor environment, said reactor environment having an activity of dissolved hydrogen sulfide gas, an activity of dissolved bisulfide ions, and a fugacity of hydrogen gas; increasing said activity of dissolved hydrogen sulfide gas and said activity of dissolved bisulfide ions and reducing said fugacity of hydrogen gas, whereby the solubility of the precious metal-bisulfide complex is increased; removing the precious metal-bisulfide complex from said reactor environment; separating said precious metal from said metal-bisulfide complex; and forming said product from said precious metal; wherein said increasing step and said reducing step are accomplished by at least one step selected from the group consisting of contacting said reactor environment with a culture of an oxyanion-reducing bacterium, and contacting said reactor environment with a stream of gas comprising hydrogen sulfide gas and a fugacity of hydrogen gas of less that 0.001 atmospheres.
Claim 17
Dependent Claim 20 words
The process of claim 12 wherein said precious metal is selected from the group consisting of gold, silver, and platinum.
Claim 18
Dependent Claim 23 words
The process of claim 12 wherein said increasing step is accomplished by contacting said reactor environment with a culture of a sulfate-reducing bacterium.

References Cited (Backward Citations)

US4974816A Cited
US4822413A Cited
US4778519A Cited
US4987081A Cited
US5076927A Cited
US4902345A Cited
US5127942A Cited
US5246486A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2000-09-29 2001-03-31 2001-09-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2004-09-29 2005-03-31 2005-09-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2008-09-29 2009-03-31 2009-09-30 $7700.00 Window Closed / Lapsed